Key takeaways
- Resin resolves closely spaced penetrations inaccessible to a blowtorch or welding iron.
- Sanding, degreasing and priming determine mechanical adhesion on all substrates.
- The non-woven fleece must be saturated in the first coat without any residual folds.
- Systematic wet film thickness testing ensures resistance to stresses and substrate cracking.
Substrate preparation and chemical compatibility at membrane junctions
On a flat roof, clusters of vent pipes, flat-anchored guardrail posts, solar panel base plates or metal sections with complex geometries prevent the continuous laying of a bituminous sheet or a synthetic membrane. A blowtorch cannot fit between two penetrations spaced a few centimetres apart, and prefabricated sleeves do not adapt to I- or H-sections. In these specific configurations, a liquid-applied waterproofing (liquid waterproofing) system based on polyurethane (PU) or polymethyl methacrylate (PMMA) resin provides the only reliable technical solution to seal the structure.
The success of a liquid waterproofing system depends on direct adhesion to the substrate. Unlike a fully torched or loose-laid membrane, liquid resin transfers its stresses directly to the substrate. Each material encountered requires specific mechanical preparation prior to coating: concrete must be shot-blasted or diamond-ground to remove cement laitance and open the capillary network; steel or zinc must be degreased with a specific solvent and then stripped by wire brushing or abrasive sanding to achieve sufficient roughness; PVC or EPDM requires solvent cleaning and sometimes a specific chemical activator.
Jointing to the main roof area requires verifying compatibility with the adjacent membrane. On bituminous waterproofing, the roofer must remove protective slate granules by hot scraping or sanding, then thoroughly remove dust over the overlap zone over a minimum width of 100 to 150 mm. Depending on the resin chemistry selected (PMMA or PU), a blocking primer is essential to prevent the migration of bituminous oils and solvents, which would inhibit polymerisation of the liquid system or cause browning along with loss of adhesion.
| Substrate encountered | Required mechanical preparation | Recommended primer type |
|---|---|---|
| Reinforced concrete / cement screed | Milling or diamond grinding, vacuum cleaning | Two-component epoxy resin broadcast with sand or two-component PMMA |
| Elastomeric bituminous sheet (SBS) | Scraping of self-protecting slate granules | Polyurethane or PMMA primer with migration barrier |
| Synthetic membrane (FPO/TPO) | Degreasing clean and light abrasive sanding | Activating bonding primer for thermoplastics |
| Stainless steel or galvanised steel base plate | Solvent degreasing and 60 to 80 grit sanding | Specific metal primer (wash primer or epoxy) |
Installation of embedded reinforcement and strict thickness control
A high-performance liquid waterproofing system on a roof is never just a thick coat of paint. To absorb differential movements between metal penetrations and the concrete slab, the resin must incorporate a non-woven polyester fleece (standard weight 110 to 165 g/m²). This textile reinforcement provides tear resistance, dimensional stability under thermal variations, and bridging of substrate microcracks.
- Dry cutting and fitting of reinforcementCut the textile fleece to the exact dimensions of the upstand and horizontal collar. Allow a minimum overlap of 50 mm between fleece strips, never creating excessive build-ups at internal or external corners.
- Application of the base coat of resinSpread the base coat with a short-pile roller or flat brush, adhering to the specified minimum consumption (often around 1.5 to 2.0 kg/m² depending on product viscosity).
- Immediate embedding and smoothing of the fleeceLay the non-woven fleece directly into the wet resin. Smooth with a de-aerating roller from the centre towards the edges to expel all air pockets and draw the liquid product up through the textile weave until fully saturated.
- Application of the top coatApply the top coat 'wet-on-wet' or after a short gelling time defined by the technical data sheet, in order to embed the fleece texture fully beneath a uniform film.
- Fleece smoothing (marouflage)
- The operation of firmly pressing textile fleece into wet liquid resin using a rigid roller or spatula to eliminate trapped air and ensure complete impregnation without folds or debonding.
System durability relies on strict compliance with cured film thickness. Insufficient thickness compromises watertightness and tear resistance, whilst excessive thickness in a single coat can cause internal stress, surface cracking, or poor through-cure. The site foreman checks wet film thickness during application using a notched comb gauge, pressing the metal teeth perpendicularly into the wet product until firm contact with the substrate is achieved.
