Skip to content
Website
🧱 CFC 282Waterproofing beneath tiles in wet areasChapter 3 of 10 in the section

Corners: flexible tape at the base, differential movement and waterproofing failure

This chapter guides you through the technical treatment of internal corners under tiling. You will learn how to size, install and smooth out the flexible reinforcing tape in the corner base in accordance with the requirements of the SIA 248 standard, in order to permanently neutralise differential movements between the floor and walls without the risk of tearing the waterproofing assembly.

Key takeaways

  • Rigid floor-wall connections systematically fail under the effect of screed shrinkage and thermal expansion.
  • The corner reinforcing tape absorbs deformations thanks to its non-adhering elastomeric central zone.
  • The SIA 248 standard requires absolute continuity of the under-tile waterproofing system without thermal bridging or failure.
  • Tape overlap of at least fifty millimetres guarantees impermeability on longitudinal joints.

The kinematics of internal corners and the risk of rigid waterproofing failure

In a bathroom or wet room, the junction between the floor and vertical walls constitutes an area of extreme stress. The floor, generally consisting of a floating screed laid on a thermal or acoustic insulation layer, experiences a mechanical life completely independent of solid or lightweight partitions. This independence results in permanent floor and wall differential movement: residual settlement of the insulation under operating load, progressive hydraulic shrinkage of the mortar, and variable thermal expansion depending on the presence or absence of underfloor heating. When the tiler applies a liquid waterproofing system directly and continuously into the sharp arris of an internal corner without decoupling, the dry film remains intimately bonded to the two perpendicular walls. From the first weeks of operation, relative movement of a few tenths of a millimetre imposes pure tensile stress across an almost zero width, which immediately exceeds the elastic limit of the mineral or synthetic resin and causes a clean tear in the assembly.

Floor-wall differential movement
Three-dimensional relative displacement observed at the junction between the horizontal structure and the vertical wall, caused by substrate shrinkage, settlement of resilient underlayers and seasonal thermal variations.

To overcome this destructive stress, good practice requires the interposition of a corner reinforcing tape. This industrial component combines two lateral wings of rot-proof non-woven fabric with a median zone consisting of a flexible elastomer membrane. The physical objective is simple: transform a point shear stress into an elongation deformation distributed over several centimetres of elastic material. By forming a slight fold or leaving the centre of the tape free from direct adhesion to the masonry corner, the tape acts as a technical bellows capable of absorbing cyclical opening, closing and vertical sliding movements without ever losing its watertightness.

Connections to adjacent building elements and movement joints must be made in such a way as to absorb foreseeable dimensional variations in the substrates without compromising the watertightness of the structure.

Norme SIA 248

Methodical installation of the flexible tape in accordance with the SIA 248 standard

The installation of composite waterproofing under tiling requires absolute geometric precision, particularly when forming coves and internal corners. The substrate must be free of all dust, traces of plaster or sharp concrete arrises that could puncture the flexible membrane. In accordance with the requirements of the SIA 248 standard, the tiler first applies a generous initial coat of liquid waterproofing product using a brush or roller over about ten centimetres on either side of the arris. The tape is then carefully positioned in the fresh bed, taking care not to stretch the elastomer excessively at the bottom of the dihedral so that it retains its full mechanical elongation capacity during future settlement.

  1. Preparation and bonding of the corner baseClean the arris and apply the waterproofing mortar or liquid resin over a minimum width of 100 millimetres on each face of the substrate.
  2. Centring and pressing down of the flexible tapeUnroll the tape, ensuring that the elastomer zone aligns perfectly with the arris. Firmly smooth out the textile edges with a smooth trowel to push out air bubbles and force the liquid material through the non-woven mesh.
  3. Overlapping of strips and preformed corner piecesAt crossings and room corners, first install the prefabricated corner pieces, then fold down the linear strips ensuring a continuous overlap.
  4. Final waterproofing coatingCover the wings of the tape with the second waterproofing coat, ideally protecting the most flexible central part from any excessive soiling that could stiffen the membrane.

