Skip to content
Website
🧱 CFC 214Traditional timber framing: trusses, purlins and raftersChapter 10 of 10 in the section

Carpentry tolerances: top levelling, straightness, and roof plane flatness

This chapter enables the carpentry foreman to master permissible deviations for top levelling, plumb, and flatness according to standard SIA 414. It details the inspection methodology on rafters and purlins using a string line and rotary laser, in order to formalise a handover report to the roofing trade without subsequent disputes.

Key takeaways

  • Standard SIA 414 governs the permissible dimensional tolerances applicable to timber structures.
  • The roof plane requires strict straightness to prevent underlying waterproofing defects.
  • Combined checks with a laser level and string line guarantee the conformity of the top levelling.
  • The joint handover report discharges the carpenter prior to the intervention of the subsequent roofer.

Flatness and straightness tolerances of the rafter plane according to standard SIA 414

On a traditional carpentry construction site, the positioning of purlin top levels and the alignment of the outer face of rafters directly determine the quality of the substrate received by the roofer. Any alignment deviation on the load-bearing framework affects battens and counter-battens. Permissible execution tolerances for cut and assembled carpentry are governed by standard SIA 414, which sets the maximum acceptable deviations relative to nominal dimensions and theoretical drawings.

Permissible execution deviations for roof structures according to standard SIA 414
Element checkedSpan or reference lengthMaximum permissible deviation
Top levelling of wall plates or ridge purlinsLess than 6 m between supports± 8 mm
Top levelling of wall plates or ridge purlinsFrom 6 m to 15 m between supports± 12 mm
Straightness of the rafter plane (local deflection)2 m straightedge placed on rafters± 4 mm
Overall slope flatnessSlope diagonal up to 10 m± 10 mm

The straightness of the roof plane does not tolerate any upward deflection (camber) on rafters or purlins, as a hollow promotes the ponding of meltwater or prevents the correct interlocking of tiles. Similarly, lip deviations between consecutive rafters must remain below 3 mm. If solid timber displays a natural drying bow after machining, the carpenter strictly aligns the curvature upwards (heart side up) so that the dead load compensates for the deformation without creating a detrimental hollow.

Rigorous inspection method and joint handover report

  1. Height survey using a rotary laserSet up the rotary laser on a fixed reference point of the building. Measure with a graduated staff the top level elevation of each wall plate, intermediate purlin, and ridge purlin at each truss or load-bearing wall to confirm absolute heights.
  2. Straightness check using a nylon string lineStretch a builder's string line from one hip to the other or from gable to gable, on the outer face of the rafters, 50 mm above the timber using packing pieces of identical thickness. Check with a rule for the absence of sag or crowning along the entire span.
  3. Local check with a two-metre straightedgePlace the 2 m aluminium straightedge across three consecutive rafters to check local lip deviations and record the points requiring backing off or packing.
  4. Preparation of the joint inspection recordSummon the roofing trade foreman to inspect the carpentry, record actual dimensions, and have the official document transferring responsibility countersigned.

The absence of systematic checks exposes the carpentry team to severe disputes during tile laying. When the roofer notices undulations on the battening, remedial work on finished timber generates unforeseen labour costs. To prevent these disputes, the team leader applies the duty to notify provided for by law in the event of an identified incompatibility with the preceding work.

if the material supplied by the client or the site designated by him is found to be defective, or if any other circumstance compromises the proper or timely execution of the work, he shall immediately inform the client thereof, under penalty of bearing the consequences (para. 3).

art. 365 CO

Transmission of frame deviations and direct impact on the roofing trade

On a timber carpentry construction site, every geometric deviation accumulated during erection has a mechanical impact on secondary components. The top levelling of wall plates, the packing of intermediate purlins, and the alignment of the upper edge of rafters determine the theoretical surface on which battens or counter-battens rest. A dip of a few millimetres on a ridge purlin or an out-of-plumb truss alters the general alignment of the roof pitch, complicating the task of the tile or slate layer, who cannot rectify these defects through simple packing without weakening the structure.

Impact of carpentry alignment defects on roofing interfaces
Carpentry geometric defectPhysical observation on the frameDirect consequence for the subsequent trade
Top levelling defect on wall plateLocalised level difference exceeding 5 mmTilting of the first course and difficulties in connecting to the verge line
Excessive deflection on intermediate purlinLongitudinal undulation visible under string lineLip deviation of battens and loss of uniform overlap for small units
Wane or lip deviation of raftersIsolated gap under the 2 m straightedgeCantilever of battening creating a hard spot or risk of capillary ingress
Out-of-square condition at the ridgeAngular deviation between adjacent slopesImpossibility of laying straight ridge components without complex recutting

Standard SIA 414 governs permissible deviations for load-bearing timber structures and sets acceptable ranges of variation depending on the nature of the components. When the carpenter fails to brace vertical timbers or tolerates an intrinsic bow from unstraightened logs, the roofline becomes unstable. Rectification work must systematically take place before the final fixing of jack rafters or common rafters, by means of targeted planing or rot-proof packing under purlin cleats, and not at the level of the roof substrate layers.

