Skip to content
Website
🧱 CFC 273Claddings, skirting boards and parquet installationChapter 9 of 10 in the section

Laminate flooring: use class, plank locking and what sets it apart from wood

Laminate flooring must never be confused with traditional parquet. Having no noble wood wear layer, it cannot be sanded afterwards and requires its use class to be strictly matched to the loads in the room. This chapter guides you through product selection, mastery of the locking systems and the management of clearances in accordance with standard SIA 343.

Key takeaways

  • The melamine wear layer makes any sanding or surface renovation technically impossible.
  • The use class determines the resistance of the board to indentation and to the foreseeable traffic.
  • Mechanical click-locking ensures tight edges and cohesion without any gluing.
  • Standard SIA 343 governs the clearances under doors to guarantee the movement of the floating floor.

Distinguishing laminate from wood and choosing the use class suited to the room

In the practice of the interior joiner, calling a laminate covering a parquet is a technical error. A parquet necessarily has a wear layer of noble wood at least two and a half millimetres thick, which allows heavy maintenance operations to be entrusted to flooring specialists. Laminate flooring consists of a central core of high-density wood fibre (HDF board), covered with a decorative paper printed under high pressure and protected by a melamine resin film loaded with corundum, called the overlay. This transparent protective film gives a high surface hardness but a very thin wear thickness.

Since the material does not regenerate, the durability of the floor depends on the initial choice of the use class. Manufacturers classify coverings according to a two-digit system combined with an abrasion resistance index. The first digit identifies the intended use of the room (digit 2 for private housing, digit 3 for commercial premises and buildings open to the public), while the second quantifies the intensity of traffic (1 for moderate, 2 for medium, 3 for heavy, 4 for very heavy). Poor sizing leads to premature wear of the overlay in corridors, in chair pivoting areas or at accesses to the outside.

Use classification of laminate floors and usual fields of application
Use classAbrasion indexLoad levelTypical rooms in French-speaking Switzerland
Class 23AC3High residentialMaster bedrooms, private living rooms, upper-floor circulation areas without direct access
Class 31AC3 or AC4Moderate commercialHotel rooms, small individual offices, staff rest rooms
Class 32AC4Medium commercialOpen-plan offices, medical practices, classrooms, residence lobbies
Class 33AC5Heavy commercialRetail shops, corridors of administrative buildings, meeting rooms
Class 34AC6Very high commercialMultipurpose spaces, public counters, reception areas with heavy continuous flow

Adjoining doors and floor coverings must have operating clearances compatible with the dimensional variations of the elements under the ambient thermo-hygrometric conditions.

norme SIA 343

Click-locking mechanisms and coordination of floating-installation interfaces

Laminate flooring is always installed in the floating manner, without full-surface bonding to the mineral or wooden substrate. The transmission of horizontal stresses and the flatness of the surface depend on the profiling of the edges machined in the HDF board. Current joints use patented locking mechanisms that eliminate the use of glue in the tongues and grooves, ensuring a clean, demountable joint that can be walked on immediately.

Fold-down locking system (5G or Fold-Down)
Joining mechanism in which the plank is inserted along the long side at a defined angle, then folded down vertically onto the adjacent short side. An elastic tongue integrated at the end of the plank clicks in automatically under pressure, preventing any vertical misalignment without the need for horizontal tapping.
  1. Preparation of the substrate and vapour barrierCheck the flatness of the substrate under a two-metre straightedge. Lay a polyethylene film at least two tenths of a millimetre thick with a twenty-centimetre overlap sealed with adhesive tape over any mineral screed to cut off rising residual moisture.
  2. Laying the acoustic underlayLay a compressible underlay specific to laminate floors to reduce footstep and impact noise. Prefer a high-density material to avoid settling under the click zones during the repeated passage of rolling loads.
  3. Longitudinal engagement and end clickingEngage the long edge at an angle of about twenty to thirty degrees in the groove of the previous row. Push forward then fold down towards the floor to lock the joint, making sure to stagger the end joints by at least thirty centimetres between two consecutive rows.
  4. Perimeter expansion gaps and clearances under doorsPlace spacers of eight to ten millimetres against all vertical elements (walls, door frames, pipework). In accordance with the requirements of standard SIA 343, trim the bottom of the door frame jambs and adjust the clearance under the door leaves to preserve the free movement of the assembly.

Overlay degradation and impossibility of renovation: technical limits compared with wood

Laminate flooring gets its surface resistance from an upper impregnation film called the overlay, made of a melamine resin loaded with aluminium oxide (corundum) particles. This transparent sheet protects a printed paper sheet reproducing the wood grain, itself pressed onto a high-density fibreboard (HDF) core. Unlike a solid or multilayer parquet, whose noble wood facing tolerates several passes of the parquet sander, laminate has a micrometre-scale wear reserve. Any mechanical sanding, even superficial, instantly goes through the melamine resin, destroys the printed decor and exposes the HDF core, making the element unsalvageable.

Severe mechanical loads produce forms of degradation entirely different from those of wood. Under the impact of a heavy or pointed object, the overlay does not undergo elastic or plastic compression that can be reversed by thermal wetting, but a brittle fracture. The melamine resin chips, exposing the core of the board. From that moment, ambient humidity or cleaning water infiltrates the compressed wood fibres of the core, causing irreversible localised swelling and chipping of the edge lips.