The most sensitive point on the construction site concerns tape overlap when butt-jointing or meeting three-dimensional corner pieces. Any interruption in continuity constitutes an immediate infiltration path. Longitudinal overlap must never be less than fifty millimetres, the minimum value established to ensure watertight and durable adhesion between membrane layers. Both thicknesses are saturated with waterproofing product, without abrupt thickness build-up that would hinder the subsequent alignment of ceramic tiles. The perimeter joint of the final tiling must systematically be made with neutral elastic mastic, positioned exactly in line with the treated corner so as not to restrain the assembly.

Evaluation criteria for internal corner installation
Control stepTechnical requirementConsequence of non-compliance
Axis alignmentElastomer zone centred in the cornerLoss of elasticity and asymmetrical tension
Lateral pressingTotal embedding of textile edges without bubblesDelamination under water vapour pressure
Tape overlapOverlap greater than or equal to 50 mmGravity-fed infiltration behind the screed
Tile installationFlexible edge joint without adhesive bridgeMechanical locking of the corner and tile breakage

Overlapping of reinforcing tapes and treatment of trihedral singular points

The treatment of internal corners tolerates no abrupt stopping or butt-jointing of the flexible waterproofing tape. Junctions between consecutive strips, just like transitions from horizontal corners to rising vertical corners, constitute the areas of maximum vulnerability for the under-tile system. According to SIA 248 standard requirements, the waterproofing must form a continuous tub free of mechanical discontinuities. System cohesion relies on the strict rule of watertight overlap, achieved by smoothing into the liquid resin or polymer waterproofing mortar.

Installing a corner reinforcing tape requires precise methodology for managing overlaps. The first section is pressed into the first fresh coat of the liquid waterproofing system, meticulously chasing air towards the edges using a flexible spatula. To connect the second section, the overlap zone of at least 50 mm must first be saturated with waterproofing coating on the upper face of the first strip. The second strip is superimposed without creating excessive thickness or folding, two defects that would prevent the flatness required for subsequent tile installation.

Components of the internal corner reinforcement system according to kinematic stress
System elementLocation areaMechanical functionIncorporation method
Flexible tape with elastic median zoneFloor-wall internal corner (floating screed perimeter)Absorption of vertical settlement and floor-wall differential shrinkagePressing of non-woven wings, neutral centre left free of rigid adhesive
Preformed internal corner piece (trihedron)Lower shower corner (junction of two walls and the floor)Elimination of complex cuts and guarantee of three-dimensional watertightnessDirect bonding in the resin bed prior to installing adjacent linear strips
Standard non-woven reinforcing tapeWall-wall vertical internal corner (heavy partitions)Bridging of assembly micro-cracks without settlement stressComplete embedding between two coats of under-tile waterproofing coating

The most critical point of the structure remains the trihedral corner, where two vertical walls meet the ground slab or screed. Attempting to shape a trihedral corner by simple folding or cutting a flat reinforcing tape with a utility knife inevitably leads to infiltration: either the cut weakens the waterproof membrane, or the folding creates a rigid bulge that is impossible to bed properly. Installing a factory-prefabricated internal corner is essential. This thermoformed piece is positioned first on the freshly coated substrate. Standard reinforcing tapes then overlap the wings of the preformed piece over a width of at least 50 mm, ensuring continuous drainage of water towards the drainage area without counter-slope.

Floor-wall differential movement and decoupling of the ceramic finish

The connecting corner between the screed and vertical partitions is subjected to permanent multi-directional stresses. A floating screed laid on thermal or acoustic insulation undergoes settlement under operating load, coupled with residual hydraulic shrinkage over time. At the same time, load-bearing walls or lining partitions exhibit different inertia. This floor-wall differential movement generates shear and tensile forces that exceed the resistance of a rigid waterproof membrane applied directly onto the arris. The elastomer tape acts here as a movement joint concealed beneath the ceramic.

To guarantee the durability of the assembly in accordance with the good trade practices of the SIA 248 standard, tile installation must scrupulously respect the kinematics of the substrate. The peripheral connection joint at the internal corner level must never be filled with rigid cementitious grout. It must obligatorily receive an elastic mastic suitable for wet rooms, resistant to mould. This surface waterproofing bead in no way replaces the under-tile waterproofing located underneath: it forms the first protective barrier against direct runoff water, while the corner reinforcing tape constitutes the main moisture-impermeable waterproofing structure.

