Reinforcing an old joint: flitch plating, scarf graft and load transfer

When dealing with a deteriorated or undersized joint, replacing the entire member is not the only option. This chapter guides you step by step through analysing the existing fabric, setting up secure load-relief propping, cutting an end-grain scarf graft, and installing structural flitch plates compliant with the timber engineer's requirements.

Key takeaways

  • Any reinforcement begins with a comprehensive diagnosis of the mechanical and sanitary condition of the timber.
  • Temporary propping must carry the loads before any cutting or removal of decayed material.
  • Flitch plating and the scarf graft reconstruct the structural layout by transferring tensile or bending stresses.
  • Structural calculations and the dowelling scheme strictly require the engineer's approval.

Survey of the existing structure and securing by temporary load transfer

Working on a weakened connection in a roof or floor requires a rigorous reading of the load path. Before picking up any cutting tool, the carpenter probes the primary members: principal rafter, tie beam, king post, or binding beam. The survey is not limited to gross cross-sectional dimensions; it maps the extent of dry or wet rot, shrinkage checks, grain direction, as well as wood-boring insect attacks. Test drilling with a fine auger bit or awl probing allows delineating the remaining sound timber, hidden beneath old paints or renders.

Relieving the failing joint requires a shoring tower or mechanical jacks sized for all remaining permanent and imposed loads. Direct propping on an intermediate floor without ensuring continuity of support down to the foundations or masonry load-bearing walls is prohibited. Pressure is applied to the jacks millimetre by millimetre: the goal is to take up elastic deflection without lifting the overall structure, which could disrupt other nodes in the timber frame or crack the ceilings below.

  • Moisture content check using a pinless or pin meter (target below 18% to stabilise the timber).
  • Installation of hardwood spreader plates under steel props to prevent floor punching shear.
  • Placement of folding wedges and telltales or dial gauges to monitor movements in adjacent structural members.
  • Immediate reconciliation of the execution survey with the civil or timber engineer to validate the feasibility on the construction site.

Flitch plating techniques, end-grain scarf grafting and engineering validation

An end-grain scarf graft is necessary when a beam end or tie-beam heel is degraded by water infiltration at the wall top, while the rest of the member remains sound. The decayed section is purged back to perfectly sound timber, with a safety overlength defined with the specialist. The graft is fashioned from a compatible timber species, ideally structural-grade spruce or oak seasoned to core moisture, using an under-squarred splayed lap joint, a half-lap joint, or a Jupiter scarf joint. This grafted end takes up contact compressive stresses, but requires external reinforcement to bridge shear and bending forces.

Structural flitch plating
Assembly consisting of two members of solid timber, glulam, or steel flitch plates sandwiching the deteriorated load-bearing component to bridge the weakened zone and fully restore mechanical load transfer.
Comparison of flitch plating solutions for historic joints
CriterionSolid timber or glulam flitch platingSteel flitch plating (channel or flat bars)
Bulk / Space requirementSubstantial: extra thickness on each side of the beamLow: thin sections easily integrated into dry lining
Workshop fabricationCutting of precise scarf joints, template-guided through-drillingLaser cutting, drilling and prior anti-corrosion treatment
Hygrothermal behaviourHomogeneous with the old member, similar dimensional movementsRisk of surface condensation against the timber if thermal bridges occur
Required fixingsHeavy-duty threaded rods with wide timber framing washersClose-tolerance bolts or dowels to minimise slip

Installing flitch plates demands precise tightening. Through-bolts must be installed in cleanly drilled holes without excessive clearance, preventing joint slip once load is transferred. Using split rings, double-sided toothed-plate connectors or cylindrical dowels significantly increases shear load capacity. Finally, responsibility for the load path and sizing of steel components rests with the timber engineer: no change of section or alteration to the drilling pattern may be made without written confirmation, in accordance with art. 364 CO governing the contractor's duty of care.

Executing flitch plating on a deteriorated node: solid timber and steel plates

Remediating a deteriorated structural node — such as a tie-beam end, brace foot or rafter head — requires selecting the flitch material based on geometric and conservation constraints. Solid timber or glulam flitch plates maintain the hygrothermal consistency of the structure, whereas fabricated steel flitch plates minimise bulk in tight bearing areas, notably against facade masonry or wall plates.

