Key takeaways
- Applying glue directly to the substrate eliminates the soaking time of the strip.
- The dimensional stability of glass fibre allows strict edge-to-edge hanging.
- The textile system durably bridges inert hairline cracks and evens out surface stresses.
- The primer coat blocks the porosity of the fleece before the acrylic dispersion is applied.
Gluing the substrate and dry hanging of strips without soaking
Hanging a non-woven wall covering or glass-fibre cloth marks a definitive break from traditional methods of hanging wallpapers made of pure cellulose. The glue is no longer applied to the back of the strip laid on a pasting table, but directly onto the substrate with a drip-free medium-pile roller of twelve to fourteen millimetres, or by mechanised spraying. This fundamental change of method removes the soaking step. Non-woven and glass fibre show absolute dimensional stability in contact with water: the fibres do not swell transversely and undergo no perceptible shrinkage when drying in a ventilated environment.
- Dry hanging
- Application method in which a dry textile strip is presented directly onto a wall previously loaded with fresh adhesive emulsion, eliminating any prior wetting time of the material.
The specific glue, formulated on the basis of water-based synthetic resins and reinforced with thixotropic agents, must be spread evenly over a width exceeding that of the strip by a few centimetres. Insufficient loading leads to hollow areas called blisters, while overloading creates ridges visible through the textile mesh. Work proceeds strip by strip to avoid premature drying of the adhesive film under the combined action of warm air and the residual porosity of the substrate.
- Marking out the alignmentMark a vertical reference line with a chalk line or laser at a distance from the corner equal to the width of the strip minus two centimetres.
- Applying the wall glueApply the glue evenly with the roller over a width of about one hundred and ten centimetres, then clear the corners with a brush.
- Presenting the dry stripUnroll the non-woven from top to bottom along the vertical line marked, leaving three centimetres overhanging at the top and bottom.
- Smoothing down and trimmingDrive the air out from the centre towards the edges with a flexible smoothing knife, then trim the excess lengths with a new blade against a metal straightedge.
Neutralising cracks and applying the paint finishes
On old substrates showing crazing or stabilised shrinkage hairline cracks, the glass-fibre cloth or non-woven reinforcing fleece performs a structural bridging function. Thanks to its high tensile strength, the textile reinforcement absorbs the slight surface stresses of the plaster or concrete, preventing the ghosting of the cracks from reappearing through the paint film. However, dynamic or structural through-cracks must first be opened up, dusted, filled with an elastic acrylic sealant and then reinforced separately before the general gluing.
| Type of defect | Recommended reinforcement | Minimum weight | Suitable painting |
|---|---|---|---|
| Capillary hairline cracks under 0.2 millimetre | Smooth cellulose-polyester fleece | 130 g/m² | Two coats of matt or satin dispersion |
| General crazing and slight irregularities | Fine-mesh woven glass-fibre cloth | 160 g/m² | Levelling primer then acrylic dispersion |
| Stabilised cracks up to 0.5 millimetre | Herringbone or coarse-grain glass-fibre cloth | 210 g/m² | Thixotropic undercoat then water-based lacquer |
| New wall under heavy mechanical stress | High-density pre-painted non-woven fleece | 180 g/m² | Two direct passes of water-based polyurethane resin |
Painting on raw cloth requires absolute vigilance regarding the absorbency of the textile system. After the glue has dried completely for a minimum of twenty-four hours, an acrylic opacifying primer coat is always applied. This step saturates the glass fibre, avoids excessive consumption of finish and prevents differential gloss along the edges. On factory pre-painted cloth, this undercoat may be omitted if the substrate is perfectly uniform.
The two final finishing coats are generally applied with acrylic or polyurethane emulsions in satin or silky matt dispersion, which favour washability in damp or heavily used rooms. Application is carried out with a twelve-millimetre textured roller, cross-rolled then evened out from top to bottom without reloading in the vertical direction, so as to ensure uniform coverage of the mesh hollows without drowning the pattern of the weave.
Treating special details, double cuts and bridging of cracking
Bridging of cracked substrates with non-woven or glass-fibre cloth relies directly on the principle of wall gluing. When the glue is spread on the substrate with a 12 to 15 mm drip-free roller, it penetrates by compression into the surface hairline cracks and stabilises the edges of the inert discontinuities. Unlike traditional wallpaper, whose material must soak up water to become pliable, the non-woven textile and the glass-fibre fabric keep their intrinsic stiffness and maximum mechanical strength from the moment of hanging. This hanging without soaking eliminates any risk of residual elongation followed by dimensional shrinkage on drying: the synthetic or mineral fibres remain perfectly edge to edge, preventing the ghosting of cracks from reappearing under the usual hygrothermal variations of the structural work.
- Trimming and fitting internal cornersNever fold a thick strip into an internal corner. The strip is trimmed cleanly in the angle with a wide spatula and a new snap-off blade cutter. The next strip restarts from the bottom of the corner with a full gluing of the substrate.
- Making the double cut at joinsFor paintable cloths or smooth non-wovens hung without a repeating pattern, overlap the edges by 3 to 5 cm on the freshly glued substrate. Cut through both thicknesses simultaneously using a rigid metal smoothing knife as a guide, remove the upper strip, then the concealed lower offcut.
