Opening joints: substrate shrinkage, adhesive, soaking time and heated room

This chapter gives you the method to identify and neutralise the opening of wall-covering joints. You will know how to match your adhesive to the weight of the covering, respect the soaking time according to the type of backing, lock down the thermal management of the room and check the stability of the substrate before pasting the first strip.

Key takeaways

  • Uneven soaking of the paper causes unavoidable mechanical shrinkage as the strips dry.
  • An unsuitable or under-dosed adhesive gives way under the transverse tension exerted by the wall covering.
  • Draughts and accelerated heating dry out the adhesive before the edges have fully bonded.
  • An unstabilised or damp mineral substrate causes shrinkage movements that cannot be compensated.

Control the soaking of the paper and select the suitable pasting system

Joints opening after drying most often result from a hygrometric imbalance during hanging. When a traditional paper-backed wallpaper absorbs the water contained in the adhesive, its cellulose fibres expand mainly in the transverse direction. If the strip is pressed onto the wall before it has reached its maximum expansion, this expansion continues temporarily on the wall, then reverses violently as the water evaporates. The paper then returns to its initial dimension, exerting a considerable lateral pull. If the adhesive has not yet developed sufficient mechanical strength at the edges, the edges separate, leaving a gaping joint of one to three millimetres.

To eliminate this risk on paper-backed coverings, the team must apply a strict waiting protocol, folding the strips book-fashion, edge to edge, to prevent premature drying of the edges. Conversely, non-woven wall coverings undergo almost no dimensional change in the presence of water. In this specific case, the soaking time is eliminated: the adhesive is applied directly to the substrate with a drip-free roller, followed by careful brushing-in with a brush along skirting boards and corners.

Dimensional behaviour and pasting method according to the type of backing
Type of backingDimensional mechanismPasting methodRequired soaking time
Standard paper backingStrong transverse expansion with moisturePaste applied to the back of the strip, folded book-fashion5 to 8 minutes according to manufacturer's data sheet
Heavy paper / vinyl backingSlow expansion and strong tension on shrinkagePaste applied to the back with reinforced adhesive8 to 12 minutes under strict control
Non-woven / textile on non-wovenAbsolute dimensional stabilityPaste applied directly to the prepared substrateNone (hang immediately into the fresh adhesive)

The choice of binder determines the ability of the adhesive film to hold the paper edges against the wall during this critical tension phase. A standard adhesive based on pure methylcellulose is suitable for light papers, but proves insufficient for heavy vinyls or textured wallpapers. These require a reinforced adhesive with synthetic resins, formulated with a higher dry content and an enhanced initial grab. Adding a concentrated adhesive emulsion on the edges or using a specific adhesive for borders ensures an immediate holding force greater than the transverse shrinkage tensions of the wall covering.

Neutralise premature evaporation and diagnose substrate movements

The drying kinetics determine the final adhesion. A water-based wallpaper adhesive needs slow, gradual evaporation so that its polymers migrate into the substrate and develop their crystalline bond. The most destructive mistake is to hang a wall covering in an overheated room or one subject to forced ventilation. When site heaters run right next to the walls, or when windows are left ajar to dissipate ambient moisture, the water in the adhesive evaporates at the surface before the binder has polymerised. The edges of the strip, thinner and more exposed, lose their water first: the adhesive dries white without bonding, and the edge lifts immediately.

Finally, the opening of joints may originate not in the covering itself but in the underlying substrate. A mineral substrate that has not completed its dimensional stabilisation phase irremediably compromises the finishing work. Plasterboard fixed to a poorly braced metal frame, lightweight partitions subject to site vibrations or freshly bonded masonry elements can undergo mechanical shrinkage or millimetre-scale settlement after pasting. If the substrate moves apart beneath the wallpaper joint, the covering tears or the edges open inexorably along the crack in the substrate.

  1. Hygrometric check of the substrateCheck that the substrate is completely dry using a contact moisture meter. Any residual moisture prevents the cellulose adhesive from setting and promotes later delamination of the edges.
  2. Checking surface cohesionCarry out a cross-cut test and an adhesive-tape pull-off test on old substrates to make sure the surface layer will not be torn off by the shrinkage tension of the paper.
  3. Regulating porosityApply a bonding primer or a pigmented primer to block excessive absorption by porous substrates, thus avoiding abrupt suction of the water contained in the adhesive.
  4. Monitoring the indoor climateMaintain a constant temperature and record the ban on creating draughts, communicated to the other trades working in the area, until the covering has dried completely through.

Systematic exclusion method: soaking, adhesion and thermal environment

The opening of a joint during drying or the day after hanging results from a specific mechanical imbalance: the tension exerted as the covering shrinks exceeds the bond strength of the adhesive film, or the substrate itself has deformed beneath the strip. To eliminate these defects on new construction sites or in major renovation, the foreman applies a chronological exclusion grid before starting to paste the rolls.

Differential diagnosis of the causes of joint opening in wallpapering
Visible symptomPhysical origin of the defectPreventive action on site
Joint open by 1 to 3 mm over the full height, clean edges, paper overstretched with no detachment from the substrateInsufficient soaking time for a strip on a paper backing: the product kept stretching on the wall and then shrank violently as the water evaporated.Strictly observe the softening time given by the manufacturer (often 8 to 12 minutes), soak with regular folding, paste evenly.
Edges lifted, paper rigid at the joint, no dry adhesive on the substrate beneath the jointSudden evaporation caused by a draught or direct heat input (directed site heating, underfloor heating switched on too strongly).Switch off spot mechanical ventilation, keep windows closed with no draught, stabilise the room temperature between 16 °C and 20 °C.
Edge-to-edge joint split with tearing off of the base primer or of the cardboard layerAdhesive unsuited to the weight of the covering (lack of tack) or substrate too porous, having absorbed the binder before setting.Apply a reinforced synthetic-resin adhesive, regulate porosity with a water-repellent penetrating primer without creating a glossy, non-absorbent surface.
Joint gaping diagonally or opening locally at a board junctionStructural movement or drying shrinkage of an unstabilised substrate (plasterboard fixed to a frame under stress, green concrete).Check the residual moisture of the substrate and verify the decoupling of the junctions between load-bearing elements before setting out the layout of the strips.

