Skip to content
Website
🧱 CFC 273Interior doors: installation, clearances and adjustmentChapter 7 of 10 in the section

Moisture attacks the bottom: bathroom door, lower edge and swelling core

After this chapter, you will be able to specify and fit interior door sets that are resistant to water splashes and to the humid atmosphere of bathrooms. You will master the resealing of a cut bottom edge, the choice of water-repellent cores and facings in accordance with SIA 343, and the precise sizing of the undercut gap required for the airflow of mechanical ventilation.

Key takeaways

  • Every cut made to trim a door to length requires immediate, watertight sealing of the planed bottom edge.
  • SIA 343 classifies the humidity loads that require cores and facings stabilised against swelling.
  • The undercut beneath the leaf ensures the extract airflow without creating a zone of standing water.
  • Cardboard honeycomb cores are strictly to be avoided in favour of solid, water-repellent treated, waterproof panels.

Capillary infiltration and the selection of components in accordance with SIA 343

In a bathroom, the premature deterioration of an interior door invariably begins at the underside of the leaf. Water splashed during showers, condensation moisture running down smooth walls and water from washing tiled floors migrate by capillary action directly into the end grain or the wood-based panels. Without airtight protection, the fibres swell irreversibly, causing veneered edges to burst, laminated or painted finishes to blister and, in the end, the leaf to rub against the threshold.

Behaviour of door leaf constructions in a bathroom's humidity
Core typeUsual facingBehaviour at the bottom edgeCFC 273 recommendation
Honeycomb (cardboard)Standard pre-painted MDFImmediate wicking, delamination and rapid rottingEntirely to be avoided in bathrooms
Tubular (particleboard)Standard or lacquered HDFMarked linear swelling, onset of delamination at the edgeTolerated only with factory-fitted waterproof lipping
Solid water-repellent particleboardHigh-pressure laminate (HPL)Very low swelling, excellent mechanical strengthRecommended for residential and rental premises
Waterproof composite coreCompact laminate or resinInsensitive to water and mould, dimensionally stableRequired in hospital or medico-social settings

The choice of leaf and facing assembly determines the durability of the work. High-pressure laminate facings with a minimum thickness of 0.8 mm provide a perfect shield on the faces. However, if the lower perimeter lipping is made of a soft species or is poorly impregnated, water infiltrates at the glue-to-material joint. For CFC 273 interior doors subject to frequent cleaning, lower lippings in rot-proof hardwood or rigid polymer, combined with adhesives of a suitable waterproofing class, prevent any interstitial moisture uptake.

The undercut for mechanical ventilation and the sealing of the bottom edge

The ventilation of wet rooms in modern housing relies on a controlled mechanical air flow. Fresh air supplied to the living rooms passes under the interior doors to be extracted in the bathroom. This function requires a precise undercut of the leaf. This clear gap under the door, commonly between 10 and 15 mm depending on the building's airflow balance, also protects the panel from standing water on the floor. However, trimming on the construction site exposes the core of the panel and breaks the original seal.

  1. Taking the dimension and marking out the undercutMeasure the finished clearance relative to the final floor covering (tiles or resin). Mark the cutting line on the leaf, including the ventilation clearance required by the airflow concept.
  2. Sawing and arris chamferingMake the cut with a plunge saw guided on a rail and a blade suited to preserving the facing without chipping. Always break the sharp lower edges with a slight chamfer using abrasive paper to prevent flaking.
  3. Dust removal and first impregnationVacuum up wood or resin particles thoroughly. Apply generously, by roller or brush, a first coat of two-component polyurethane resin or a fluid water-repellent sealing varnish that penetrates the porosity of the core.
  4. Final sealing and checking of the waterproof filmApply a second, cross-direction coat of the waterproofing product to form a continuous, non-porous protective film covering the core, the facings and the lipping joint. Allow it to cure before hanging on the hinges.

On new-build or refurbishment construction sites, the temptation is great to plane the bottom of a door to compensate for an extra thickness of tiling without reapplying a sealing product. This negligence exposes the core of the material to the ambient hot water vapour. An ordinary acrylic wall paint is in no way a waterproof barrier. Only products formulated for blocking the substrate in interior joinery, such as cross-linking polyurethane varnishes or hot impregnation waxes, prevent the facing from losing adhesion.

Cores and facings: composition of the leaf in the face of humidity differences

In a bathroom, the leaf is subjected to a constant asymmetric stress: hot air saturated with water vapour on the inside during showers, opposed to drier ambient air on the corridor or bedroom side. This climatic difference causes internal stresses in the panels. If the door is made with a cardboard honeycomb core or a standard particleboard panel, vapour migration causes rapid cupping and bursting of the bottom edge through capillary absorption. SIA 343 governs the requirements for interior doors, in particular their dimensional stability and mechanical strength under differing climates.

Climate class for interior doors
Standardised ability of a door leaf to retain its flatness and mechanical function when it separates two rooms with different temperature and relative humidity conditions.

To avoid warping or irreversible swelling of the core, the joiner selects leaves that meet the loads of a severe indoor climate. The central panel must imperatively show increased water resistance, while the surface facings must form a waterproof barrier against direct splashes and residual mist.

