Key takeaways
- SIA 343 sets perimeter clearances between two and a maximum of four millimetres.
- A perfectly consistent visual clearance ensures operation without rubbing against the frame rebate.
- Transverse shrinkage of timber during the heating season alters plumb and dimensions.
- The clearance at the bottom of the leaf includes the air passage or the compression of the automatic drop seal.
Perimeter fitting tolerances and the visual impact of the joint line
On an interior communicating door or an apartment entrance door, the eye perceives a parallelism deviation of half a millimetre before even noticing the finish of the panel. A frame installed out of square or a leaf that is not properly trued produces a trapezoidal gap line that immediately catches the eye of the site management at handover. Beyond the aesthetic aspect, the consistency of the perimeter clearance directly determines how the latch bolt engages in the strike plate and the continuous contact of the acoustic seal.
Doors must be installed so as to ensure flawless, durable operation without rubbing. The clearances between leaf and frame must remain consistent all the way round and absorb the permitted tolerances without compromising the required performance.
norme SIA 343 (Portes)
| Clearance location | Nominal dimension at installation | Permitted tolerance | Critical check point |
|---|---|---|---|
| Hinge side | 2.0 to 2.5 mm | +/- 0.5 mm | No edge binding against the rebate when opening to 90° |
| Head rail (lintel) | 3.0 mm | +/- 0.5 mm | Strict parallelism with the top edge of the panel |
| Lock side (strike plate) | 3.0 to 3.5 mm | +/- 0.5 mm | Full penetration of the bolt and acoustic seal maintained under pressure |
- Checking the squareness of the frameMeasure both internal diagonals of the frame before fitting the leaf. The difference between the diagonals must not exceed 1.5 mm, to avoid an out-of-plumb strike jamb.
- Temporary wedging of the panelInsert bevelled wedges or calibrated 3 mm spacers into the head rebate and the jambs to hold the door closed while the fixings are tightened.
- Three-dimensional adjustment of the hingesUse the micrometric adjustment screws of the hinges to distribute the lateral clearance evenly and correct any lean without planing the stile prematurely.
Dimensional variation of timber and management of the ground clearance
Solid timber stiles and wood-based panels (tubular solid cores, chipboard or high-density fibreboard) react continuously to the relative humidity of the ambient air. During the construction phase, before the ventilation unit or heat production is put into service, relative humidity frequently reaches 70% to 80%. Timber elements absorb moisture and swell. Conversely, during the first heating season in the middle of a Swiss winter, the indoor air dries out and drops below 30% to 35% relative humidity.
For a standard leaf 830 mm wide, a 4% drop in timber moisture content between the as-delivered state on the construction site (around 11%) and the dry winter environment (around 7%) causes an overall transverse shrinkage of nearly 2 mm. If the joinery was fitted too tightly in summer with only 1.5 mm of perimeter clearance, the clearance will indeed widen in winter, but any subsequent humid summer warming will cause the leaf to jam immediately against the rebate. Even more critical, the differential thermal and hygrometric warping between one face exposed to a heated room and the other to a colder corridor makes the top or bottom edge rub against the frame.
| Threshold configuration | Nominal clearance under leaf | Tolerance | Functional requirement |
|---|---|---|---|
| Standard communicating door | 5.0 to 7.0 mm | +/- 1.5 mm | Free passage above carpet fibres or flatness variations |
| Controlled mechanical ventilation (CMV/single-flow) | 10.0 to 12.0 mm | +/- 1.0 mm | Air transfer opening in line with the ventilation design |
| Sealed threshold with automatic drop seal | 4.0 to 6.0 mm | +/- 0.5 mm | Mechanical compression travel of the neoprene seal without jamming the mechanism |
| Apartment entrance door with metal threshold stop | 3.0 mm | +/- 0.5 mm | Uniform compression of the air and smoke seal lip |
The junction at the foot of the frame also requires careful coordination with the laying of floor coverings. SIA 343 prescribes that doors must in no case obstruct free circulation or be affected by differential settlement of the load-bearing structure. When accepting the substrate, the joinery foreman checks the expected deflection of the floor under permanent load in order to adapt the bottom clearance before finally tightening the reveal fixings.
