Skip to content
Website
🧱 CFC 411Low walls, retaining structures and external stairsChapter 8 of 10 in the section

Long wall: expansion joint, regular vertical crack and joint position

Thermal stresses and hydraulic shrinkage cause unavoidable vertical cracks in continuous landscape masonry. In this chapter, you will learn how to calculate the optimal joint spacing according to SIA 318, position each expansion joint at singular points along the alignment, and execute watertight and durable finishes.

Key takeaways

  • External temperature variations and shrinkage require joints every five to eight metres.
  • Standard SIA 318 governs tolerances and dimensional behaviour in external masonry.
  • A through-joint must cut through the wall and its coping without interrupting the footing.
  • Joint sealing combines a closed-cell backing cord and an elastomeric sealant compatible with the facing.

Understanding thermal movements and determining regulatory spacing

An external landscaping wall is directly exposed to the climatic temperature ranges of the Swiss Plateau and the Jura or Alpine foothills. In summer, a south-facing facade regularly reaches fifty degrees under direct solar radiation, while winter frost frequently drops below minus ten degrees. This external thermal variation, with an amplitude of over sixty kelvins, generates permanent cycles of expansion and contraction. Added to these cyclical movements is the irreversible hydraulic shrinkage of the binder during the first few months after pouring the infill concrete or laying manufactured concrete blocks.

In the absence of a clean break, the wall is restrained by its base anchored to the unreinforced or lightly reinforced concrete foundation footing. Since the tensile strength of masonry or unreinforced concrete remains modest, the accumulated tensile stress quickly exceeds the mechanical capacity of the material. The release of tension then manifests as a clean, vertical, through-going crack appearing at regular intervals along the linear structure.

External works in masonry and concrete must be designed to absorb dimensional variations caused by thermal influences, moisture, and the behavior of component materials without damage.

Norme SIA 318
Permissible intervals for expansion joints according to the type of facing
Type of elevation materialDirect solar exposureRecommended maximum spacingNominal width of the gap
Cast-in-place concrete (unreinforced low wall)Due south or west5 to 6 metres15 to 20 millimetres
Cast-in-place concrete (reinforced low wall)Shaded or north-facing6 to 8 metres15 millimetres
Rendered manufactured concrete blocksAll exposures6 metres15 millimetres
Mortared natural stone masonryDue south or south-west6 to 7 metres15 to 20 millimetres

Positioning the joint on the alignment and achieving a watertight finish

The layout of an expansion joint is not done in a purely arithmetic manner. The team leader or site foreman must prioritize aligning the mechanical breaks with the natural weak points of the longitudinal profile. Every foundation step, level change, internal or external corner, and every abrupt change in elevation height concentrates fracture lines. Placing a clean joint at these singularities neutralizes shearing before an erratic crack tears the render or shatters the block edges.

  1. Complete decoupling of the elevationInstall a rot-proof compressible panel made of extruded polyethylene foam or dense mineral wool across the entire thickness of the wall. The break must be total across the elevation without interruption from one facing to the other.
  2. Maintaining foundation continuityThe strip footing in blinding or foundation concrete remains continuous in the absence of differential ground settlement. It acts as a horizontal guide and does not receive a through-joint, except when crossing heterogeneous backfill.
  3. Installation of joint backing and adhesion controlInsert a round closed-cell polyethylene foam backing cord into the base of the groove, with a diameter twenty-five percent greater than the width of the joint. This joint backing prevents the sealant from adhering on three faces.
  4. Application of the finishing elastomeric sealantExtrude a polyurethane or polymer hybrid sealant approved for exterior masonry. The optimum application ratio requires a joint depth equivalent to half the joint width, smoothed flush.

On the rear side of the low wall, in contact with the backfill soil, protection against infiltration requires equal vigilance. The expansion joint must be bridged at the back by a flexible waterproofing strip or a heavily anchored non-woven geotextile, in order to prevent fine particles from entering the empty gap. If sand or gravel infiltrates the expansion void, the joint jams during summer expansion, shifting the compressive stresses towards the visible facing and shattering the masonry facings.

Joint continuity: from foundation footing to coping

In external works under CFC 411, the most frequent mistake consists in interrupting the elevation of a wall without uncoupling its base, or conversely in pouring a continuous coping over an elevation break. Standard SIA 318 reminds us that stresses induced by external thermal variation and hydraulic shrinkage act on the entire structural section. A functional expansion joint must cross the entire visible height of the structure without any mechanical blockage point.

  1. Management of unreinforced or lightly reinforced concrete foundationsFor a low garden retaining wall on a shallow strip footing, the foundation is poured in successive bays delimited by edge boards or a high-density expanded polystyrene panel. If the footing remains continuous on homogeneous soil, a break starter is created by partial sawing or by placing a dry joint aligned exactly with the future vertical joint of the elevation.
  2. Installation of the compressible strip in the elevationThe interlayer material, consisting of a 15 to 20 mm rot-proof closed-cell foam strip, is inserted during the laying of the courses or fixed against the stop formwork. It prevents any hard stone-on-stone or concrete-on-stone contact which would generate spalling during the very first phase of summer expansion.
  3. Clean sectioning of coping elementsPrefabricated copings, head slabs, or sandstone flashings must imperatively be sawn or interrupted along the strict vertical axis of the joint. Filling this upper gap with hard mortar cancels the expansion effect and shifts the bending stress to the last course of the facing.
  4. Connection of the rear drainage systemAt the rear of the wall, the geotextile filter strip and the studded geomembrane must be laid with a loose overlap without tension at the joint. Rolled 16/32 drainage gravel must not insinuate itself into the slot: the upstream face of the break is protected by a flexible bituminous or EPDM flap dry-pressed into place.