Behaviour of leaf components in a humid environment
Leaf componentStandard material (dry room)Suitable water-repellent material (bathroom)Risk in case of unsuitability
Central coreStandard cardboard honeycomb or tubular structureSolid panel of polyurethane-bonded particles or water-repellent composite coreInternal delamination, loss of squareness, irreversible swelling
Edge facingStandard 3 mm MDFHigh-density water-repellent HDF or resin compactSurface waviness, blistering of the finish film
Surface coveringLight decorative melamine paperHigh-pressure laminate (HPL) or cross-linked polyurethane lacquerVapour penetration, edges lifting on contact with splashes
Side and bottom edgesMelamine edging or heat-bonded paperHardwood lipping or ABS/polypropylene strip bonded with reactive polyurethane adhesiveInfiltration under the edge, swelling of the substrate and lifting of the edge

Trimming on the construction site, sealing of the bottom rail and air passage

Fitting the leaf on a construction site in French-speaking Switzerland almost systematically requires trimming the bottom rail to suit the finished floor covering and to ensure the mechanical airflow. As soon as the saw blade cuts into the raw panel, the factory protection disappears. Leaving this cut face open in a wet room exposes the wood fibres directly to washing water and to condensate running down the door. Moisture then rises vertically by capillary action to ten to fifteen centimetres within a few months.

  1. Marking out and mechanical trimmingTransfer the finished floor level, including the ventilation clearance calculated by the ventilation engineer. Cut the leaf with a plunge saw guided on a rail and fitted with a splinter guard, so as to obtain a clean edge free of tear-out on the laminate facing.
  2. Chamfering the edgesAlways break the sharp lower corners with 120-grit sandpaper or a joiner's plane. This easing of the edge allows the sealant to coat the joint between the decorative facing and the sawn bottom edge properly.
  3. Application of the impregnating primerApply, by roller or brush, a coat of penetrating water-repellent base coat or a two-component polyurethane varnish. Let the open fibres of the core and of the wooden stiles soak it up until fully saturated.
  4. Final waterproof sealingApply a second protective coat based on liquid epoxy resin, marine varnish or a thixotropic polyurethane adhesive spread with a spatula. The film must form a continuous membrane, free of micro-porosity, perfectly covering the full thickness of the bottom rail.

When making the final adjustment of the hinges and butts, the inspector checks that the undercut remains constant across the whole opening width. Where there is a Swiss-type threshold or a tile-to-parquet transition, the ventilation gap must never rub against the metal strip or the flexible sealing gasket. A regular gap protects the bottom seal from the repeated mechanical impacts caused by dust or residual grit from the construction site.

Door-bottom damage: diagnosing swelling, responsibilities and compliant repair

Swelling at the bottom of a leaf in a bathroom rarely occurs because of an isolated manufacturing defect. It almost always results from an accumulation of standing water on the tiling combined with a lack of protection of the bottom edge after a trimming adjustment. When a leaf starts to rub on the floor or its lower lipping bursts under the pressure of the moistened core, the joiner must first determine the origin of the water: cleaning with large amounts of water without drying, direct splashing from a threshold-free shower, or the complete absence of an undercut preventing the mechanical extraction of stale air.

Diagnosis of damage at the foot of the door in accordance with SIA 343
Visual findingPhysical mechanismCorrective action
Burst lower lipping, facing detached over 50 mmContinuous capillary infiltration through unsealed raw bottom edgeReplacement of the leaf with a water-repellent model with factory sealing, or repair with epoxy resin
Rubbing on the floor without delamination, clearance reduced to less than 2 mmRelative humidity of the room saturated through lack of permanent ventilationCheck of the extract airflow, planing and immediate renewal of the sealing varnish
Warping of the leaf towards the inside of the wet roomExcessive humidity gradient between dry corridor and poorly ventilated bathroomCompliance check of the indoor climate class in accordance with SIA 343

In contractual terms, if the adjustment trimming on the construction site was carried out without reapplying the prescribed waterproofing barrier, the non-conformity falls directly on the installation. On the other hand, if the ventilation flow rates prescribed by the engineers are not delivered by the building's technical installation, permanent condensation exposes any standard panel to premature failure.

Frequently asked questions

How can an already swollen bottom edge be repaired without replacing the door?

Unhang the leaf and let it dry in the workshop at controlled humidity. Once the wood is stabilised, trim off the delaminated part with a plunge saw on a rail, keeping the minimum height required for ventilation. Clean the exposed core, then apply two saturating coats of polyurethane resin or a two-component epoxy sealant over the whole bottom rail before rehanging the panel and checking the clearance.

Which product should be used on the construction site after trimming the bottom of a bathroom door?

A single coat of water-based paint does not form a sufficiently waterproof barrier against washing water. Always use a solvent-based polyurethane varnish, an edge-impregnating wax or an epoxy primer applied with a lacquer roller in two crossed coats. The product must saturate the tubular or solid particleboard core and seal the joint between the laminate facing and the lipping.

What is the minimum undercut height required under a bathroom door?

In rooms connected to single-flow controlled mechanical ventilation, the air passage under the leaf requires a constant functional gap of 10 to 15 mm above the finished floor. This gap ensures the airflow without creating an acoustic whistle and prevents the bottom rail from coming into direct contact with puddles or cleaning products spilled on the tiling.

Why is a standard honeycomb door prohibited in a wet room?

The embossed cardboard honeycomb core has no resistance to vapour and absorbs ambient moisture at the slightest micro-crack in the edge. As soon as the surface film gives way, the cardboard network wicks up water by capillary action, causing immediate buckling of the hardboard facings and rapid rotting of the untreated softwood lower lipping.

Texts and standards cited

  • SIA 343Doors: requirements, classification and performance criteria according to climatic exposure

In the same section