  • Preliminary check of the resilient perimeter edge strip of the screed: trim flush with the tiling only after the liquid waterproofing has cured.
  • Neutralisation of adhesion at the joint base: insertion of a closed-cell polyethylene foam backer rod if the depth of the gap requires it, in order to avoid adhesion on three sides of the silicone mastic.
  • Wall tile installation stopped 5 mm above the surface of the floor tiling to allow free deformation under load.
  • Careful elastic caulking of vertical internal corners receiving direct water splashes in the protection volumes defined by the planning.

The durability of the whole relies on this technical hierarchy: a flexible under-tile waterproofing, capable of moving with the building without failing, topped by a finish whose rupture lines are carefully offset and cushioned. Any misalignment between the screed decoupling plane and the waterproof tape transfers stress directly into the tile, leading to its detachment or chipping of the enamelled edges.

Corner pathologies and repair protocol for cracked waterproofing

The absence of flexible tape or its crushing at the bottom of the dihedral inevitably leads to failure of the under-tile waterproofing film. During screed shrinkage or under the effect of acoustic insulation settlement, the floor and wall differential movement shears the rigid resin applied without elastic bridging. Water infiltration does not always manifest directly at the joint: the fluid migrates by capillarity beneath the floating screed or soaks the base of the lightweight partition, generating major damage in adjacent rooms or beneath the slab.

  1. Selective removal of tilesGrind grout lines without damaging the substrate, then remove the first row of wall tiles and the first row of floor tiles over at least 15 cm on either side of the faulty internal arris.
  2. Remediation and exposureRemove residual tile adhesive with a flat chisel or by gentle mechanical sanding. The substrate must be clean, dry, dust-free and free of any trace of non-adherent torn membrane.
  3. Bridging and installation of corner reinforcing tapeApply an initial coat of liquid waterproofing system. Press in the preformed flexible tape with its unbonded stretchable central zone aligned with the crack, respecting a tape overlap of at least 50 mm on sound areas.
  4. Overlapping and closureApply the second waterproofing coat over the meshed wings after the first coat has dried, then restore the ceramic finish with a flexible surface perimeter joint.

Rigid management of interfaces between trades in accordance with finishing work good practices avoids these costly disputes. Any finding of active structural cracking in the substrate prior to tile installation must be the subject of a formal notice recorded with the site management.

Frequently asked questions

How to repair an internal corner if existing tiling cannot be replaced entirely?

Local removal of the lower wall edge and floor perimeter edge is unavoidable. No surface coating or mastic can restore the continuity of the under-tile waterproofing. After careful cutting of the tiles with a diamond disc, an internal corner reinforcing tape is inserted with a tape overlap of at least 50 mm on the previously cleaned existing waterproofing, before re-gluing identical tiles or a technical finishing strip.

Why must the flexible tape not be fully bonded at the bottom of the cove?

The median zone of the corner reinforcing tape comprises an elastomer membrane without non-woven mesh. This central zone must be able to stretch freely to compensate for floor and wall differential movement caused by insulation settlement or thermal expansion. If the bottom of the dihedral is completely blocked by rigid glue or resin, allowable deformation drops drastically, causing the waterproofing assembly to tear at the first mechanical shrinkage.

What minimum overlap width must be observed at tape connections?

The SIA 248 standard and Swiss technical rules require a tape overlap of at least 50 mm between two successive sections or with preformed internal and external corner pieces. Continuity must be ensured by careful smoothing into the first coat of liquid resin or polymer waterproofing mortar, avoiding any formation of folds or air bubbles that would compromise final impermeability under the action of moisture.

Does the surface silicone joint dispense with inserting waterproofing tape in the corner base?

No. The elastomeric mastic bead applied between tiles constitutes solely a finishing and maintenance joint subject to ageing, mould and mechanical stress. The watertightness of the structure relies exclusively on the under-tile membrane and its corner reinforcing tape. According to good trade practices, tiling and its grouting are never considered watertight under frequent exposure in wet areas.

Texts and standards cited

  • SIA 248Tiled and paved finishes, installation specifications and under-tile waterproofing