Workstation organisation must comply with safety regulations applicable to construction sites. In accordance with art. 3 OPA, the employer shall take protective provisions and measures that comply with recognised occupational safety and industrial medicine rules. The use of liquid resins emitting volatile organic compounds (VOCs) thus requires the wearing of respiratory protective equipment suited to organic vapours and impermeable nitrile gloves. Furthermore, pursuant to OTConst art. 17, measures must be taken at workstations and traffic routes so that workers are not endangered by the collapse of building components or falling objects and materials during the handling of drums and equipment on the roof.
Critical configurations on flat roofs: where bituminous or synthetic sheets fail
On an industrial or commercial flat roof, the proliferation of technical upstands quickly turns the installation of prefabricated membranes into a methodological dead end. Bundles of solar cables emerging together from a single opening, structural steel H-sections (HEA or HEM) anchored to support ventilation units, or guardrail base plates fixed flush with upstand curbs prevent clean detailing with elastomeric bitumen or synthetic sheets. A blowtorch cannot fold an angle fillet without burning adjacent cables or leaving a gaping void in the internal corners of an I-beam. Meanwhile, thermoplastic membranes welded with hot air require a minimum clearance of at least 100 mm to insert the hot-air welding nozzle and pass the silicone seam roller. Below this clearance, a homogeneous weld becomes technically impossible.
In these congested configurations, reinforced liquid waterproofing systems provide the only technical solution meeting the requirements of standard SIA 271. Its initial fluidity allows it to conform to the millimetre around twisted geometries, nut ribs, threaded rods, and sharp edges that are impossible to detail with a factory-made membrane. However, this geometric adaptability does not excuse any lack of rigour: resin tolerates no lapses in mechanical anchorage or in the continuity of the reinforcing fleece. Simply brushing on resin without reinforcement or dry-film control quickly leads to fatigue cracking under the effect of differential thermal movements between metal and concrete.
| Penetration configuration | Limitation of prefabricated membrane | Installation of reinforced liquid system (PMMA or PU) |
|---|---|---|
| Structural steel I-beam column base (HEB / HEM sections) | Impossible to weld internal corners without folds or unbonded overlap build-ups. | Custom cutting of non-woven fleece into four fitted pieces; immediate smoothing into the base coat of resin. |
| Closely spaced photovoltaic cable penetrations (spacing under 50 mm) | Welding nozzle inaccessible; immediate risk of puncturing cable sheathing with open flame. | Liquid encasement with individual sleeving or casting a continuous watertight flashing block enclosing the penetration cluster. |
| Fall-protection posts with bolted base plates | Poor adhesion beneath the base plate and lateral capillary water ingress under screw heads. | Pre-treatment of fixings with compatible sealant, followed by complete encapsulation of base plate and post with 100 mm reinforced overlap. |
| Smooth pipe penetrations immediately adjacent to a parapet | Insufficient space to fit a mechanical clamping collar or preformed sleeve. | Seamless connection from curb to pipe via continuous reinforced liquid bridging, without mechanical breaks. |
Detailing complex shapes and quality control protocol
- Exposing and abrasive preparation of penetrationsStrip all residual rust, unadhered paint, or grease from metal components by grinding, power wire brushing, or 40-grit disc sanding to achieve an impeccable standard of surface cleanliness. On rigid PVC or polyolefin pipes, roughen the surface with abrasive sandpaper and clean using an activating solvent recommended by the system manufacturer.
- Application of specific bonding primerApply the appropriate primer for each material type: non-ferrous metal primer on copper or zinc, primer for bare steel, or adhesion primer for plastics and existing synthetic membranes. Strictly observe the drying time window before applying the first coat of resin.
- Pattern cutting and impregnation of synthetic reinforcing fleeceDry-cut the synthetic fibre (polyester) non-woven fleece to the exact geometry of the penetration: make uniform petal- or star-shaped cuts to conform to cylindrical shapes without folding. Apply the base coat of resin (approximately two thirds of total consumption), immediately embed the fleece into the wet liquid using a mini-roller, then remove all air bubbles by rolling from the centre outwards.
