Skip to content
Website
🧱 CFC 272Painted floors and resins: substrate moistureChapter 3 of 10 in the section

Opening the substrate: shot blasting, diamond grinding and surface laitance

The success of a poured floor covering depends on the mechanical condition of the mineral substrate. This chapter teaches you how to identify cement laitance, how to choose between steel-shot blasting and diamond surfacing, how to manage industrial extraction, and how to verify the opening of the concrete by a direct pull-off test before the primer is applied.

Key takeaways

  • Surface laitance forms a fragile film that prevents any synthetic resin from bonding durably.
  • Shot blasting remains the reference method for stripping large areas of industrial concrete.
  • Diamond grinding treats edges and thresholds and levels substrates without microcracking the matrix.
  • The direct pull-off test validates the minimum surface cohesion required before the wearing layers are applied.

Removing surface laitance to reach the mechanical cohesion of the concrete

Surface laitance
A whitish, friable surface film made up of bleed water, cement fines and admixtures without aggregates, formed during the setting of fresh concrete or during power floating.

Applying a thin epoxy film or a polyurethane screed onto a raw slab without prior mechanical treatment inevitably leads to delamination in sheets. During pouring and mechanical smoothing of the structural work, the fine particles migrate to the surface under the effect of vibration and create a surface crust whose mechanical strength is negligible. This laitance blocks the natural porosity of the substrate and prevents impregnation resins from penetrating. Its tensile strength is often lower than the differential shrinkage stresses of the future covering.

Surface preparation pursues a precise physical objective: removing this sterile crust to expose the sound cement paste and the underlying aggregate skeleton. The floor-resin painter must achieve a cohesive surface, free of curing compound, form-release oils and carbonation. Careful preparation represents half of the time spent on the construction site and determines the long-term adhesion of the entire resin system.

Choosing the mechanical process, controlling dust and checking the bond

Two mechanical technologies dominate slab preparation, depending on the geometry of the rooms, the hardness of the substrate and levelling constraints. Steel-shot blasting propels metallic abrasives in a closed circuit by means of a centrifugal turbine. This technique strips the laitance uniformly without thermally stressing the substrate, while creating a homogeneous roughness ideal for self-levelling resins or float-finished screeds. Modern shot blasters automatically separate the dust from the reusable shot, reducing residues on the construction site.

Diamond grinding is the right choice for small areas, along edges, under skirting boards and on concrete with uneven levels. Its metallic or resinoid segments mounted on rotating plates cut the mineral peaks without cracking the body of the concrete. Diamond surfacing avoids excessive hammering of thin screeds but requires rigorous monitoring of disc clogging, particularly in the presence of residues of bituminous adhesive or old levelling compounds.

Technical comparison of mechanical floor preparation methods
CriterionSteel-shot blastingDiamond-plate grinding
Average outputVery high on large open areasMedium to low, fine manual guidance
Roughness profilePronounced, comparable to coarse-grit sandpaperSmooth to micro-rough, regular profile
Areas treatedCommon flat surfaces, car parks, warehousesEdges, corners, thresholds, cluttered rooms
Mechanical impactSteel projection, opens closed poresRotary levelling, removes bumps

Mechanical machining releases large quantities of crystalline silica dust. Under the ordinance on safety and the protection of workers' health in construction work, air quality at the workstation must be guaranteed by capturing hazardous dust. Grinding or shot-blasting equipment is systematically coupled to an industrial vacuum of dust class H fitted with absolute filters and pneumatic filter cleaning. Preliminary sweeping or simple manual dusting is prohibited: careful extraction over the entire surface, immediately before the epoxy primer is applied, determines the wetting of the open pores.

  1. Main mechanical strippingRun the shot blaster in straight lines with a pass overlap of about two centimetres, adapting the forward speed to the hardness of the slab.
  2. Reworking edges and perimetersDiamond-grind the edges, column bases and areas the shot blaster cannot reach with a shrouded edge grinder.
  3. Industrial vacuum dust removalSystematically vacuum the entire floor with a wide nozzle connected to a sealed extraction unit fitted with certified filter cartridges.
  4. Direct pull-off checkBond metal dollies with methacrylate resin, core around them with a diamond bit down to sound concrete, then apply axial tension with a dynamometer.

Qualifying the roughness profile and industrial dust removal after stripping

Mechanically opening a concrete slab is not limited to destroying the surface film of laitance. To guarantee the bond of an epoxy or polyurethane primer, the substrate must present an open surface profile, free of any friable material and calibrated to the viscosity of the selected system. Professionals assess this roughness according to concrete surface profiles, graded by the international concrete surface profile standards ranging from fine grinding to heavy shot blasting.

Choosing the mechanical stripping method according to the resin to be applied and the profile required
Mechanical processRoughness profile obtainedVisual appearance of the substrateCompatible resin system
Diamond grinding (medium grit)Fine to very fine profile (CSP 1 to 2)Smooth surface, matt cement paste, aggregates flush with the surfaceWater-based floor paints, thin epoxy films
Aggressive diamond grinding (PCD segments)Medium profile (CSP 2 to 3)Homogeneous micro-roughness, open cementitious matrixThin poured self-levelling coatings (1 to 2 mm)
Steel-shot blastingTextured to rough profile (CSP 3 to 5)Aggregate edges exposed, laitance completely absentThick self-levelling systems (2 to 4 mm), resin mortars
Mechanical planing or millingCoarse profile (CSP 6 and above)Pronounced grooves, uneven relief with fractured aggregatesPolyurethane-cement screeds, float-finished resin mortars

After the shot blaster or floor grinder has passed, the substrate is covered with silica micro-dust and stripping residues trapped in the crevices of the concrete. Manual sweeping or a basic site vacuum cleaner cannot extract the fine particles lodged in the pores. Residual dust acts as a separating layer and prevents the binder from properly wetting the sound concrete.