Execution according to materials and tolerance rules

The behaviour of an external wall subjected to temperature differences sometimes reaching 50 °C between winter and direct solar exposure heavily depends on its construction method. The criteria of standard SIA 318 require adapting the frequency and caulking method depending on whether cement concrete blocks, cast-in-place formwork blocks, or assembled riprap modules are being built.

Execution characteristics of expansion joints according to the type of low landscaping wall
Type of wall (CFC 411)Recommended spacingInterlayer materialVisible treatment of the joint
Solid or hollow concrete block masonry6 to 8 m in the sun, max. 10 m in the shadeClosed-cell expanded polyethylene panelPE cord joint backing and elastomeric polyurethane sealant
Exposed aggregate or unrendered cast-in-place low wall5 to 6 mRot-proof compressible strip inserted before pouring15 mm clean recessed joint with peripheral chamfer
Dry-stacked dressed natural stone low wall10 to 12 m (or self-compensated)No rigid binder (free movement of blocks)Vertical butt joint set without concealed mortar
Dry-stacked modular retaining blocks8 to 10 mInterruption of continuity for keys or interlocking featuresMatched finishing profile or reserved free space

To guarantee the watertightness and aesthetics of the elastomeric sealant on the facade, applying the sealant requires a rigorous method. Clean the joint lips with a wire brush and then compressed air to remove any sawing dust. Inserting a calibrated round foam joint backing cord, compressed by about 25%, ensures the shape factor is respected: the depth of the sealant must equal half its width so that it works in pure tension rather than triaxial adhesion.

Pathologies of the long wall: diagnosis of a crack and corrective measures

On an external landscaping structure, the appearance of a clean vertical crack running through the entire height of a low wall almost systematically indicates the absence or blocking of an expansion joint. Faced with this defect, the team leader or site foreman must carry out a precise diagnosis before any intervention: does the crack result from initial hydraulic shrinkage or recurring seasonal thermal variation? In the cantons of western Switzerland, temperature differences between winter frost and direct summer radiation on the masonry generate considerable elongation and shortening stresses. When the spacing recommended by standard SIA 318 has not been respected, the masonry creates its own plane of rupture.

  1. Installing gauges and monitoringInstall millimeter gauges or plaster patches across the crack to measure its range of movement over several weeks and check for the absence of differential settlement in the foundation soil.
  2. Creating a relief joint by mechanical sawingIf the wall is restrained, vertically cut the element with a diamond disc saw to create a continuous straight void of 15 to 20 mm, also cutting through the coping or capping.
  3. Cleaning and repairing cut lipsClear debris with a wire brush and compressed air, remove friable edges, and patch the side walls with repair mortar if necessary to obtain parallel flanks.
  4. Flexible caulking and waterproofingInsert a cellular backing in extruded polyethylene to ensure adhesion on two faces only, then apply a weather-resistant polyurethane elastomeric sealant.

In the event of water infiltration from the rear of the structure, the backfill drainage must be inspected. The accumulation of water behind a low wall worsens the opening of cracks under the effect of frost. Underpinning or drilling drainage weep holes helps relieve hydrostatic pressure before finalizing the flexible repair of the joint.

Frequently asked questions

How to differentiate a thermal crack from foundation settlement?

A thermal crack is vertical, straight, runs through the entire height of the wall without horizontal offsets, and opens wider in winter than in summer due to the cold. A settlement crack is generally oblique or stepped, follows the masonry bed joints, and widens upwards or downwards depending on the tilting of the footing. A millimeter gauge confirms the mechanism over a complete climatic cycle.

Can an expansion joint be concealed behind a decorative facing?

No. The expansion joint must pass through the entire structure, from the foundation footing to the coping, including all facing and cladding elements. If a continuous facing of slips or stones covers the joint, the thermal stress exerted by the body of the wall will crack the cladding erratically. The joint must be replicated exactly in alignment within the facade cladding.

Why does a south-facing wall require closer joint spacing?

A south-facing wall experiences an extreme temperature range. In summer, direct radiation raises the mineral surface temperature to over fifty degrees, while in winter, night-time temperatures drop below zero. This thermal variation amplifies the dimensional expansions and contractions of the material. Bringing the expansion joints closer together at intervals of five to eight metres limits the amplitude of movement absorbed by each individual joint.

What to do if the coping blocks crack above the wall?

Failure of the coping indicates that the expansion joint in the wall body has not been extended into the coping. The fractured elements must be dismantled, a clean cut sawn in alignment with the vertical joint of the wall, the blocks relaid on a mortar bed with an inserted compressible strip, and the resulting void filled with a joint backing and a watertight elastomeric polyurethane sealant.

Texts and standards cited

  • norme SIA 318External works: design requirements, tolerances, and execution of masonry structures and low retaining walls
  • norme SIA 118General conditions for the execution of construction works and management of structural defects

In the same section