Timber as a load-bearing material: species, classes and moisture: execution guide
This section is intended for foremen, chargehands and site managers in timber framing in Switzerland. It brings together the key criteria for inspecting and accepting load-bearing timber as soon as it is unloaded: rigorous measurement of residual moisture, decoding of strength marking, identification of unacceptable defects, compliance with service classes and storage conditions on the construction site complying with the requirements of standards SIA 265 and SIA 265/1.
- 10chapters
- 22 000words
- 6sections in the training course
- 60chapters in total
Key values to remember 4
12 %
Reference equilibrium moisture content in service class 1
20 %
Critical moisture threshold promoting fungal growth
150 mm
Minimum ground clearance for ventilated blocking of timber stacks
0.7 mm/min
Nominal charring rate assumed for softwoods
Technical scope of the load-bearing material and responsibilities upon acceptance
The acceptance of framing and structural timber represents the first critical milestone in the structural safety of a building. The carpenter accepts responsibility as soon as the packages are taken over on the construction site. According to art. 365 CO, the contractor is liable for the material provided and must notify without delay any defect that jeopardises the structure. The requirements of standards SIA 265 and SIA 265/1 require verification of the mechanical, geometric and moisture compliance of the timber before any lifting or final assembly operations.
| Parameter checked | Tool or verification method | Usual conformity criterion |
|---|---|---|
| Core residual moisture | Calibrated moisture meter with insulated pins | Strict match with the defined service class |
| CE marking or certificate of conformity | Visual examination of package stamps and labels | Minimum class C24 or GL24h according to the design |
| Cracking and wane | Steel rule, inspection of the central third | No exceeding of split size tolerances |
| Flatness and storage deflection | Spirit level, line and packer shims | Continuous blocking 15 cm above the ground without residual camber |
A batch of timber with unsuitable moisture or excessive natural defects leads to irreversible deformations once the walls are closed. The scrupulous application of standard SIA 265 prevents differential framing settlement, shearing of connections due to restrained shrinkage and serious disputes linked to structural glue debonding.
Learning pathway and operational logic of the chapters
The sequence of the ten chapters follows the chronological and technical order encountered in the field: from the arrival of the lorry to accounting for fire scenarios, through physical grading and material physics. This pragmatic approach equips the practitioner with the benchmarks required to decide on a delivery refusal in the presence of the driver or carrier.
- Phase 1: Immediate physical inspection on the dockChapters B1-01 to B1-03 detail measuring residual moisture with a pin moisture meter, reading strength stamps according to standard SIA 265 and searching for delamination on glued laminated timber.
- Phase 2: Preservation and quality sorting on siteChapters B1-04 and B1-05 establish the rules for ventilated stacking to prevent rot under impermeable tarpaulins and define the permissible geometric limits for knots, splits and wane.
- Phase 3: Integration into the indoor and outdoor environmentChapters B1-06 to B1-08 link the equilibrium moisture content of the structure to the service classes, determine the need for preservation treatment versus design detailing and quantify volumetric shrinkage.
- Phase 4: Wood-based components and accidental situationsChapters B1-09 and B1-10 clarify the selection of wood-based panels for bracing and explain the calculation of the residual load-bearing section under the effect of fire charring according to applicable standards.
📘 Chapters in this section 10
Residual moisture of timber: measure it upon receipt and reject timber that is too wet
Master insulated pin measurement to refuse timber that is too green immediately.
Timber as a load-bearing material: species, grades and moistureStrength grading: what the marking on a beam says and what it entails
Decode strength stamps to guarantee the load-bearing capacity specified by the engineer.
Timber as a load-bearing material: species, grades and moistureGlulam: what to check at unloading and what causes downgrading
Spot lamella debonding and grain splits as soon as the load leaves the crane.
Timber as a load-bearing material: species, grades and moistureStoring timber on site: blocking, ventilation, and sheeting that does not trap water
Ban impermeable tarpaulins that turn your timber stacks into destructive steaming ovens.
Timber as a load-bearing material: species, grades and moistureKnots, splits, and wanes: permissible defects and those that cause timber rejection
Distinguish permissible seasoning checks from structural defects requiring rejection.
Timber as a load-bearing material: species, grades and moistureService Class: Adapting Timber to the Ambient Moisture of the Structure
Anticipate equilibrium moisture content to prevent swelling and jamming during finishing work.
Timber as a load-bearing material: species, grades and moisturePreservative treatment: when it is needed and when design suffices
Prioritise construction detailing to eliminate superfluous and costly chemical treatments.
Timber as a load-bearing material: species, grades and moistureShrinkage and swelling: allowing for clearance in all three grain directions
Calculate shrinkage clearances accurately to maintain the alignment of bolted connections.
Timber as a load-bearing material: species, grades and moistureWood-based panels: OSB, plywood and solid wood panel, which for which use
Select the appropriate panel based on its actual structural shear wall or diaphragm capacities.
Timber as a load-bearing material: species, grades and moistureTimber in fire: charring rate and load-bearing residual cross-section