Sizing the perimeter clearance and hygrometric balance under SIA 343
The straightness of the joint line between the frame and the leaf is the first criterion for the visual assessment of an interior door set. A trained eye or a client spots a deviation of half a millimetre on a jamb before even touching the lever handle. Beyond this immediate aesthetic requirement, the allocation of fitting dimensions responds to a strict physical imperative: anticipating the dimensional variation of timber with ambient humidity over the heating seasons.
Doors must operate flawlessly and have fitting tolerances compatible with the foreseeable climatic variations between the rooms they separate.
norme SIA 343
A solid-core or tubular-core leaf reacts directly to thermo-hygrometric transitions. During the summer period or in a new building whose structural work has not yet released all its residual moisture, the relative humidity of the air frequently exceeds 65 to 70%. The timber absorbs this moisture and swells mainly across the grain. If the joiner sets a consistent perimeter clearance of only 1.5 or 2 mm during an autumn installation, the element will work for the first few weeks but will come under stress as soon as the indoor air is circulated.
Conversely, the start of the first heating season in winter abruptly lowers the relative humidity below the 35% threshold, particularly in recent dwellings fitted with controlled mechanical ventilation. The panel then undergoes transverse shrinkage that can reach 1.5 to 2 mm over the total width of the leaf. If the mitre cuts of the frame or the initial squareness lack rigour, the clearance becomes asymmetrical, the latch bolt rubs against the strike plate or the space at the head of the door shows an unsightly gap.
| Control zone | Target nominal clearance | Permitted range in service | Direct consequence of undersizing |
|---|---|---|---|
| Hinge edge | 3.0 mm | 2.5 to 3.5 mm | Rear edge binding on the frame during rotation |
| Lock edge | 3.0 mm | 2.5 to 4.0 mm | Bolt jamming, edge rubbing on the strike plate, failure to close |
| Head rail | 3.0 mm | 2.0 to 4.0 mm | Rubbing under the lintel following settlement of the frame or door sag |
| Bottom of leaf (standard) | 6.0 mm | 5.0 to 8.0 mm | Scraping on the floor covering after deformation or fitting of a carpet |
| Bottom of leaf (CMV transfer) | 10.0 to 12.0 mm | 10.0 to 15.0 mm | Negative pressure in windowless rooms, whistling air, restricted airflow |
Workshop adjustment methods and correcting the clearance at the bottom of the leaf on the finished floor
Achieving a consistent perimeter clearance starts with the mechanical fixing of the frame in the masonry opening or lightweight partition. A frame installed out of plumb or bowed in the middle will inevitably transfer its defects to the geometry of the leaf. The systematic use of non-deformable tapered wedges at the screw points and the use of a precision spirit level make it possible to lock the jambs perfectly parallel before injecting fixing foam or making the mechanical anchoring.
- Checking the frame diagonalsMeasure the frame diagonals with a steel tape before any hardware fitting. The difference between the two measurements must not exceed 1 mm, to rule out any parallelogram distortion.
- Three-dimensional adjustment on hingesUse the micrometric screws of the concealed hinges or adjustable 3D hinges to balance the lateral clearance at a constant 3 mm on each side, with the leaf in the closed position.
- Adjusting the lock edgeCheck the relief of the closing edge with a finishing plane if the edge rubs against the rebate, keeping a slight bevel of 1 to 1.5 degrees to ease engagement.
- Checking the clearance above the finished floorCheck the clearance at the bottom of the leaf using a set of flat feeler shims over the whole opening travel in order to detect screed bumps or raised parquet boards.
