Key takeaways
- Aggressive sanding of the anhydrite screed removes the friable film that prevents mechanical bonding.
- An industrial vacuum cleaner connected directly to the sander prevents clogging of the pores of the mineral substrate.
- The SIA 253 standard makes any bonding conditional upon a clean, sound, cohesive and dust-free substrate.
- The bonding primer must correspond precisely to the chemistry of the parquet adhesive being used.
Remove anhydrite laitance by abrasive sanding and industrial vacuuming
Calcium sulphate-based self-levelling screeds systematically exhibit, during setting and drying, an upward migration of water laden with additives and fine particles. This phenomenon creates a whitish, powdery film on the surface with almost zero mechanical strength, commonly known as laitance. Installing bonded parquet on this residual layer without mechanical intervention is equivalent to fixing a floor covering to chalk: under the effect of the natural shrinkage and swelling of solid or engineered wood, the adhesive film tears off the friable film, causing widespread detachment of the boards.
The substrate intended to receive a bonded floor covering must have a flat, dry surface, free of detrimental cracks, clean, resistant to tensile stress and free from any laitance or non-adherent material.
norme SIA 253
Mechanical opening of the surface constitutes a mandatory operation falling under the scope of the parquet layer's work prior to bonding. It is carried out using a heavy single-disc floor machine or a concrete surface grinder equipped with diamond segments or silicon carbide abrasive discs of grit 16 to 24. The objective is to expose the hard, stable body of the screed. Superficial fine-grit scuffing is strictly ineffective; the action must abrade the entire shiny film until the compact granular structure of the mortar appears.
- Mechanical surface strippingPass the heavy rotary machine equipped with very coarse carbide discs in regular overlapping passes, insisting on areas of dense bleeding until the matt colour of the screed core is fully exposed.
- Synchronous vacuuming and cleaningConnect the sander to a sealed industrial dust extractor to capture particles at source. Then carry out a second slow vacuuming pass over the floor using a flat nozzle fitted with hard brushes.
- Surface strength testingCheck the mechanical strength using a cross-scratch test with a steel screwdriver or sclerometer: the scratch must be clean, without crumbling or detachment of mortar flakes.
Select and apply the adhesion primer according to the adhesive binder
A calcium sulphate screed differs from a cement screed in its chemical sensitivity and reactivity with certain hydraulic binders or solvents. The application of a primer is not merely a comfort measure: it ensures the fixation of microscopic dust residues inaccessible to vacuuming, regulates the porosity of the base to prevent premature drying of the adhesive bead, and neutralises any risk of undesirable chemical reaction between the gypsum and the adhesive formulations.
| Type of parquet adhesive | Required primer | Mode of action on sulphate screed | Indicative drying time |
|---|---|---|---|
| Silane-terminated polymer (MS) | Special acrylic dispersion or approved primer-free | Fixation of residual dust and homogenization of absorption | Two to four hours depending on ventilation |
| Two-component reactive polyurethane | Two-component epoxy resin blinded with sand | Mechanical barrier and adhesion bridge via quartz silica | Twelve to twenty-four hours before installation |
| Single-component polyurethane | Solvent-based or water-based polyurethane primer | Deep impregnation and surface hardening of the mortar | Three to six hours depending on humidity |
The choice of product must imperatively be made within the framework of the complete system approved by the adhesive manufacturer. In the case of wide solid parquet flooring subject to high shear stresses, the interposition of an epoxy primer with broadcast oven-dried quartz sand creates an impeccable mechanical bonding bridge. For multi-layer parquet flooring installed with modern elastic silane-based adhesives, water-based synthetic resin primers are generally sufficient, provided that the dry film is completely transparent and non-tacky before spreading the adhesive beads.
Surface cohesion check and acceptance according to standard SIA 253
Aggressive sanding with an abrasive disc or diamond exposes the hard matrix of the calcium sulphate screed, but the operation is only complete after formal verification that the laitance has disappeared. According to standard SIA 253, the substrate intended to receive bonded parquet must have a flat, dry, clean surface, free of untreated cracks and possessing sufficient surface cohesion. Anhydrite laitance forms a film of powdery cells without structural consistency. If whitish or powdery areas remain after industrial vacuuming, the parquet layer must repeat the mechanical surfacing before authorising any application of liquid product.
| Controlled parameter | On-site test method | Acceptance criterion | Corrective action |
|---|---|---|---|
| Removal of laitance | Cross-scratch with hardened steel nail (surface hardness test) | Regular groove without peripheral crumbling, visible sand grain | Resand with grit 16 or 24 down to the core of the matrix |
| Residual cleanliness | Application and removal of high-strength adhesive tape | No dust or gypsum particles on the bonded side | Second pass with an industrial vacuum cleaner equipped with a class M filter |
| Substrate porosity | Deposit of a drop of clean water at room temperature | Complete absorption between one and three minutes | Adjust the primer dilution rate or choose an epoxy resin |
| Skin strength | Grid pattern cut with a utility knife at 5 mm spacing | Clean edges without cracking of the plaster squares | Surface milling or consolidation with penetrating primer |
The evaluation of surface hardness is carried out systematically on several representative areas of the room, particularly along walls and in corners where heavy sanding machines are less accessible. The hardened nail scratch test confirms whether the powdery layer has been penetrated over the entire surface. Any area producing white dust under the metal tip indicates an unstable laitance residue that would cause delamination under the tensile stress exerted by the wood during its dimensional changes.
