Key takeaways
- The coved fillet removes the internal angle where dirt and standing water under pressure accumulate.
- A thixotropic epoxy resin mortar makes it possible to shape the cove before the coating is applied.
- The skirting height is adjusted from ten to one hundred centimetres depending on the severity of the cleaning.
- The top termination must always be made in a chase to guarantee a perfectly flush wall junction.
Forming the coved fillet in resin mortar
In a communal laundry, a professional kitchen or a food-processing workshop, the ninety-degree change of plane between the screed and the partition prevents any effective washing. Water sprayed by high-pressure lances strikes the sharp angle, deposits organic residues there and forces the paint film by hydrodynamic pressure. To make the surface cleanable in accordance with good practice, the painter forms a cove skirting, commonly called a coved fillet, creating a continuous transition between the horizontal plane and the vertical substrate.
- Cove fillet
- Continuous concave profile formed at the floor-wall junction using a thixotropic synthetic mortar, intended to eliminate the internal angle to facilitate run-off and mechanical cleaning.
The wall substrate must be sound, dry and free beforehand of any laitance or plaster. The painter begins by mechanically sanding the bottom of the wall over the height of the future skirting as well as the adjoining strip of floor. Careful dust removal with an industrial vacuum precedes the application of a pure epoxy primer. On this still-tacky primer, the technician spreads the resin mortar to form the curve without creating a dry joint.
- Mechanical preparation and marking outSand the vertical substrate and the floor with a diamond disc. Mark the upper line with a blue chalk line and delimit the edge with a durable cloth-backed adhesive tape.
- Application of the bonding primerApply a solvent-free epoxy resin with an angled brush to the floor and the wall, taking care to saturate the mineral pores without leaving any runs.
- Placing the resin mortarMix a two-component epoxy resin with fine quartz sand and a thixotropic agent to prevent the paste from sagging vertically.
- Compacting the fillet with the gougeShape the cove with a corner trowel or a half-round metal float with a radius of thirty to fifty millimetres, smoothing the material firmly.
Sizing the upstand and the junction with the wall substrate
The useful height of the upstand depends solely on the cleaning method prescribed by the client. A simple damp mop tolerates a low skirting of one hundred millimetres. As soon as a hose or a pressure washer comes into use, the water spray requires continuous protection of the wall. The resin system must form an integral watertight tray that prevents moisture from penetrating by capillarity behind the substrate or into the insulation at the foot of the partition.
| Room use | Type of liquid exposure | Minimum height | Recommended fillet radius |
|---|---|---|---|
| Technical rooms, boiler rooms | Occasional damp sweeping | 100 mm | 25 to 30 mm |
| Commercial kitchens, abattoirs | Pressurised hot water jet | 300 to 500 mm | 35 to 50 mm |
| Communal shower rooms | Continuous direct spray | 150 to 200 mm | 30 mm |
| Industrial laundries | Intensive washing and foams | Up to the ceiling or 1000 mm | 50 mm |
The most sensitive point of the work lies in the top termination of the skirting. If the painter applies the resin in direct excess thickness on the wall, the edge forms a horizontal ledge where dirt inevitably accumulates. Moreover, the sheet of water running down from the upper wall infiltrates under this exposed lip. Two compliant solutions eliminate this problem: mechanical chasing or the installation of a metal stop profile.
- Chasing: horizontal grooving of the wall with a grinder to a depth and width of five millimetres. The resin ends in the groove, creating a recessed, completely flush junction.
- The stop profile: an angle or strip in aluminium or stainless steel fixed mechanically to the wall. The resin is drawn up flush with the metal bevel.
- The wall coating junction: the wall paint or the upper polyurethane enamel must cover the edge of the chase or the metal profile with an overlap that sheds water, avoiding any reverse step.
Continuity of the resin film and bridging from the fillet to the floor without a break
In a working room cleaned daily with a pressure water jet or a lance, the coved fillet only plays its sanitary role if the resin system forms a perfectly monolithic envelope from the floor to the top of the upstand. The vulnerable point is invariably the transition zone between the horizontal surface and the radius of curvature. A simple overlay of coats applied without rigour on a dry resin mortar generates divergent curing stresses. The differential shrinkage between the thick fillet mortar and the thin film of the poured screed then causes linear micro-cracks, immediately exploited by pressurised water to infiltrate under the system.
To guarantee the durability of the work, the applicator must ensure chemical continuity or a rough mechanical key at the floor-fillet interface. If the epoxy or polyurethane screed-to-falls mortar has cured beyond its direct chemical overcoating window, sanding with a medium-grit diamond disc followed by industrial dust removal with full vacuum extraction becomes unavoidable. On substrates subject to slight thermal or structural variations, incorporating a low-weight non-woven glass mat impregnated with resin in the radius of curvature neutralises the risk of shear at the junction between the slab and the masonry.
- Sanding and dust removal of the filletRemoval by manual or mechanical sanding of the ridges left by drawing the fillet mortar. Complete vacuuming of the dust to open the pore network without damaging the curved profile.
- Impregnation and vertical bonding bridgeApplication of a two-coat thixotropic epoxy primer on the vertical wall and the fillet radius, with a light broadcast of oven-dried quartz sand to create a keyed texture.
- Safety reinforcement at the angleInstallation of a synthetic fabric reinforcing strip rolled into the still-tacky resin layer along the axis of the screed-wall junction in zones with high thermal loading.
