Key takeaways
- The outer charred layer insulates the underlying timber and slows down the thermal penetration in depth.
- The charring rate remains constant and predictable according to standard SIA 265 for each timber species.
- The residual cross-section retains its initial mechanical properties almost intact within the core of the member.
- Protective oversizing compensates for pyrolysis without requiring chemical fire-retardant treatment or additional encasement.
Protective pyrolysis and standardised charring rates
Unlike steel, which loses its stiffness abruptly at around 500 °C, solid timber exhibits highly predictable thermal behaviour under the effect of flames. The mechanism relies on self-protection: under increasing temperatures, surface cellulose and lignin decompose without immediate flaming combustion within the dense layers, generating a layer of charcoal. This charred zone exhibits a thermal conductivity approximately six times lower than that of the original sound timber. It forms an insulating shield that significantly limits heat flux towards the centre of the load-bearing element, automatically slowing down the progression of the flame.
- Charring rate
- Rate of linear advance of the pyrolysis front through a timber cross-section exposed to standard conventional fire, expressed in millimetres per minute.
This rate of advance of the thermal front remains linear and constant throughout the standardised exposure duration. For carpenters and timber engineers working in Switzerland, the nominal or design charring rate constitutes the baseline datum for any preventive sizing under fire action.
| Load-bearing material family | Nominal charring rate | Thermal behaviour |
|---|---|---|
| Solid softwood (fir, spruce) | 0.8 mm/min (including corner roundings) | Steady charring, formation of a stable porous char layer |
| Glued laminated timber (softwood) | 0.7 mm/min | Uniform progression, certified adhesive resistant to high temperatures |
| Dense hardwoods (oak, solid beech) | 0.5 to 0.6 mm/min | Reduced rate due to higher density |
Just 20 mm beneath the active charring front where the temperature exceeds 800 °C, the inner wood rarely exceeds 100 °C. The residual moisture evaporates first, consuming thermal energy without impairing the strength of the inner fibres. The timber located in this uncharred zone retains its stiffness and standard deformation characteristics.
Calculation of the load-bearing residual cross-section and oversizing method
Structural fire verification is not performed by trying to prevent the timber from blackening, but by ensuring that after the prescribed evacuation period, the intact core of material is sufficient to carry permanent and quasi-permanent loads. The calculation method of standard SIA 265 relies on the effective residual cross-section. The engineer deducts the cumulative charred depth on all faces exposed to fire from the gross geometry.
The fire resistance of a structural member exposed to fire is determined on the basis of an effective cross-section obtained by subtracting from the initial cross-section the charring depth increased by a transition layer with reduced mechanical properties.
norme SIA 265
- Definition of the required fire resistance durationIdentification of the occupancy requirement set out by the VKF fire protection regulations (for example R30 or R60 for 30 or 60 minutes of load-bearing capacity).
- Calculation of the charring depthMultiplication of the standardised charring rate by the theoretical exposure time, taking corner rounding on unprotected faces into account.
- Removal of the thermal transition layerAdditional standard deduction of a material thickness (generally taken as 7 mm) corresponding to the heated zone whose modulus of elasticity and strength are degraded.
- Stress verification on the residual cross-sectionVerification of bending, compression, or tensile stresses applied to the remaining geometry in accidental design situations according to standard SIA 265.
Protective oversizing consists in deliberately adding, right from the workshop timber-framing phase, this sacrificial thickness onto the visible faces of purlins, primary beams, and posts. A glulam main purlin requiring R60 resistance will typically receive an enlargement of at least 45 to 50 mm per exposed face. No intumescent paint or reinforced plasterboard encasement is then required to validate the structural execution file with the cantonal fire authorities.
Elevated-temperature mechanical behaviour and impact on connections
Contrary to the widespread misconception associating timber combustibility with sudden structural collapse, a massive timber member retains its stiffness under thermal action. The wood located in the core of the load-bearing residual cross-section remains at very moderate temperatures, often below 100 °C, even while the outer faces are engulfed in flames exceeding 800 °C. There is no destabilising thermal expansion likely to push supporting masonry or distort plumbness, unlike the behaviour of unprotected steel frames. The modulus of elasticity and mechanical strength of this central zone remain intact as long as the charring front has not advanced into the resisting core.
