Skip to content
Website
🧱 CFC 214Timber as a load-bearing material: species, grades and moistureChapter 8 of 10 in the section

Shrinkage and swelling: allowing for clearance in all three grain directions

This chapter provides calculation tools and workshop habits to anticipate dimensional changes in load-bearing timber. You will learn how to quantify differential shrinkage along the three anatomical axes, adapt installation clearances in your hardware according to SIA 265, and position mechanical fasteners judiciously to prevent any predictable shrinkage crack.

Key takeaways

  • Anisotropy dictates that tangential shrinkage is twice radial shrinkage, with axial shrinkage remaining practically negligible.
  • Standard SIA 265 governs dimensional variations according to service humidity classes.
  • A rigid connection without slotted holes blocks transverse shrinkage and causes the timber to split.
  • Solid timber develops a predictable shrinkage crack as soon as it drops below the fibre saturation point.

Quantifying differential shrinkage along the three anatomical directions of timber

Timber reacts to thermo-hygrometric variations exclusively below its fibre saturation point, located around 28 to 30 % moisture content. During workshop drying or during service beneath a heated roof, bound water leaves the cell walls, causing fibre shortening. This variation is not uniform: the highly anisotropic behaviour of the material requires distinguishing tangential, radial and axial shrinkage for each load-bearing cross-section.

Average dimensional variation coefficients for common domestic softwoods (spruce and fir)
Anatomical directionShrinkage coefficient per moisture content pointOrder of magnitude for Delta u = 5 %Direct consequence in structural design
Axial (along the grain)0.01 % per % of delta u0.05 % (i.e. 0.5 mm per metre)Negligible on short members, noticeable on tall columns
Radial (perpendicular to growth rings)0.15 to 0.19 % per % of delta uApproximately 0.8 to 1.0 % of the dimensionMeasurable variation on quarter-sawn timber
Tangential (tangent to growth rings)0.30 to 0.36 % per % of delta uApproximately 1.5 to 1.8 % of the dimensionMajor factor in gap opening or splitting

For a glulam purlin or a spruce girder with a depth of 600 mm delivered at 15 % moisture content and drying to 9 % in a heated space, the total depth reduction routinely reaches 5 to 7 mm. If this member rests on a fixed steel bracket with no vertical sliding capability for the dowels, the mechanical restraint leads to transverse tensile stresses that are fatal to the integrity of the member.

Predictable shrinkage crack
Longitudinal tear in the wood grain resulting from the shrinkage differential between the perimeter of the log (high tangential shrinkage) and the pith (moderate radial shrinkage), inevitable in boxed-heart solid timber.

Designing expansion clearance in the connection to eliminate defects

Dimensional variations resulting from changes in timber moisture content must be taken into account when designing construction details and choosing the arrangement of fasteners, in order to prevent unwanted secondary stresses or brittle failures due to tension perpendicular to the grain.

norme SIA 265

To prevent a beam from splitting at its supports or joints, the carpenter must release the degrees of freedom perpendicular to the wood grain. As soon as the depth of a group of dowels exceeds 150 to 200 mm, rigid restraint constitutes a direct workmanship defect. Concealed web plates and hidden joist hangers must incorporate slots allowing the free shrinkage of the timber depth.

  1. Machining slotted holes in steelDrill metal connection plates with a circular hole for the upper load-bearing bolt, and vertical slotted holes of at least 6 to 10 mm for the lower fasteners.
  2. Clearance allowance at head and undersideProvide a minimum air gap of 10 mm beneath the bottom of joists or girders inserted into internal-flange hangers so that the member does not hang up on the fasteners during shrinkage.
  3. Limiting shoulder distancesReduce the distance between the support point and the furthest dowel to limit the absolute magnitude of cumulative transverse movement.

Managing predictable shrinkage cracks in heavy solid timber also requires orienting the growth rings during sawing. When the element contains the pith, provide a longitudinal relief kerf on the non-visible face or opt for glued solid timber. Adhering to these details ensures overall mechanical performance in accordance with SIA 265 requirements and protects the carpenter against web splitting failures during service.

Differential hygrometric behaviour and predictable shrinkage cracks

Moisture management in load-bearing timber structures requires a rigorous analysis of volume changes below the fibre saturation point, located around 28 to 30 % moisture content on a dry basis. According to SIA 265, structural design must integrate the equilibrium moisture state expected in service. Solid framing timber or a heavy beam installed at a moisture content above the building's equilibrium level will inevitably dry, developing severe internal stresses due to shrinkage anisotropy. Dimensional change does not occur with the same intensity along the three anatomical axes, which makes the occurrence of shrinkage cracks predictable and almost systematic in boxed-heart solid timber.

Orders of magnitude of shrinkage coefficients and behaviour by anatomical direction (average values for domestic softwoods: spruce, silver fir)
Anatomical directionAverage shrinkage coefficient (% per % moisture content)Typical variation (drop from 18 % to 10 % moisture content)Mechanical and kinematic sensitivity
Axial (along the grain)0.01 %Less than 0.1 mm/m (often negligible on short members)Stable; variations noticeable only over long spans or multi-storey continuous columns.
Radial (perpendicular to growth rings)0.15 % to 0.19 %From 1.2 % to 1.5 % (i.e. 1.2 to 1.5 mm for 100 mm thickness)Moderate movement guided by medullary rays providing relative resistance.
Tangential (tangent to growth rings)0.30 % to 0.36 %From 2.4 % to 2.9 % (i.e. 2.4 to 2.9 mm for 100 mm width)Critical zone: shrinkage approximately twice radial shrinkage, causing warping and surface checking.