- Pouring and connecting the base coatApplication of the self-levelling resin on the floor with the upstand carried up using a flat trowel or a lacquer roller onto the still-reactive fillet, avoiding any build-up of material or standing excess thickness in the hollow of the cove.
- Water-repellent sealing coatApplication of a film-forming polyurethane or epoxy sealing varnish without a joint, applied crosswise from the top of the skirting down to the horizontal plane to unify chemical resistance and cleanability.
Treatment of the top edge and junctions with wall finishes
The water escape angle is not limited to the foot of the partition: the top of the skirting upstand is the second critical line of infiltration. Water sprayed against the walls runs downwards and strikes the upper edge of the resin directly if it forms a flat protruding edge. To prevent any penetration from behind the film, the head of the skirting must absolutely be integrated into a mechanical chase or terminated under a protective metal profile suited to hygiene requirements.
| Adjoining wall covering | Top termination device | Technical execution of the waterproofing | Risk in a room washed with a jet |
|---|---|---|---|
| Two-component epoxy wall paint | Bevelled chase cut with a grinder (5 mm) | Direct overlap of the chase by the wall paint running down over the resin | Infiltration in case of a scratch on the wall if the chase has not been primed to saturation |
| Wall tiles, ceramic or stoneware | Termination under the first tile with a stainless steel profile | Filling with a polyurethane or hybrid elastomeric sealant under the ceramic tile bevel | Degradation of the sealant under the direct action of the rotary nozzle if the profile does not conceal the joint |
| Smooth sandwich panels or PVC cladding | Clip-in finishing profile with a flexible lip | Resin carried up behind the panel, then mechanical fixing sealed with a compressed gasket | Build-up of mould behind the lip if the mechanical tightening is insufficient |
| Raw smooth cement render | Mechanical stop profile in anodised aluminium | Profile fixing embedded in the resin with a 45° drip chamfer | Cracking of the upper render transmitting moisture by downward capillarity |
The groove or chase is the most robust rule of good practice when the walls receive a watertight wall paint of a compatible class. A groove 5 millimetres deep by 5 millimetres wide is cut with a diamond-disc grinder at the height prescribed by the contracting authority. The upper edge of the fillet mortar and the resin base coat are fully inserted into this cut. When the wall finish is applied, the paint film runs down into the chase and overlaps the skirting by a minimum of two centimetres, neutralising any shoulder where water could stagnate.
Diagnosis of defects and remedial protocol for a failed skirting
During washing with a pressure jet, hot water and detergents penetrate the slightest start of a break. Typical defects appear as blistering under the resin, outright delamination of the fillet mortar or blackening by mould behind the top edge. Infiltration almost systematically comes from two execution defects: a poorly recessed upper edge that opens under the direct impact of the lance, or the absence of a bonding primer on a smooth, soiled concrete wall. Water then infiltrates behind the film, migrates by downward capillarity and lifts the floor resin from the heel of the skirting.
- Mechanical removal and cutting backCut the damaged area with an angle grinder fitted with a diamond disc and integrated dust extraction, penetrating 5 mm into the wall substrate and the floor. Chip out all the delaminated mortar with a flat chisel down to sound concrete. Remove every non-adherent residue.
- Moisture check and dryingMeasure the residual moisture of the exposed mineral substrate. In the presence of saturated masonry, carry out forced mechanical drying by infrared radiation. Do not apply any synthetic binder until the level prescribed by the manufacturer is restored.
- Rebuilding the fillet and bridgingApply an epoxy primer broadcast with sand to refusal, then reprofile the coved fillet with a flat trowel using a thixotropic mortar. Connect the mortar to the existing floor by bevelling the transition to avoid any excess thickness under trolley wheels.
- Head sealing and closureCover the repair with the identical tinted resin system, overlapping the sound areas, previously sanded, by 50 mm. Fill the head chase with a polyurethane sealant suited to chemical exposure.
Frequently asked questions
What minimum skirting height should be adopted for a room subject to high-pressure cleaning?
In a room cleaned with a lance or a foam cannon, the minimum useful height is 150 mm. It rises to 300 mm in food preparation areas or breweries where direct spray and brine discharges are constant. Below 100 mm, the rebound of the jet against the foot of the wall inevitably reaches the non-resin-coated transition zone of the wall.
Can a resin coved fillet be formed directly on a plasterboard partition?
No. Even with water-repellent cardboard facing, plasterboard does not have the mechanical cohesion required to withstand the shrinkage of a resin mortar and the thrust of pressurised water. A hardened mineral base in cement masonry must be required, or a calcium silicate or cement-bonded backing board fixed mechanically must be installed, treated with a specific vapour-barrier primer before the fillet is drawn.
How should the skirting upstand be treated where it passes a flush metal door frame?
The mortar fillet must end against the frame without creating a dead spot for water. Form a 45-degree stop chamfer in the thickness of the skirting just before the jamb. Grind and de-dust the metal to obtain a mechanical key, apply a compatible anti-corrosion primer, then seal the junction with an elastomeric sealant resistant to cleaning cycles.
What should be done if the wall has too high a moisture content for the skirting resin?
If the wall substrate exceeds the moisture limit permitted by the technical data sheet, stop placing the standard mortar. You must notify the site management of the non-conformity and prescribe a specific rising-damp barrier, such as a three-component epoxy primer for damp substrates, or wait for natural drying. Applying onto a saturated substrate causes delamination in the form of osmotic blisters within a few weeks.
Texts and standards cited
- norme SIA 252Poured floor coverings: requirements for substrates, execution and junctions
- norme SIA 118General conditions for the execution of construction work