Execution comparison between timber flitch plates and steel plates for joint reinforcement
Execution criterionTimber flitch platingSteel flitch plating
Transverse bulkSubstantial: adds thickness to both faces of the original member.Low: thick steel plates allow housing the joint within existing wall pockets.
FastenersThrough-bolts with toothed-plate connectors or fitted dowels in stepped boreholes.Fitted solid steel dowels or through-bolts torqued to the specified setting.
Hygrothermal risksMatching shrinkage behaviour; low risk of interstitial condensation.Localised thermal bridging and condensation in contact with masonry: thermal break required.
Substrate preparationMechanical removal of deteriorated wood, chisel paring and sanding of contact faces.Stripping of irregularities, careful planing to guarantee gap-free steel-to-timber contact.
  1. Selective removal and sanitationCut away spongy sapwood or areas damaged by brown rot using a chisel and circular saw. Stop removal as soon as sound wood appears, avoiding unnecessary weakening of the load-bearing cross-section.
  2. Bearing adjustment and templatingFabricate a thin sheet template to trace the exact node deformation, the profile of retained members, and the locations for fittings or planned dowel holes.
  3. Drilling and fitting fastenersDrill main members and flitch plates in a single pass using a drill guide to ensure strict alignment. Drive dowels with a tight push fit or torque bolts using wide bearing washers.

Installing end-grain scarf grafts and load transfer under engineering supervision

The end-grain scarf graft replaces the ruined end of a beam without removing the entire span. Where bearing shear is high, the graft can combine a newly cut timber piece joined with a Jupiter scarf, or an internal steel or fibre connector bonded with epoxy resin. This operation alters the line of thrust and requires absolute compliance with instructions issued by the timber engineering office.

Striking the props is the most critical phase. Under art. 17 OTConst, measures must be taken at workstations and passageways to ensure workers are not endangered by the collapse of building components. De-jacking is performed in steady millimetre increments using linked hydraulic jacks or torque wrenches on screw props. The site foreman monitors for cracking sounds in the new wood, lateral buckling of flitch plates, and the complete stability of the new wall bearing.

The average cost of an end-grain graft on a main beam with steel flitch plates generally ranges from 2,500 to 4,500 CHF per joint depending on access and load-relief difficulties, to be verified on /soumissions/ according to bill of quantities details.

Managing structural unforeseen conditions and stop-work protocol

When working on historic timber frames, exposing the wood frequently reveals defects concealed during the initial inspection: brown rot spreading beyond the purge area, through-checks across planned bolt paths, or unexpected twisting of an element during joint de-tensioning. As soon as a worse structural condition than expected is uncovered, the site foreman must immediately halt all cutting or drilling operations.

In accordance with CO, the contractor must notify the client of any circumstance that compromises the correct or timely execution of the work. On site, this duty to notify takes the form of an immediate stop-work notice sent to the site management and the responsible timber engineer. The condition survey must be updated on the spot, recording remaining sound cross-sections with millimetre-accurate dimensions.

Adapting the technical solution — such as replacing timber flitch plates with heavy steel plates or lengthening an end-grain scarf graft — systematically requires an updated calculation report from the timber engineer. The carpenter must never attempt makeshift wedging under a relieved load-bearing member. Following formal approval of the revised drawings, load transfer is carried out in millimetre stages while monitoring deflections using dial gauges or levelling instruments.

Frequently asked questions

What should be done if the sound wood remaining after removal is too short for flitch plating?

If mechanical removal eliminates so much length that required end distances for through-bolts cannot be maintained, standard flitch plating is ruled out. The carpenter stops cutting and alerts the timber engineer. The approach then shifts to an end-grain scarf graft with a pinned half-lap or a spliced repair using glued-in steel rods, sized according to the remaining load capacity.

How should one react in the event of excessive residual deflection during temporary jacking?

A deflected member that fails to return to level under jacking force indicates a jammed adjacent joint or a risk of grain crushing in compression. Hydraulic jacking must stop immediately. The temporary load is maintained at that height by locking mechanical collar rings, and the timber engineer is asked to recalculate the reinforcement for the observed deformed profile.

Can additional connector holes be drilled without the engineer's approval?

No. Every extra borehole reduces the net timber section and alters the shear stress distribution within the repaired node. Even when encountering a local grain defect, fastener placement, minimum spacing, and bolt or dowel diameters must strictly match the setting-out drawings provided by the structural timber engineer.

Which checks must be documented before striking temporary load-relief props?

The foreman records the final torque of the threaded rods, the correct placement of wide bearing washers, and the status of packings in the daily site log. Jack decompression is carried out gradually under continuous visual monitoring of the bearings. Load transfer is only deemed complete after verifying the complete closure of all reinforced scarf or spliced joints.

Texts and standards cited

  • COmaterials and ground: the contractor is liable for the sound quality of the materials they provide; if materials provided by the client or the ground designated by the client are found to be defective, or if any other circumstance compromises the correct or timely execution of the work, the contractor must immediately inform the client, under penalty of bearing the consequences (para. 3).
  • OTConstrequirements for propping and trench shoring: they must withstand foreseeable loads and forces, be constructed according to good practice, and be dimensioned taking into account supplementary loads (vehicles, plant, stockpiles).

In the same section