The tangential-to-radial shrinkage ratio, often between 1.5 and 2.0, induces major transverse tensile forces during desorption. In a boxed-heart squared timber, the outer circumference attempts to shrink twice as fast as the internal rays. When the tensile stress perpendicular to the grain exceeds the characteristic strength of the material—which is particularly low in spruce—the radial shrinkage crack opens from the surface towards the pith. This phenomenon is not a defect within the meaning of art. 365 CO alinéa 3 if the contractor uses timber conforming to the visual or mechanical grading specifications ordered, but constitutes a physical property inherent to through-and-through or boxed-heart sawing.

Construction details and installation of expansion clearances to preserve load capacity

To prevent shearing of a framing member or splitting of a connection fitting, freedom of movement perpendicular to the grain must be physically provided. The most common error consists in locking components with rigid connections on their outer edges. When a girder crosses a column base or a primary beam rests on a metal base shoe, stacking transverse thicknesses leads to substantial dimensional changes.

  1. Positioning slotted holesIn steel column bases or internal-flange brackets, machine slotted holes oriented in the direction of transverse movement (depth or width of the member) to allow free play of the dowel without initiating a splitting crack under permanent loading.
  2. End clearance and pockets in masonry supportsSystematically leave a clearance of at least 15 to 20 mm at the end of a purlin or girder built into a concrete pocket. This prevents wedging against the masonry during summer swelling while ensuring end-grain ventilation.
  3. Decoupling plates and secondary structuresOn stud frames, fix rigid cladding elements or service battens using screws through oversized pilot holes, thus preventing storey settlement from crushing services or cracking structural panels.

Managing shrinkage damage and retrofitting locked fittings

On a timber construction site, the appearance of mechanical binding or an out-of-tolerance predictable shrinkage crack often indicates an initial lack of clearance combined with poorly anticipated in-service drying. When dowels, bolts or connection plates restraining the timber perpendicular to the grain trigger transverse tensile failure initiation, the foreman must intervene before structural safety is compromised according to SIA 265 criteria.

  1. Dimensional diagnosis and moisture assessmentMeasure core timber moisture content using an insulated pin-type moisture meter. Compare the measured dimension to the nominal fabrication drawing dimension to quantify actual tangential or radial shrinkage. Examine crack geometry: a stabilized crack parallel to the grain, located away from connection shear zones, generally does not affect overall load-bearing capacity.
  2. Mechanical relief and clearance liberationInstall temporary propping if the connection contributes to purlin or girder stability. Loosen fasteners under transverse tension. In metal components enclosing the timber piece, slot the holes using a reamer or workshop milling machine to restore the free travel required for expansion clearance within the joint.
  3. Strengthening with fully-threaded screws and notificationIf the fracture plane threatens shear resistance or splits a nodal zone, install self-tapping fully-threaded screws perpendicular to the grain to stitch the member together, following the timber engineer's instructions. Immediately notify site management of the observed dimensional discrepancies to document the state of the works.

If the client challenges the appearance of a split element, point out that drying induces natural tangential stresses. In accordance with art. 365 CO, the contractor reports without delay any environmental or design anomalies that compromise the sound performance of the works, particularly an excessively dry ambient moisture level caused by rapid initial heating of the building.

Frequently asked questions

How do you distinguish a harmless shrinkage crack from a structural crack?

A shrinkage crack strictly follows the timber grain orientation and stops naturally at the pith or a knot. It relieves differential tangential shrinkage. Conversely, a structural crack crosses the section diagonally under shear stresses or tears through fastener holes under transverse tension. As soon as a crack runs completely through a support or isolates mechanical fasteners, strengthening with fully-threaded screws becomes mandatory.

What slotted hole dimension should be used for an internal web bracket?

Over a solid or glulam beam depth exceeding 240 mm, transverse dimensional variation easily reaches 4 to 8 mm between installation and service conditions. The top hole acts as the standard fixed point with a minimal 1 mm clearance. The lower holes must be machined as vertical slots with free travel corresponding to the maximum shrinkage calculated according to SIA 265.

What should be done when a CLT column is restrained between two concrete slabs?

In the axial direction, timber moves very little, about 0.01 % per percent of moisture content. Settlement stems mainly from transverse compression of sole plates or bearing clearances. If the slabs dry and shrink transversely while the column retains its axial length, point-load shedding occurs. Adjustable base shims or compressible strips beneath the base plate must be provided to prevent buckling.

Why do halving-joint joists systematically split at the notch?

The halving cut or end notch creates a sharp stress concentration at the re-entrant corner. When tangential and radial shrinkage occur, tension perpendicular to the grain combines with vertical shear, initiating a continuous horizontal crack. According to Swiss trade rules, preference is given to concealed metal hangers, dovetail connectors, or inclined screws that preserve the full cross-section without geometric restraint.

Texts and standards cited

  • SIA 265Timber structures - Actions and design of timber structures
  • CO art. 365materials and site: the contractor is liable for the sound quality of the materials he provides; if the materials supplied by the client or the site designated by him are found to be defective, or if another circumstance compromises the regular or timely execution of the work, the contractor immediately informs the client, under penalty of bearing the consequences (al. 3).

In the same section