Skip to content
Website
🧱 CFC 211.1Section 6 of 610 chapters

Reinforced concrete defects, diagnosis and strengthening: standard

Intended for site managers, site foremen and team leaders, this section covers structural defects in ageing reinforced concrete. It deals with the analysis of alterations, from carbonation to corroded reinforcement, and details proven non-destructive investigation methods as well as heavy strengthening techniques using bonded composites or resin injections, in compliance with SIA 262 and SIA 269 standards.

  • 10chapters
  • 22 000words
  • 6sections in the training course
  • 60chapters in total

Key values to remember 4

norme SIA 262

pH < 9

pH threshold leading to complete depassivation of non-prestressed reinforcement

norme SIA 262

0.2 mm

Limiting crack width in standard exposure classes without waterproofing

norme SIA 269

1.5 MPa

Minimum surface tensile strength of concrete for bonding carbon strips

norme SIA 262

100 bar

Minimum pressure for removing surface laitance prior to strengthening

Technical scope: integrity diagnosis and framework strengthening

This section covers exclusively integrity diagnosis, mechanical behaviour and structural strengthening operations on existing reinforced concrete building frameworks. The scope encompasses chemical and physical degradations that compromise the strength of slabs, load-bearing walls, structural beams and pillars: neutralisation front, corrosion with loss of steel cross-section, internal expansive reactions or defects resulting from unforeseen overloads.

Supervision of alteration construction sites requires complete mastery of technical responsibilities. When hacking out contaminated concrete or sawing delaminated elements, compliance with accepted technical rules is imperative to guarantee the temporary stability of the structure. Any negligence in propping or demolition may incur criminal liability on the construction site under art. 229 CP in the event of endangering third parties.

  • Accurate identification of degradation causes: carbonation, chloride ion attack and alkali-aggregate reaction.
  • Strict technical distinction between minor passive cracking and progressive structural defects.
  • Non-destructive testing techniques to locate reinforcement and map defects without weakening the supports.
  • Execution methodology for strengthening using composite materials and structural resin injections.

Methodological organisation: from inspection to load transfer

The assessment and rehabilitation of a deteriorated structure cannot be improvised under the pressure of the construction site schedule. To intervene effectively and without compromising the stability of the building, supervisory teams must follow a rigorous procedure that systematically begins with in-situ chemical and mechanical analysis before any corrective action.

  1. Understanding physical and chemical alteration processesChapters [A6-01] to [A6-03] break down binder neutralisation, spalling of concrete covers due to steel oxidation and swelling linked to alkali-aggregate reactions, in order to identify the exact kinetics of potential collapse.
  2. Characterising defects and inspecting the existing structureChapters [A6-04], [A6-08] and [A6-09] make it possible to distinguish the origin of cracks, probe residual cross-sections using high-frequency radar and draw up a load-bearing capacity assessment prior to any load modification.
  3. Implementing curative techniques and strengtheningChapters [A6-05] to [A6-07] guide heavy works: selective hydrodemolition preserving sound reinforcement, consolidation by epoxy resin pressure injection and bonded tensioning of carbon fibre strips.
  4. Ensuring the final durability of the rehabilitated assemblyChapter [A6-10] concludes the approach by detailing the mineral or organic surface protections essential to definitively stop the penetration of further aggressive agents.

📘 Chapters in this section 10

Pathologies of reinforced concrete, diagnosis and strengthening

Concrete carbonation: mechanism, depth measurement and consequences

Measure the carbonation front down to the millimetre to halt corrosion before the first defects appear.

Pathologies of reinforced concrete, diagnosis and strengthening

Reinforcement corrosion: from rust stains to cover spalling

Anticipate rust expansion to save steel cross-sections before concrete spalls.

Pathologies of reinforced concrete, diagnosis and strengthening

Alkali-aggregate reaction: characteristic crazing, diagnosis and next steps

Detect the first networks of expansive microcracks to manage alkali-aggregate reactions without panicking.

Pathologies of reinforced concrete, diagnosis and strengthening

Structural or surface crack: distinguish them before raising alarm

Identify the mechanical or thermal origin of an opening to act solely on structural defects.

Pathologies of reinforced concrete, diagnosis and strengthening

Injecting a crack: resin selection, injector installation, and inspection

Restore the monolithic load-bearing capacity of a cracked component through perfectly controlled pressure injection.

Pathologies of reinforced concrete, diagnosis and strengthening

Strengthening with bonded carbon laminate: substrate preparation and bonding

Increase the tensile load-bearing capacity of slabs without added thickness using composite strips.

Pathologies of reinforced concrete, diagnosis and strengthening

Hydrodemolition: purge degraded concrete without damaging sound rebar

Remove contaminated concrete at very high pressure without cracking the substrate or bending the reinforcement.

Pathologies of reinforced concrete, diagnosis and strengthening

Non-destructive testing of a structure: radar, ferroscan and test pits

Map the location of reinforcement bars and internal voids without any destructive coring into the element.

Pathologies of reinforced concrete, diagnosis and strengthening

Assessing load-bearing capacity of an existing structure prior to transformation

Scientifically verify the permissible load of an older floor slab before any core drilling or change of use.

Pathologies of reinforced concrete, diagnosis and strengthening

Protecting a concrete surface: water repellent, anti-carbonation and maintenance

Apply the appropriate protective system to definitively block CO2 and residual moisture.