Checking the cohesion of the substrate by direct pull-off test

Once the surface has been exposed and carefully vacuumed, the applicator painter cannot rely on a simple visual examination to authorise application of the resin. The absence of visible laitance does not guarantee that the underlying zone has sufficient mechanical strength. Carbonated concrete, excess water at pouring or defective curing can produce a friable layer several millimetres deep. Checking surface cohesion by direct pull-off is the only objective way of validating the soundness of the substrate.

  1. Preliminary coringUsing a diamond bit cooled without excess water, make a circular cut 50 mm in diameter through the prepared zone, penetrating at least 10 to 15 mm into the core of the solid concrete, so as to isolate the dolly from the rest of the slab.
  2. Bonding the pull-off dollyDegrease and thoroughly dry the cored surface, then fix a rigid metal dolly with a fast-setting two-component epoxy adhesive. Allow the adhesive to cure fully before applying any mechanical load.
  3. Applying axial tensionCouple the tensile dynamometer perpendicular to the metal dolly. Apply a continuous, progressive tensile force at a rate between 0.05 and 0.1 N/mm² per second until the assembly fails completely.
  4. Analysing the failure patternRecord the maximum stress shown by the instrument and examine the fractured surface. The failure must occur within the body of the concrete itself (cohesive failure of the substrate) and not at the surface of the substrate or at the adhesive joint.

The results of these pull-off tests must be recorded in a substrate acceptance report stating the location of the test points, the stresses recorded in megapascals and the nature of the failures observed. This document protects the painting contractor and certifies that mechanical preparation has turned raw concrete into a clean, rough substrate that is structurally capable of receiving the synthetic resin system.

Remedial protocols in case of lack of cohesion or mechanical failure

When the pull-off test after stripping reveals a cohesive failure within the body of the concrete at values that are too low, the painter suspends the work. Mechanical removal of the surface laitance has eliminated the friable film, but the underlying substrate itself proves to lack bearing capacity. Continuing with an epoxy or polyurethane primer on a powdery slab guarantees that the resin will delaminate under thermomechanical stresses. The painter records these contradictory findings and sends a formal written notice to the site management, in application of standard SIA 118.

Faced with a non-compliant result, the origin of the defect dictates the corrective measure. If diamond grinding has closed the pores and produced thermal glazing, the segments chosen are unsuitable: very hard concrete requires an extra-soft diamond matrix that self-sharpens without clogging. A new corrective pass with the appropriate grit is essential. If deep contamination by oils or hydrocarbons is exposed beneath the surface crust, heavy chemical degreasing or localised planing precedes the bonding phase. When the roughness obtained is correct but the adhesive tape test reveals embedded micro-dust, the painter carries out slow industrial vacuuming with a brush head connected to a certified sealed dust extractor. No primer is tolerated on a loose film that compromises mechanical adhesion.

  • Suspend application as soon as the dolly pull-off test reveals early failure in the concrete.
  • Notify the client in writing of the lack of substrate cohesion in order to establish responsibilities.
  • Resume grinding with suitable diamond segments if the surface has been glazed without capillary opening.
  • Carry out a final high-performance industrial vacuuming pass before applying the impregnation coat.

Frequently asked questions

What should be done if shot blasting leaves visible pass marks as ridges and grooves?

Pronounced pass lines appear when the forward speed is irregular or the overlap is poorly adjusted. With a thin or semi-thick resin, this relief shows directly through the finishing coat. The painter must intervene with a heavy planetary grinder fitted with suitable diamond segments to level the ridges and even out the profile. Careful dust removal by industrial vacuuming then immediately precedes application of the pore filler or the resin.

Why does diamond grinding sometimes create a surface that is too smooth for a resin?

This phenomenon occurs when the diamond segments are too hard in relation to the hardness of the concrete: the diamonds blunt without renewing themselves, rub the substrate and cause surface glazing instead of clean abrasion. The pores of the concrete end up clogged by dust fused by the heat. To restore the capillary opening that is essential, it is necessary to go over the surface again with soft-bond discs or carry out light shot blasting, ensuring constant extraction.

How can you verify that dust removal after mechanical preparation is truly satisfactory?

The check is carried out with the transparent adhesive tape test: the tape is pressed firmly onto the prepared floor and then peeled off. The presence of visible particles on the sticky side indicates a powdery residue incompatible with applying an epoxy resin. Since the traditional broom is prohibited because it disperses the fines into the air, only repeated passes with an industrial vacuum with an absolute filter, fitted with a rubber lip as close to the floor as possible, guarantee complete removal of the dust.

What waiting time is required between mechanical preparation and primer application?

The adhesion primer must be applied as soon as possible after mechanical preparation, ideally the same day. Leaving stripped and vacuumed concrete exposed to the air encourages contamination by construction site traffic, fallout of ambient dust or renewed uptake of atmospheric moisture. If application has to be deferred by more than forty-eight hours, meticulous industrial vacuuming and a complete visual inspection must be repeated before mixing of the resins begins.

Texts and standards cited

  • SIA 118General conditions for the execution of construction work

In the same section