Cross-inspection protocol and handover report between trades

Validating the timber framing plane requires a joint measurement procedure. The carpentry foreman sets up surveying instruments on a stable datum at ground level or on the bare concrete slab. The combined use of a rotary laser level calibrated to the official level mark and a high-tension polyamide string line allows for detecting planarity irregularities. Critical points such as valleys, hips, and eaves undergo a systematic altimetric survey at every primary support.

  1. Setting up the laser reference planeStationing the rotary laser on a stable tripod away from walkways; transferring the building's absolute altimetric benchmark to the purlin heads and wall plates.
  2. Pulling the pitch string lineFixing a steel or polyamide string line across the roof slope, flush with the top surface of the end rafters, to measure peak deviations.
  3. Joint recording of dimensionsWalking the slope in the presence of the site manager of the subsequent trade; millimetric recording of positive or negative deflections every three metres.
  4. Signing the handover recordDrafting on a tablet or carbonless form the document recording measurements, potential reservations, and formal acceptance of the substrate.

Drafting a handover report formalises the transfer of the rough structure. Under art. 365 CO, if any circumstance compromises the regular or timely execution of the work, the contractor immediately informs the client. This provision protects the carpentry firm by recording the geometric compliance of trusses and the ridge at the time of transfer. The signed document defines physical liability: any misalignment observed after this stage stems from accidental overloading or modifications attributable to subsequent trades.

The report specifies the date of inspection, contact details of attendees, average residual timber moisture measured by a pin-type moisture meter, and the list of areas accepted without reservation. In the event of an off-tolerance deviation, a short intervention timeframe is recorded to perform planing or cleat adjustment rectifications. Art. 367 CO specifies that after delivery, the client examines the condition of the work as soon as feasible and notifies the contractor of defects. The joint signing of the reservation clearance form concludes structural operations and authorises safe access for finishing teams.

Non-conformance management and arbitration prior to roofer intervention

When the joint inspection record reveals a straightness defect of the roof plane or a top-level lip deviation exceeding permissible values under standard SIA 414, the carpentry site foreman must intervene prior to delivery of materials for the subsequent trade. The roofer must not compensate for these deviations with improvised shimming beneath battening. This bad practice creates hard points, weakens fastenings, and transfers liability for geometric defects to the secondary trade.

  1. Immediate inspection and interface stopWritten notification to site management during the endorsement of the handover report to the subsequent trade. Out-of-tolerance rafters are marked out on the roof slope.
  2. Top levelling and straightness rectification measuresLocalised planing of wanes or solid wood overthicknesses, backing off, or installing structural firrings mechanically fastened in accordance with instructions from the engineering office.
  3. Final joint inspectionRepeat rotary laser check and straightedge pass in the presence of the roofing foreman, documented by the joint signing of the rectified report.

A contractor identifying an interface issue with previous work or constraints disrupting their own execution relies on the duty to notify. According to art. 365 CO, if the material supplied by the client or the ground designated by them is found to be defective, or if another circumstance compromises the regular or timely execution of the work, the contractor informs the client immediately. If the carpenter refuses to carry out rectification of their top levelling, site management can apply the defective execution rules provided for by the Code of Obligations (CO), setting a deadline to eliminate the defect prior to delegating to a third party.

Frequently asked questions

Can the roofer refuse to sign the handover report?

Yes. If geometric checks with a string line or laser reveal deviations exceeding the tolerances set by standard SIA 414, the foreman for the roofing trade refuses acceptance without reservations. They record the observed lip deviations precisely on the handover report to the subsequent trade. This refusal suspends the transfer of custody of the roof slope until the carpenter has rectified the alignment of load-bearing elements.

How should raftering displaying a sag of more than 15 mm be corrected?

Correction is carried out by adding backed-off packing boards or tapered solid wood firrings, securely nailed or screwed to the sagging rafters. The carpenter must never merely stack isolated shims beneath counter-battens. The bearing surface must remain flat and continuous across the entire span length to ensure proper transmission of climatic loads without subsequent subsidence.

Which method is best for checking the flatness of a large roof slope?

Checking is ideally carried out by combining two techniques: a rotary laser set parallel to the theoretical roof plane to detect elevation deviations across the whole surface, combined with a nylon string line pulled diagonally from edge to edge. This dual check enables rapid verification of roof plane straightness and prevents twists that are invisible with a simple 2 m straightedge.

Who bears shimming costs if the roofing trade starts work without reservations?

If the roofer begins installing materials without having established a joint inspection record or issued written reservations, the work is deemed accepted as is. The roofer then assumes liability for appearance defects or water ingress resulting from the level defect. Additional costs associated with subsequent adjustments or dismantling battening can no longer be recharged to the carpenter by site management.

Texts and standards cited

  • SIA 414Dimensional tolerances in building construction
  • CO art. 365Material and ground: the contractor is liable for the sound quality of the material supplied; if the material supplied by the client or the ground designated by them is found to be defective, or if another circumstance compromises the regular or timely execution of the work, the contractor informs the client immediately, under penalty of bearing the consequences (para. 3).