- Butting and smoothing without tensionPress the two edges edge to edge onto the fresh glue film. Run the conical polyurethane seam roller or the flexible spatula over the join without crushing the fibre structure, to obtain an invisible join before complete drying.
Painting systems and behaviour of the system in service
The success of the finish depends on observing the drying times of the glued system and on the choice of dispersion paint. Applying a water-based paint too soon on a dry-hung non-woven reactivates the water in the wall glue if it has not polymerised right through, causing blisters and linear detachment along the joints. A waiting time of at least 24 hours under normal construction site conditions (about 20 °C and 60% relative humidity) is essential before the primer coat or the first filling pass. The paint does not serve only to colour: it mechanically consolidates the fibre reinforcement and locks in the bridging of the cracks.
| Room and loading | Application system | Indicative consumption | Dry film requirements |
|---|---|---|---|
| Dry rooms and offices (standard use) | Matt or velvety acrylic dispersion in two coats | 140 to 170 g/m² per coat | Preserves the relief of the cloth without clogging fine patterns |
| Corridors, stairwells and schools (heavy traffic) | Satin acrylic dispersion or reinforced latex | 160 to 200 g/m² per coat | High mechanical resistance to rubbing and high washability |
| Occasionally damp rooms (toilets, changing rooms) | Water-based acrylic enamel with fungistatic component | 150 to 180 g/m² per coat | Blocking of condensation water and protection against mould |
When applying the final coat, the tradesperson makes sure to distribute the paint evenly with a medium-pile textured roller (10 to 12 mm) without overloading the weave. An excess of material in the hollows of the weave distorts the pattern and leads to surface microcracking as the dry film shrinks. Acceptance of the work is carried out under diffuse natural light, at normal viewing distance, in accordance with the usages and requirements of standard SIA 118 and Swiss professional guidelines. No inspection is to be approved on the basis of direct artificial raking light, which would artificially accentuate the unavoidable variations in thickness inherent in the weaving of fibres.
Handling claims, remedial work on defects and limits of bridging
When the wall covering shows defects after drying or following painting, the cause almost systematically lies in poor management of the gluing of the substrate or in an exceeded time limit. Open joint edges indicate an insufficient supply of adhesive at the edge or an exceeded open time of the glue. In this situation, the fibre was laid on a superficially skinned film that no longer wets the back of the strip. Blisters that appear after the application of the acrylic finish betray localised lack of glue, which the drying tension of the paint film then lifts.
To treat localised blisters without removing the work, the intervention is carried out by a discreet incision with a straight cutter in the direction of the fibres. A reinforced vinyl glue is introduced using a touch-up syringe, then careful smoothing with the conical roller outwards drives out the air and the surplus adhesive before wiping with a clean sponge. If the strip shows a visible lack of flushness or a distortion of the weave caused by unsuitable tool pressure on a projecting edge, surface sanding is to be avoided because it tears the fibre and creates an indelible area of tearing.
When the defects affect the overall continuity or when lack of adhesion multiplies over a large surface, the repair requires complete removal of the defective strip. Dry stripping of a non-woven strip takes place without tearing of the backing if the base coat has blocked the porosity; on a glass fibre blocked by the dispersion, removal requires an incision along the adjacent joints and then a clean cut. The painter then restores flatness with a light skim of smoothing filler, reapplies a primer coat, hangs a new strip and then paints the entire wall to hide any difference in shading or gloss at the joins.
Frequently asked questions
Why do bubbles appear only after the paint roller has passed?
The water contained in the finishing paint penetrates the mesh and locally relaxes the fibre where the wall glue was originally lacking. When dry, the covering seemed held flat by simple mechanical tension. As it dries, the paint pulls on the system and brings out the areas that are not bonded. The blister must then be incised, suitable glue re-injected with a syringe, then smoothed down before applying a very fine local touch-up.
How should a joint that opens by two millimetres after complete drying be treated?
A visible gap indicates excessive stretching of the strip during smoothing or shrinkage following an excessive room temperature during setting. A simple strip of paint never hides this gap. The painter must fill the space with a fine tinted acrylic filler or an ultra-fine surfacing filler, smooth it perfectly with the painter's knife without overflowing onto the relief of the cloth, then sand lightly with fine grit before repainting the whole strip.
Can surplus dried glue on the cloth be sanded before painting?
Dry sanding of dried glue directly on a glass fibre or non-woven destroys the textile structure and makes the surface fluffy. This damage remains visible after several coats of satin or matt dispersion. Smears of fresh glue must be dabbed off immediately with clear water and a clean sponge. If the glue has hardened, it should be softened with lukewarm water before gentle scraping with a non-sharp plastic spatula.
What precaution should be taken if the wall has an old active crack?
Hanging a non-woven or glass-fibre cloth provides no structural resistance against a live crack caused by the movements of the structural work. Before any gluing, the painter reports the defect to the client in accordance with the contractual rules of standard SIA 118. The intervention requires specific bridging with polyurethane sealant or a compressible reinforced tape, because simple smoothing of fibre will eventually tear or detach under the stress of thermal movements.
Texts and standards cited
- norme SIA 118General conditions for the execution of construction work (notice of defects in the substrate and duty to warn)