Primer-adhesive interface and parquet installation
Once the screed has been stripped and dust-removed, the application of the primer regulates the porosity of the anhydrite and creates the adhesion bridge required for the chosen adhesive. On a calcium sulphate binder, the direct use of an adhesive without a suitable primer exposes the assembly to two major risks: rapid desiccation of the adhesive due to suction by the porous substrate, or conversely, a harmful chemical reaction between the components. Water-based primers are suitable for dispersion or silane adhesives subject to complete drying, whereas polyurethane or epoxy resins chemically block residual resins for reactive adhesives.
- Final dust removalPass the flat nozzle of the class M filtration industrial vacuum cleaner along edges, corners and the main surface just before bonding.
- Roller application of primerDistribute the product evenly in a cross pattern without leaving puddles in depressions or missing spots on screed ridges.
- Core drying checkWait for the complete evaporation of the solvent or water in accordance with the technical data sheet, while monitoring the ambient humidity and temperature of the room.
- Combing the parquet adhesiveSpread the adhesive using the appropriate notched trowel to ensure continuous transfer onto the back of the boards without contaminating the primer with construction site dust.
Coordination with other trades is paramount as soon as primer application is completed. A sanded and primed anhydrite screed must no longer receive construction site traffic: walking with dirty soles or the falling of plaster would cancel out the action of the primer by reintroducing a separating film. The bonding of the parquet boards must proceed without interruption as soon as the primer is walkable, ensuring optimal transmission of expansion stresses to the mineral substrate in accordance with Swiss professional rules.
Adhesion failure and remediation of non-compliant substrates
When adhesion fails after bonding, the finding is almost always identical: the adhesive detaches from the substrate, carrying with it a whitish or powdery film. This phenomenon indicates the presence of residual surface laitance on the anhydrite screed, due to insufficient mechanical abrasion or inadequate vacuuming prior to installation. According to standard SIA 253, the parquet layer must refuse to bond to a powdery substrate or one from which friable residues have not been removed.
- Work stoppage and traceabilityInterrupt installation at the first doubt regarding the cohesion or wetting of the primer. Photograph the underside of the pulled-off boards and record the powdery condition of the laying bed.
- Full mechanical strippingRemove unbonded elements and eliminate surface mortar by heavy planing or diamond disc sanding until the sound anhydrite matrix is recovered.
- Dust removal and chemical requalificationUse an absolute-filtration industrial vacuum cleaner, then apply a barrier primer or polyurethane/epoxy bonding primer suited to the new planned bonding resin.
If the adhesion primer flakes off by itself even before filling, the error often stems from chemical binder incompatibility or a violated drying time. On a calcium sulphate-based screed, the direct use of an adhesive containing water without a prior barrier forms swelling compounds that destroy adhesion. Remediation requires returning to the bare mineral substrate by aggressive sanding, followed by further vacuuming under continuous suction.
Frequently asked questions
How to reliably spot residual laitance before installing parquet?
Pass a steel blade or flat screwdriver at an oblique angle over the surface of the anhydrite. If the metal produces a powdery, tender or whitening groove without clear resistance, laitance is still present. On a properly sanded substrate in accordance with standard SIA 253, the mineral grain appears clean, uniform, dark and hard. If in doubt, apply high-strength fabric adhesive tape: it must not pull off any dust.
Can anhydrite laitance be remedied with a highly penetrating primer without sanding?
No. No bonding primer, even one based on solvents or highly fluid epoxy resins, can transform a crust of friable laitance into a structural foundation capable of withstanding the dimensional movements of solid wood. The primer risks superficially hardening a layer without cohesion that will eventually split under the parquet due to seasonal shrinkage. Mechanical abrasion by sanding remains a mandatory and unavoidable step.
What type of vacuum cleaner must be connected to the floor sander?
An industrial construction site dust extractor equipped with an automatic filter cleaning system and fine mineral dust filtration is essential. The suction must operate directly on the guard of the parquet sander or heavy single-disc machine during abrasion. The use of a simple construction broom is strictly forbidden, as it redeposits milky dust into the open micropores of the screed and ruins the adhesion of the primer.
Which primer should be chosen under a silane adhesive on calcium sulphate?
On an anhydrite screed free of laitance, a modified silane polymer-based adhesive can be applied without a primer if expressly authorised by the manufacturer. However, in the event of heterogeneous porosity or slight underlying powdering after sanding, apply a solvent-free polyurethane or acrylic primer approved by the adhesive manufacturer. Scrupulously respect the drying time before beginning the bonding of the parquet boards.
Texts and standards cited
- SIA 253Installation of bonded floor coverings and mineral substrate preparation requirements