Exterior painting: facade, wood and metal: the execution reference guide
Intended for team leaders, foremen and site managers, this guide brings together the Swiss rules of good practice for successful exterior construction sites. Under SIA 257, the durability of a paint system depends on weather conditions, a rigorous diagnosis of the substrate and the compatibility of the paint films. Here you will find the execution protocols for mineral facades, woodwork and metalwork, control of application risks, and contractual management of works warranties in the face of climatic attack.
- 10chapters
- 22 000words
- 6sections in the training course
- 60chapters in total
Key values to remember 4
3 °C
Minimum margin required above the dew point for application
3 m
Fall height requiring the installation of façade scaffolding
15 %
Maximum moisture content by mass of softwood before painting
5 years
Legal limitation period for asserting defects in a real-estate structure
Scope of this section and interfaces on the construction site
The painter's exterior work begins where the structural work and the assembly of building elements end. Under SIA 257, the painter applies protection and finishing systems to stabilised substrates. This guide deals specifically with the mechanical and chemical preparation of existing substrates, targeted stripping, the bonding primer, and the application of intermediate and finishing coats on mineral render, exterior wood, ironwork and traffic floors.
Acceptance of the substrate is the decisive step. Before any exterior work, the painter checks dryness, roughness, surface cohesion and the absence of expansive salts. In application of CO, if the designated substrate has defects likely to compromise the performance of the specified system, the contractor immediately notifies the client of their reservations in writing before applying the first stroke of the roller or starting the airless pump.
| Building element | Painter's responsibility (CFC 272) | Outside the CFC 272 scope |
|---|---|---|
| Existing rendered facade | Cleaning, biocide treatment, priming, painting | Repair of reinforced base render (CFC 221) |
| Wooden joinery | Sanding, localised filling, microporous stain or lacquer | Replacement of rotten timber, pure joinery work |
| Wrought-iron railings | Manual descaling, brushing, rust converter, lacquer | Removal of unstable anchors or structural welding (CFC 215) |
| Exterior floor or ramp | Preparatory shot blasting, resin screeding, silica broadcasting | Regrading of slope, structural levelling or screed waterproofing |
Logical order of work and technical navigation
The planning of exterior work follows a strict physical sequence, which the ten chapters of this section detail. The first site decision concerns the application window. Chapter O3-01 details the critical impact of surface temperatures, dew point and imminent rain on the drying and coalescence of water-based resins. Starting a coat under a blazing sun or on a damp substrate ruins the adhesion of the paint film.
- Phase 1: Weather diagnosis and surface cleaningConsult the climatic requirements (O3-01), then calibrate pressure washing without disturbing the substrate (O3-10). Treat biological damage and chalking on facade renders (O3-02).
- Phase 2: Treatment of sensitive substratesSelect the system suited to exterior joinery: transparent stain or opaque finish depending on UV exposure (O3-03), taking particular care with end-grain cuts and window rebates (O3-04).
- Phase 3: Metals and traffic areasRemove active corrosion on metalwork (O3-05), treat the embedded feet of balconies prone to water ingress (O3-06) and apply the frost- and salt-resistant coating on garage floors (O3-09).
- Phase 4: Securing the workstation and legal frameworkEnsure collective protection and wind containment on scaffolding (O3-07), then lock down the minutes and the durability clauses (O3-08).
Working at height imposes strict constraints. As soon as the fall height exceeds 3 m on building structures, façade scaffolding compliant with art. 26 OTConst is required to work safely. The painter adapts the protective netting to contain overspray without creating a dangerous wind load on the tubular framework.
📘 Chapters in this section 10
The weather decides: temperature, forecast rain, direct sun and evening dew
Master temperature differences and the dew point to eliminate any risk of the coating being soaked.
Exterior painting: facade, timber and metalRepainting a façade: cleaning, algae, chalking and water vapour permeability
Neutralise micro-organisms and stabilise chalking renders before applying a permeable siloxane paint.
Exterior painting: facade, timber and metalTimber outdoors: stain or paint, south-facing exposure, and the maintenance you announce
Determine the ideal technical compromise between stain and opaque paint according to the level of sun exposure.
Exterior painting: facade, timber and metalTimber windows: edges, rebates, drip rails and rot hot spots
Effectively seal sills and water-drainage rebates to prevent premature rotting.
Exterior painting: facade, timber and metalRusted metal: surface preparation grade, brushing, anti-rust primer and limits
Choose the right level of mechanical stripping and the appropriate primer for oxidised steel.
Exterior painting: facade, timber and metalBalcony guardrail: preparation, embedded post base, and the area that rusts first
Isolate the anchoring of metal base plates in the floor to prevent detachment at the foot.
Exterior painting: facade, timber and metalOn the scaffolding: access, sheeting, wind and overspray on neighbouring property
Sheet the facades without endangering the anchorage of the structure against gusts.
Exterior painting: facade, timber and metalWhat is guaranteed outdoors: warranty on the work, service life and normal wear
Distinguish normal wear from abnormal ageing under the legal warranties of Swiss construction.
Exterior painting: facade, timber and metalGarage floor and ramp: adhesion, freeze-thaw, de-icing salt and anti-slip
Formulate a resin system resistant to mechanical stress, frost and de-icing agents.
Exterior painting: facade, timber and metalHigh pressure: working pressure, distance, and the substrates it destroys
Adjust the flow rate and angle of attack of the pressure washer without delaminating the substrate or opening up water ingress.