Managing the lower gap requires strict coordination with the level references on the construction site. The level mark set out at 1.00 m above the finished floor is the only absolute reference for positioning the frame heads. When the joiner works before the floor coverings have been fully delivered, the final thickness of the floor build-up (adhesive and parquet or tile) must be confirmed in writing with the site management.
On doors fitted with a recessed automatic seal (Swiss threshold seal or drop seal), the travel of the mechanism generally tolerates a maximum gap of 12 mm between the underside of the panel and the finished floor. A larger gap prevents the seal from exerting sufficient compression against the floor, which instantly degrades the certified smoke-stop and acoustic sealing performance of the door assembly.
Remedial protocols: dealing with binding and clearance defects in service
When the leaf rubs against the stop or the bolt refuses to enter the strike plate when the heating is switched on, the joiner must distinguish a normal dimensional variation of the timber due to humidity from a mechanical deformation of the frame. The SIA 343 standard prescribes functional operability requirements that call for a methodical approach. Before using any cutting tool, the ambient humidity and the moisture content of the panel must be systematically checked with a calibrated pin-type moisture meter. If the element was installed in a building still laden with moisture, the radial shrinkage or swelling of the stile often explains the alteration of the consistent perimeter clearance.
- Diagnosis with feeler shims and plumb checkMeasure the actual gap all round. A clearance falling below the critical value of 1.5 mm on the strike jamb indicates swelling or an out-of-plumb hinge jamb.
- Mechanical adjustment of the hardwareUse the three-dimensional adjustments of the hinges or concealed hinges first. A lateral correction of 1 mm is often enough to restore the clearance without damaging the factory finish.
- Edge correction and recessingIf the hardware reaches the end of its adjustment range, remove the leaf and correct the edge with a guided plane or a router, then be sure to reapply a water-repellent varnish to the exposed timber.
As regards the clearance at the bottom of the leaf, direct rubbing on the finished floor after a few months generally indicates slight settlement of the hinges or a perimeter lifting of the floating screed. If the panel incorporates an automatic drop seal, begin by readjusting the travel of the push button on the hinge side before any decision to trim. When trimming the underside becomes unavoidable, the cut must be made with a plunge-cut track saw fitted with a splinter guard, taking care to keep the clearance needed for air transfer of the controlled ventilation and reapplying a sealing primer coat to the raw edge.
Frequently asked questions
What should be done if the leaf binds in summer in a new building?
This is generally swelling of the timber caused by residual moisture in the plasters and screeds. The edge must not be planed hastily. The first step is to adjust the hinges to gain a millimetre of clearance. If planing is carried out on timber at 14% moisture content, winter contraction under heating will dry the leaf to 7%, creating an unsightly, non-compliant gap of more than 5 mm.
What perimeter clearance tolerance does SIA 343 require?
SIA 343 and the professional rules allow a very strict flatness deviation in order to preserve the visual alignment between leaf and frame. As a general rule, the perimeter clearance must remain between 2.5 mm and 3.5 mm on the jambs and the head rail. A visible variation of more than 1 mm along the length of a jamb is immediately perceived as a workmanship defect and may be the subject of a complaint at acceptance of the work.
Why does the clearance at the bottom of the leaf change after the first heating season?
Two phenomena often combine. On the one hand, heated screeds undergo thermal stabilisation and a slight elastic settlement of the floor insulation. On the other hand, the leaf loses volume under the effect of dry indoor air. If the joiner has not anticipated this behaviour by allowing at least 5 mm under the leaf for ordinary interior doors, the bottom of the door may scrape on tile joints or parquet boards.
How can a consistent visible clearance be ensured when installing a frame?
The consistency of the recessed joint depends above all on the rigidity of the frame installation. The jambs must be wedged at the fixing points and checked with a 2 m straightedge to eliminate any bowing. The use of temporary adjustable spreaders during foam injection or screwing ensures perfect parallelism. Before final drying, a check with feeler shims all round makes it possible to validate the required parallelism.
Texts and standards cited
- SIA 343Doors: functional requirements, operability and fitting tolerances