Adhesive management directly determines how well the edges hold. A conventional methylcellulose adhesive does not have the holding force needed against the transverse tensions of heavy papers, vinyls with a heavy non-woven backing or textile textures. In these cases, adding synthetic resins in dispersion is essential to ensure a high initial tack and sufficient shear strength during the phase in which the substrate regulates the excess water.

Checking the unstabilised substrate and remedies for open joints

An unstabilised substrate compromises the integrity of the wallpaper, even if the adhesive is applied flawlessly. In new buildings, lightweight plasterboard partitions undergo differential movements linked to the drying of screeds or to operational vibrations. When the junction between two boards opens under the effect of shrinkage of the structural work, the strip pasted across this joint takes up the tensile force. If the tear resistance of the paper is greater than the adhesion of the adhesive, the joint opens without tearing; otherwise, a split appears along the edge.

To eliminate this risk, the hanging team must identify the layout of the boards beneath. The wallpaper joints must under no circumstances coincide exactly with the longitudinal joints of the plasterboard. A minimum lateral offset of twenty centimetres allows the residual tensions of the substrate to be spread over the central part of a strip, which has a much greater elastic elongation capacity than an edge-to-edge joint line.

  1. Targeted re-moistening of the edgesGently moisten both edges of the open joint using a wrung-out sponge and lukewarm demineralised water to soften the material without altering the surface decoration or delaminating the cardboard.
  2. Injection of a specific repair adhesiveIntroduce a seam adhesive in a tube with a fine nozzle directly under the dry edges. Avoid spreading a standard adhesive whose water content would reactivate excessive shrinkage.
  3. Repositioning under friction and pressingCarefully slide the edges towards each other using a conical seam roller or a flexible plastic spatula, without mechanically stretching the fibre, which would risk recreating a return stress.
  4. Immediate wiping and maintaining the hygrometryRemove adhesive squeeze-out immediately with a clean damp microfibre cloth, then keep the room free from any draught during final setting.

Remedial protocol and assessment of open-joint defects

When strip joints part after complete drying, the finding on the work requires a rigorous methodology before any attempt at repair. The painter must never conceal an open joint with acrylic filler or by surface pasting: filling a gaping joint without identifying the failure mechanism inevitably leads to rejection of the work at acceptance under the SIA 118 standard. A methodical diagnosis must be made, if necessary destructive on a discreet area, to determine the exact cause among dimensional shrinkage of the paper, thermal shock in the room and structural movement of the substrate.

  1. Hygrometric survey and examination of the edgesMeasure the ambient temperature and relative humidity of the room. Observe the edges of the strip: edges curved outwards betray insufficient soaking time of the paper or drying that was too fast under direct heating.
  2. Probing adhesion at the edgeGently peel back the edge with a smoothing knife. If the adhesive remains attached to the substrate with no cohesion with the paper, the adhesive was unsuitable or was absorbed prematurely by an overly porous, unprimed substrate.
  3. Checking the underlying crackCut locally along the axis of the joint to probe the plaster or plasterboard. A continuous crack in the substrate shows mechanical shrinkage of the structural work or of the partition, clearing the painter of the pasting error.

When the joint expert assessment concludes that there was an application failure, complete redoing of the strips concerned remains the only technically admissible solution under the recognised rules of the trade. The panel is carefully removed by moistening or with low-pressure steam, the starch residues are washed off without damaging the primer undercoat, then a replacement strip from the same batch number is hung, this time ensuring a rigorously timed soaking period and a reinforced adhesive.

Frequently asked questions

How can you repair a joint open by a few millimetres without replacing the whole strip?

On a non-woven or heavy vinyl wallpaper with no loss of material, moisten the edges locally with a fine brush to soften the covering. Then insert a ready-to-use high-adhesion seam adhesive under each edge, and gently press the lips together with a conical polyoxymethylene seam roller, without crushing the grain of the pattern. Wipe off the squeeze-out immediately with a damp natural sponge.

Why can a non-woven wallpaper open at the joint even though it does not shrink?

Non-woven has excellent dimensional stability, but its joints open if the adhesive applied to the wall has dried too quickly before pressing. The initial adhesion then becomes insufficient at the edges, which lift under the effect of draughts or excessive absorption by the plaster. The absence of a regulating base primer or a transverse draught during the first few hours explains most of these lateral detachments.

Who bears the cost of the repair if the joint opens because radiators were switched on by another trade?

Within the contractual framework of the SIA 118 standard, the contractor is responsible for his services, but the client bears the consequences of an unforeseen disturbance of the ambient conditions. If the painter has recorded the absence of heating and hot-air blowers were activated without coordination during drying, he promptly sends a written notice to the site management. This record relieves him of technical responsibility and allows the remedial work to be invoiced.

How can you tell a joint opening caused by the paper from a movement of the plasterboard substrate?

Carefully cut a triangular sample along the axis of the parted joint to examine the underlying substrate. If the reinforcing tape of the plasterboard is sheared or if the original jointing shows a continuous micro-crack, the defect comes from movement of the structure or of the partition. On the other hand, a perfectly sound, smooth plaster base clearly points to an adhesive error or a soaking time that was not respected.

Texts and standards cited

  • norme SIA 118General conditions for the execution of construction work

In the same section