- Saturation coat and tie-in to the main roof membraneImmediately apply the second coat of wet resin over the still-wet fleece to saturate the weave until its white texture completely disappears. Extend the liquid waterproofing onto the adjacent membrane (pre-bevelled bitumen or prepared synthetic) over a minimum width of 100 mm to secure a watertight joint.
Compliance of the installation is established by continuous monitoring of resin application rates per unit area. On irregular geometries, thickness cannot be measured with a comb gauge without risking snagging the wet fleece; it is verified by mass ratio. The site foreman calculates the true developed surface area of each base plate or penetration—including hidden profiles—and allocates an exact count of resin tins to that specific location. Total consumption below the nominal value of the approved system (generally between 2.5 and 3.5 kg per square metre reinforced) provides an immediate indication of low thickness, resulting in reduced elasticity and premature permeability at the penetration.
Remediation and repairs for non-compliant liquid waterproofing
On a flat roof construction site, failures affecting a liquid waterproofing system almost always stem from three causes: a damp or poorly degreased substrate, insufficient resin thickness leaving the fleece exposed, or chemical incompatibility at the junction with bituminous or synthetic sheets. When resin blisters, fails to cure, or peels around a complex penetration, the site foreman must follow a methodical procedure to stop infiltration and restore the watertight integrity of the structure.
- Defect diagnosis and immediate work stoppageUpon observing blisters, tacky areas, or debonding on upstands, stop work immediately. Measure residual substrate moisture and check the dew point temperature. If the substrate proves non-compliant or damp to the point of compromising system adhesion, apply the principles of CO by notifying the client in writing of the defects discovered.
- Mechanical strip-out of the defective areaNever attempt to recoat under-dosed or uncured resin. Cut back the liquid membrane with a utility knife to sound material, extending 100 mm beyond the defect. Fully strip the debonded film back to the bare substrate by diamond grinding, sanding, or mechanical scraping to remove all contaminated residues.
- Preparation and reactivation of contact surfacesThoroughly clean the masonry or metal substrate and apply the specific primer suited to the material. For the junction with adjacent synthetic membranes or remaining cured liquid waterproofing, scuff the edges with fine-grit sandpaper, then wipe with the solvent activator specified by the manufacturer.
- Reconstruction of the reinforced systemApply the base coat of polyurethane or PMMA resin, smooth in a patch of non-woven fleece without wrinkles or trapped air, then immediately top-coat wet-on-wet. Ensure a minimum overlap of 50 mm onto the sound existing coating and check wet film thickness with a comb gauge.
Frequently asked questions
What should be done if the non-woven fleece wrinkles when applied to a curved pipe?
On a curved penetration or rounded base plate, never stretch the fleece by force, as this creates air pockets where water can pond. Neatly snip the non-woven fleece with roofing shears to relieve textile tension, then apply a second reinforcement patch with a minimum 50-millimetre overlap, fully embedded in the wet liquid resin between two saturating coats.
Why does liquid resin fail to adhere to an existing bituminous membrane?
Adhesion fails when the bituminous membrane is contaminated with talc dust, sand granules, or residual welding oils. The bitumen must be mechanically abraded with a wire brush or ground to expose fresh material, vacuum cleaned, and coated with a bonding primer that blocks oil migration prior to applying the reinforced resin.
How can applied thickness be checked on a construction site non-destructively?
During installation, the quality inspector or site foreman presses a notched comb gauge into the wet film to measure the wet film thickness specified in the technical data sheet. In addition, systematically verify the material balance by dividing the weight of consumed product tins by the treated surface area in square metres, ensuring minimum consumption of fleece and resin.
What should be done if rain falls before polyurethane resin cures fully?
Rain falling on single-component polyurethane during curing causes surface foaming and microbubbles that destroy watertightness. Once completely dry, remove the damaged skin by light mechanical sanding down to dense, sound film, vacuum away dust, wipe with a rag soaked in activating cleaner, and reapply a protective top coat of resin.
Texts and standards cited
- COMaterials and site conditions: the contractor is liable for the sound quality of materials supplied; if materials supplied by the client or the ground designated by the client are found to be defective, or if any other circumstance compromises the proper or timely execution of the works, the contractor shall immediately inform the client, on pain of bearing the consequences (para. 3).