The critical point of structural safety in the event of fire does not therefore lie in the body of the beam, but in its structural joints. The steel of fasteners transfers heat with striking speed. A through-bolt or an exposed steel bracket heats up through conduction and transmits this thermal energy directly into the core of the wood, causing internal charring that is invisible from the outside. If the design does not take this thermal bridge into account, the joint fails through local rupture long before the load-bearing residual cross-section of the main member reaches its ultimate limit state.
| Joint configuration | Thermal vulnerability | Required detailing measures |
|---|---|---|
| Concealed flitch plate with dowels | Low: the steel is protected by the outer timber thickness | Minimum dowel embedment depth and systematic plugging with timber plugs |
| Bolted external steel plates | Critical: direct heating of the plate and rapid conduction toward the axis | Surface cladding with fire-rated panels or solid timber build-up of at least 30 mm |
| Traditional wood-to-wood joinery (mortise-and-tenon, half-lap) | Moderate: no conductive metal, but local reduction of geometry | Increase in end cross-sections and shear verification on the residual interlocking cross-section |
Implementation of protective oversizing and on-site verifications
For the site foreman and the team leader, protective oversizing directly affects cutting, transport, and lifting constraints. Adding a sacrificial margin all around a glulam profile or a solid timber beam requires anticipating significantly larger gross volumes than what a simple cold static calculation would dictate. This volume of material has no other function than to burn at the specified charring rate to safeguard the effective cross-section throughout the statutory 30, 60, or 90 minutes.
In practical terms, applying this principle demands flawless execution during machining in the timber framing workshop and on-site adjustments. Sharp edges undergo bilateral combustion that rounds off the corners and accelerates local loss of material. It must therefore be ensured that actual chamfers match the timber engineer's assumptions to avoid any premature weakening of the effective outer fibres. Likewise, no secondary drilling for building services must be improvised without validating its impact on the geometry of the load-bearing residual cross-section.
This approach based on the charring rate restores timber to a leading role in projects subject to strict fire requirements. By accepting the controlled sacrifice of an outer skin, timber framing ensures measurable, predictable, and fully calculable fire stability without requiring intumescent paints that are complex to maintain or systematic boarding. Safety within the meaning of art. 82 LAA then rests on the carpenter's precision when fabricating connections and adhering to sacrificial dimensions.
Dimensional non-conformities, fire incidents and corrective measures
On the construction site, failure to respect protective oversizing directly compromises the required fire resistance. Two critical situations frequently arise: an unauthorised reduction of the timber cross-section during service chasing, and early exposure to an incipient fire before acceptance of the work. In both cases, the team leader or site manager must react following strict technical protocols to ensure the integrity of the load-bearing structure according to standard SIA 265.
- Identification and immediate cessation of notchingAs soon as an unapproved service penetrations or cut-out on the shop drawings cuts into the sacrificial margin, halt the subcontractor's core drilling. Record the remaining actual dimension with callipers.
- Contractual noticePursuant to CO, the contractor notifies the client when any circumstance jeopardises the timely or proper execution of the work. The letter records the location of the notched member and the loss of thickness.
- Post-incident diagnosisAfter an incipient fire has been extinguished on the construction site, scrape the char layer with a chisel or wire brush down to the sound, unpyrolysed timber. Measure all four residual faces to recalculate the remaining load-bearing capacity.
- Validation of compensatory measuresSubmit the revised sizing to the timber engineer. Approved solutions include encasement with rated fire-stop boards, reinforcement using concealed steel plates, or the outright replacement of the load-bearing member.
If the engineer's calculation shows that the sound residual cross-section no longer ensures the service load conditions, retrofitted encapsulation represents the final recourse before dismantling. Fire-stop boards must be fitted with meticulous care at joints to recreate the lost thermal insulation, without generating thermal bridges through metal fixings.
Frequently asked questions
How do you accurately measure the thickness of charred timber after a partial fire?
On the construction site, the friable charcoal must be scraped off using a gouge or a wire brush until reaching the zone of hard, thermally undamaged timber. The measurement is then taken with thickness callipers or a rigid folding rule relative to the remaining sound reference faces, providing the exact geometry of the load-bearing residual cross-section for verification by the timber engineer.
Can a timber cross-section undersized for fire be compensated for with intumescent paint?
Yes, subject to approval by the responsible civil engineer and compliance with VKF directives. An approved intumescent paint slows down temperature rise and delays the ignition of solid timber. However, on the construction site, its application requires dry film thickness to be strictly checked with a wet/dry film gauge—a delicate operation rarely accepted to offset major structural geometric deficiencies on primary beams.
Does a 20 mm cable penetration really compromise a beam designed for 60 minutes of fire resistance?
Yes, if the hole is located in a governing tension or compression zone. Even when small, an opening allows flames and hot gases to penetrate the core of the member. The charring rate then develops from within the hole, which destroys the load-bearing residual cross-section far more quickly than the uniform thermal attack on external faces assumed in the calculation model.
What squaring tolerance is permitted on the protective oversizing of solid timber?
The sacrificial margin permits no negative deviation from the minimum dimensions calculated for the required fire resistance. If a 200 by 300 mm beam cross-section requires 40 mm of protective oversizing on each exposed face, any planing or geometric defect reducing the gross dimension below the specified millimetre invalidates the standard-compliant fire performance under standard SIA 265.
Texts and standards cited
- norme SIA 265Timber construction: structural design and fire behaviour
- COMaterials and site: the contractor is liable for the sound quality of the materials he provides; if the materials supplied by the client or the ground designated by him are found to be defective, or if any other circumstance jeopardises the timely or proper execution of the work, he must immediately notify the client, failing which he shall bear the consequences (para. 3)