Comparative behaviour of laminate floor and wood parquet in the event of surface damage
Degradation criterionLaminate covering (CFC 273)Multilayer or solid parquet
Surface scratchLocalised whitening of the melamine resin, irreversible without a specific filler productScratch in the varnish or oil, repairable by local light sanding or re-oiling with care oil
Deep point impactChipping of the overlay and exposure of the HDF substrate; risk of swelling starting with waterDenting of the wood fibre without systematic loss of material; can be raised with heat
Continuous abrasion wearLoss of the protective film, loss of the printed pattern, exposure of the brown boardStripping of the finish, patina of the wood, wood material preserved over the full thickness
Restoration optionSurface renovation impossible: complete replacement of the damaged plankComplete sanding of the facing, application of a new varnish or impregnation

Replacing a trapped plank and coordination at thresholds in accordance with standard SIA 343

Since the surface cannot be renovated, a plank that is badly damaged must be replaced individually. When the plank is located in the middle of a large floating surface, complete dismantling from the last edge would pose a high risk of breaking the locking tongues. The joiner then uses a precise extraction method with a plunge-cut circular saw fitted with a guide rail and set exactly to the thickness of the plank, so as to spare the vapour barrier film and the resilient underlay beneath.

  1. Cutting out and extracting the damaged plankMake two longitudinal cuts about 15 mm from the inner edges of the plank to be replaced, completed by two triangular cuts at the ends. Remove the trapezoidal central piece, then carefully release the remaining side strips from the adjacent locking profiles using a short lever.
  2. Preparing the replacement plankOn the new plank from the site's reserve batch, carefully trim off, with a well-sharpened wood chisel or a router, the lower lip of the longitudinal groove and the shoulder of the end lock. This operation removes the mechanical clip, which can no longer be engaged by tilting.
  3. Gluing and catch-up lockingApply a calibrated bead of class D3 vinyl wood glue to the receiving grooves and tongues of the existing floor. Insert the intact longitudinal tongue of the new plank into the adjacent groove, then lay the plank down flat. Place a load of at least 20 kg spread over the piece while the glue sets.

Connections at interior doors must be carefully coordinated by the joiner. Standard SIA 343 defines the functional requirements for interior doors and closures, in particular the air clearances needed at the bottom of the leaf to guarantee free swing and air circulation without rubbing on the finished covering. Since laminate flooring must be installed decoupled from the building structure, it must be able to slide freely under the door frame or the casing.

Where a door opening is crossed, continuity of the floating covering from one room to the next is to be avoided whenever the rooms have different occupancy patterns or different areas. The expansion joint under the door leaf must be concealed by a threshold profile mechanically fixed into the underlying screed, making sure that the screws pass through the laminate without ever restraining it, thus maintaining the independence of movement of each laid field.

Managing defects on laminate floors: diagnosis and repair methods

On a laminate floor, any mechanical or water-related defect quickly leads to a dead end if it is treated like a traditional parquet. As soon as the protective overlay has been broken through by a point impact or water infiltration has caused the edges of the HDF board to swell, no remedy by sanding, filling or varnishing is possible. Melamine resin does not regenerate, and the compressed wood fibre core, once swollen by moisture, never regains its original thickness after drying.

When planks open or lift in the centre of the room, the joiner must first check the freedom of movement of the floating floor. Standard SIA 343 prescribes clear perimeter clearances along partitions, under skirting boards and at door frames. If a rigid fixing, a forgotten wedge or the excessive tightening of a door stop blocks the expansion, the whole floor buckles under hygrothermal variations. In this situation, the repair consists of removing the skirting boards, trimming the perimeter with a plunge saw with dust extraction to restore the necessary clearance, then re-clicking the detached rows.

  • In the case of irreparable local damage, dismantling is carried out in the reverse order of installation from the nearest wall, tilting the planks to release the mechanical lock without breaking the click profiles.
  • For an isolated plank in the middle of a large area, cutting out the defective piece with a router allows its extraction, followed by partial trimming of the lower tongue of the replacement plank and targeted gluing with polyurethane glue.
  • If the swelling results from a burst pipe or a damp screed, the entire floating assembly and the vapour-barrier underlay must be removed to allow the technical drying of the structural work in accordance with the rules of the art of finishing work.

Frequently asked questions

Can a surface chip on a laminate plank be repaired without replacing the element?

An isolated chip in the overlay can be filled with a hard, hot-melt wax tinted throughout, applied with a cabinetmaker's melting iron. This cosmetic treatment seals the decor to prevent dust and moisture from penetrating the HDF board. However, this local touch-up remains visible in raking light and does not restore the original mechanical resistance of the wear film under intensive traffic.

What should be done if the longitudinal joints of the laminate lift after the first winter?

This cupping of the edges generally indicates excessive moisture in the substrate or the absence of a perimeter expansion joint. First check that the clearance under the skirting boards is effective all around, in accordance with the recommendations of standard SIA 343. If the floor butts against a partition or a door casing, trim the edge with a plunge saw. If the board has taken on water through excessive washing, the deformed planks must be replaced.

Which use class should be installed in a professional office subject to the rolling of castor chairs?

For an administrative room or a work area with sustained traffic, specify at least use class 32, ideally class 33. These classifications guarantee a corundum-enriched overlay that resists wear from circular abrasion. The combined use of type W castors suited to hard floor coverings and an underlay with high compressive strength prevents premature degradation of the click mechanism under repeated dynamic loads.

Why is it out of the question to sand a dulled laminate floor in order to apply a varnish?

Unlike solid wood or laminated wood with a noble facing of at least 2.5 millimetres, laminate has no real wood thickness at the surface. The visible layer is only a decorative sheet impregnated with melamine resin covering a board of compressed fibres. Passing a sander over it would instantly destroy the decorative pattern by exposing the HDF substrate, rendering the floor unusable. No varnish can adhere durably to a worn, glazed overlay.

Texts and standards cited

  • SIA 343Doors and closures: coordination of installation clearances, threshold interfaces and floor connection tolerances

In the same section