Treating joints: paper tape, three-coat filler and internal corners

This chapter details the installation rules for treating flat joints and internal corners on plasterboard in accordance with SIA 242. You will master bedding the paper tape, the three-coat application cycle and strict compliance with the drying times between coats, to prevent any structural cracking or later detachment.

Key takeaways

  • Micro-perforated paper tape offers far greater mechanical strength than self-adhesive mesh tape.
  • Embedding the tape requires the recess to be filled completely, leaving no air void.
  • Observing the drying times between the three coats determines the final mechanical stability.
  • Treating internal corners requires a clean axial fold of the tape and two carefully applied coats.

Embedded paper tape ensures mechanical strength against deformation

On dry-construction sites in French-speaking Switzerland, the treatment of connections between plasterboards is governed by the requirements of SIA 242 (Plastering, rendering, dry construction). Although self-adhesive mesh tape is sometimes attractive because it appears quick to apply, its use remains prohibited on works subject to slight expansion or to structural stresses, particularly in internal corners. Self-adhesive glass-fibre mesh is too elastic and its thickness hinders coating. Under the tension exerted by differential movements of the structural work or by the thermo-hygrometric variations of the metal profiles, the mesh stretches and the filler cracks at its core.

Conversely, paper joint tape has a considerably higher longitudinal and transverse tensile strength when it is correctly embedded in a filler matrix. Standard paper tape has a surface sanding that improves mechanical grip and a central groove that makes it easier to fold into a right angle. Micro-perforated to release air trapped during pressing, it forms an inseparable composite with the compound once hardened. Under art. 364 CO, the contractor is liable for the proper and faithful execution of the work entrusted to them; using an unsuitable tape that fails at the first movements of the building directly engages their contractual liability.

Technical comparison of joint reinforcements
CharacteristicMicro-perforated paper tapeSelf-adhesive mesh tape
Tensile strengthHigh (rigid behaviour under stress)Low (notable elastic elongation)
Suitability for internal cornersOptimal thanks to the factory-made mechanical foldNon-compliant (systematic risk of voids)
Application methodEmbedded in a bed of bonding compoundStuck dry onto the plasterboard facing
Risk of later crackingVery low with full dryingHigh during differential shrinkage

Three-coat method and rigorous execution of the internal corner

Treating a joint between tapered-edge boards requires three distinct successive operations that the dry-lining installer must never merge or shorten. Skipping a coat or applying a coat over still-damp compound is the primary cause of hollow shrinkage, blistering and rejection at acceptance of the finished surfaces under the criteria of SIA 242.

  1. Coat 1: Filling and bedding the tapeApply a generous bed of compound to the bevel with a 150 mm filling knife, filling the bottom of the joint. Apply the paper tape, sanded face against the plaster, centring it exactly on the axis. Press the tape with the blade inclined at 45 degrees to expel excess material and air bubbles, while leaving a regular thickness of compound of about 1 mm under the paper.
  2. Coat 2: Second filling coatAfter the first coat has dried completely, apply a layer of filling compound with a 200 to 250 mm blade. This coat compensates for the slight hydraulic shrinkage of the binder and covers the edges of the tape to restore flatness between the cardboard facings of the boards.
  3. Coat 3: Finishing and skimAfter hardening and complete evaporation of the free water from the second coat, apply a thin finishing compound with a trowel or a 300 mm knife. Remove burrs from the ridges without digging into the material. The total width of the finished joint thus reaches 300 to 350 mm.

In an internal corner formed by two dry partitions or between a partition and a ceiling, the embedding method is adapted accordingly. The paper tape is first folded along its central crease, with the edge towards the inside. After filling both faces of the corner right to the end over a width of 100 mm with a corner tool or a straight knife, the folded tape is positioned at the bottom of the angle. Pressing is carried out one side after the other, working from the centre towards the ends to avoid any creasing of the paper.

When finishing an internal corner, it is forbidden to load both sides simultaneously during the finishing coat unless you have the required skill with a dedicated corner tool. Treat one side first, let it dry perfectly, then finish the second side the next day. This procedure avoids cutting into the opposite fresh compound with the corner of the tool and guarantees a perfectly straight edge before handover to the painter.

Thermo-hygrometric conditions and drying kinetics on the construction site

Treating joints and internal corners in plasterboard tolerates no shortcuts in the programme. On construction sites in French-speaking Switzerland, the mechanical success of a joint reinforced with paper tape depends directly on the evaporation of the mixing or dispersion water. According to the rules of the trade and the application guidelines of SIA 242, jointing work must never be started when the ambient and substrate temperature falls below 10 °C, or when the relative air humidity exceeds 70 %. If these thresholds are not respected, the water remains trapped in the binder, blocking the crystallisation of setting compounds or delaying indefinitely the coalescence of drying compounds.

The choice between a chemically setting powder compound and a ready-mixed paste compound determines how the team organises itself on the slab. A quick-setting compound makes it possible to fix the paper tape and fill hollows within a few hours, but it demands perfect control of mixing to avoid trapping air bubbles. Conversely, a physically drying compound requires controlled shrinkage volume and a rigorous waiting time of at least one full day before any overcoating, otherwise a damp film is trapped under the finishing coat.

Behaviour of binders for joint tapes according to the application phases
Type of compoundHardening mechanismTime between coats (at 20 °C and 50 % RH)Sensitivity in internal corners
Setting powder (additive-modified plaster base)Rapid chemical crystallisation2 to 4 hours depending on the specified setting timeVery low mechanical shrinkage; excellent holding of the central fold
Ready-mixed paste (resin base)Water evaporation (physical drying)12 to 24 hours per coat appliedMarked shrinkage on drying; risk of hollowing if the coat is too thick
Mixed slow-setting compoundProgressive crystallisation and drying6 to 8 hours depending on ventilationGood compromise for large surfaces without acute thermal stress

Internal corners, SIA 242 quality levels and prevention of defects

In an internal corner formed by two dry partitions or at the junction of a suspended ceiling, the differential movements of the structure stress the connection in shear and tension. Self-adhesive glass-fibre mesh tape is prohibited in this configuration: its open mesh cannot withstand angular stresses and lets micro-cracks through at the first expansion of the metal framework. Only micro-perforated kraft paper tape, folded precisely along its factory crease, provides the transverse cohesion needed to absorb the micro-rotations of the corner without tearing.

To achieve the internal corner at the agreed finish level, the fitter loads each face of the angle generously with a 100 mm knife or a wheeled corner applicator. The folded paper tape is inserted into the sharp edge, then pressed firmly from the centre towards the edges with a right-angle corner tool or a flexible blade inclined at 45 degrees. This mechanical pressing must expel the excess compound without drying out the interface: a uniform film of at least 1 mm of compound must remain trapped under the paper to guarantee permanent adhesion.

After the bedding coat has dried completely, the dry-lining plasterer carries out the filling coat on one face of the corner, leaving the edge free to avoid tearing off the fresh compound on the adjacent side. Only after this coat has hardened is the second face coated, using a trowel or a 150 mm smoothing blade. The final fine-grit sanding is carried out by hand or with an orbital sander fitted with suitable dust extraction, taking care never to damage the protective fibre of the paper tape on the corner edge.

Diagnosis and repair of defects on joints and internal corners

On a dry-lining construction site, jointing-related failures almost always stem from two execution faults: a lack of material behind the paper causing blisters, or loading too early before the bedding coat has dried completely. In an internal corner, the improper use of self-adhesive mesh tape invariably results in a straight crack at the building's first structural movement. When the defect appears before acceptance of the work under SIA 242, the team must intervene without adding parasitic thicknesses that would degrade local flatness.

  1. Open and probe the blisterUsing a trapezoidal-blade cutter, cut the blister at the centre of the detached area, following the grain of the paper tape. Gently lift the edges to check for dry or powdery compound on the underside.
  2. Clear out and re-bond under the reinforcementRemove the dehydrated, non-adherent compound. Inject fresh joint compound of soft consistency directly behind the paper with a corner knife or a narrow spatula, then press the tape firmly to expel surplus air and compound.
  3. Treating an internal corner crackIf a mesh tape has failed at the ceiling-partition junction, cut out the failed reinforcement along its entire length. Clean the edge, re-inject a quick-setting adhesive compound, then embed a genuine paper tape folded along its mechanical axis before repeating the coats.
  4. Refill and respect the drying sequenceAfter the repair has dried completely, apply a widened finishing coat with a smoothing blade of at least 300 mm to feather out the extra thickness. Allow the compound to harden for 24 hours before any hand sanding with fine grit.

In the case of marked shrinkage caused by excessive humidity in the building during application, the compound hollows along the joint axis. The team leader then applies a levelling coat of stiff consistency, without trying to fill the hollow in a single pass. The requirements of SIA 242 impose strict flatness criteria that prohibit any visible flashing under raking light, particularly at the higher finish levels Q3 or Q4.

Frequently asked questions

Can a paper tape that is blistering be repaired without having to tear it off completely?

Yes, if the detachment remains localised. Simply cut the blister lengthwise with a cutter, open the edges slightly to work in fresh joint compound of fluid consistency, then re-press the tape with a stainless-steel spatula to expel the air. If the blister extends over more than 50 centimetres continuously, complete removal and replacement of the section is required.

Why is self-adhesive mesh tape prohibited in internal corners?

Glass-fibre mesh tape has an open weave that lets the compound pass through without creating a continuous, tear-proof plane. In an internal corner subjected to differential micro-movements between walls or under a ceiling, the mesh offers no resistance to shear. Factory-folded paper tape, on the other hand, provides a continuous mechanical hinge that absorbs stresses without the edge failing.

How long should you wait between the bedding coat and the finishing coat on an unheated construction site?

On a cold or damp construction site, drying compound evaporates its water very slowly. Allow a minimum of 24 to 48 hours between coats. Applying a finishing coat over a still-fresh bedding coat blocks the residual evaporation, weakens the mechanical strength of the assembly and later produces visible shrinkage as a hollow along the plasterboard facing.

How do you get a straight internal corner without soiling the adjacent board?

The professional method is to work one face at a time. After folding and embedding the paper tape in the compound on both sides, load and smooth the first wall completely with the filling knife. Let this first coat harden fully before tackling the adjacent face. This avoids catching the opposite facing with the metal edge of the blade while pulling the compound.

Texts and standards cited

  • SIA 242Plastering, rendering, dry construction: flatness requirements, execution tolerances and surface quality levels Q1 to Q4.

In the same section