Skip to content
Website
🧱 CFC 272Interior paint systems: selection and applicationChapter 2 of 10 in the section

Hiding power, flashing and lap marks: working wet on wet and finishing the wall

In interior painting, a visible lap mark shows the exact spot where the film had begun to cure or dry before the next pass was joined on. This chapter details the application rules for finishing an entire wall section in one continuous run, controlling the open time of the product, preventing differences in sheen, and accepting the surfaces under diffuse natural light in accordance with professional rules.

Key takeaways

  • A wall surface is painted in a single continuous run so that the application edge stays wet at all times.
  • Flashing indicates uneven absorption of the substrate, creating a local break in the sheen of the dry film.
  • Wet-on-wet application requires a coordinated pace between cutting in and the main rolling.
  • The final visual inspection must always be carried out in diffuse natural light, without artificial raking light.

Understanding the physical origin of flashing and lap-mark patterns

Flashing
Area of a paint film showing a local loss of sheen or abnormal dullness, caused by excessive and uneven absorption of the binder by the substrate.

Visible lap marks and flashing are the two main homogeneity defects of a finishing film. A lap mark results from the drying time being exceeded between two adjacent passes. When a roller overlaps an area whose emulsion has already begun its coalescence or solvent-loss phase, the resins no longer fuse homogeneously. This local excess thickness disturbs the tension of the film and changes the orientation of the mineral fillers and pigments. The optical result is immediate: a darker, glossier or rougher band appears at the junction of the working strips. The site rule allows no compromise: a wall section that has been started must be finished without the slightest pause, otherwise the defect cannot be remedied without complete sanding and re-application over the whole surface.

Flashing, for its part, reveals uncontrolled porosity of the underlying substrate. If the substrate shows uneven absorption (for example between a sanded skim coat and an old sealed surface), it draws the liquid binder out of the fresh paint before the film has structured itself. Without enough binder matrix at that precise spot, the surface becomes depleted at the surface, increasing the microscopic roughness. The result is a sharp drop in the degree of sheen, noticeable as dull, matt patches. The only technical remedy is the prior application of a primer coat or a regulating water-repellent impregnating sealer, calibrated to even out capillary absorption across the whole surface to be painted.

Technical distinction between flashing and lap marks
ParameterFlashingLap mark
Physical mechanismExcessive suction of the binder by the substrateDouble coat over a film that is still drying
AppearanceMatt, discoloured or chalky-looking patchRaised band or linear difference in sheen
Origin of the defectMissing or poorly calibrated primerBreak in pace or stopping in the middle of the wall section
Remedial action requiredSealing the substrate, then a new general coatLight sanding of the excess thickness and complete repainting

Carrying out wet-on-wet application and acceptance according to standard SIA 257

To guarantee perfect continuity of the film without a noticeable lap mark, the painter applies the rigorous wet-on-wet technique. This method requires working methodically in vertical strips fifty to eighty centimetres wide, joining each new pass into the still-liquid edge of the previous pass. Cutting in around skirting boards, external corners, window reveals and ceilings must be strictly synchronised with the central rolling. If a worker cuts in an entire room before starting to build up the film with the roller, the dry edge will have formed an irreversible skin, inevitably producing a visible frame around the perimeter of the walls.

  1. Adjusting the drying conditionsClose the windows and cut off draughts to extend the open time of the water-based product.
  2. Coordination of the application teamOne worker cuts in the edges with a brush while the second immediately spreads the paint with a short- or medium-pile roller.
  3. Laying on and cross-rolling the productLay the material on generously from top to bottom, cross-roll horizontally to even out the film, then smooth vertically towards the light.
  4. Continuous joining in the wet zoneOverlap the edge of the previous pass by five centimetres at most while the film is still liquid.

Aesthetic assessment in diffuse light makes it possible to judge optical flatness without artificially amplifying the fine roller grooves or the slight variations in thickness that are inseparable from careful manual application. If an accidental join occurs in the middle of a panel following a work stoppage, the visual tolerances of standard SIA 257 are systematically exceeded because of light diffraction. In this situation, localised touching up is strictly prohibited: the painter has no technical option other than to let the surface dry completely, lightly abrade the defective film, and repaint the entire wall section from one corner to the other.

Organising the work station and application sequence to keep the edge open

A lap mark or flashing appears when the liquid film is broken in continuity. As soon as the water of a dispersion evaporates, the resins begin to coalesce. If the roller lays fresh material onto an area that is already going matt, the film thickens locally, changes the texture of the roller stipple and disturbs the orientation of the fillers. The phenomenon is irreversible: the overlapped area creates an optical excess thickness and a permanent difference in sheen. The organisation of the work station must guarantee continuous progress without interruption between the two edges of the wall. On long runs or in rooms of great floor height, the application is carried out by two painters: the first opens up the cut-in lines and edges, the second loads and unloads the main roller without waiting.

  1. Synchronising cutting in and building up the filmCutting in of internal corners, skirting boards and frames runs ahead of the rolling by one strip only. Painting the entire perimeter before building up the panel condemns the film to dry at the edge, creating a glossy or rough frame. Brushing is carried out one metre ahead at most.
  2. Cross-rolled strips and wet overlapThe application is organised in vertical strips sixty to eighty centimetres wide. Paint is applied from top to bottom, cross-rolling to even out the load, then biting a few centimetres into the previous strip while it is still perfectly liquid.
  3. Levelling and vertical smoothing without pressureEach strip is smoothed from top to bottom without reloading the roller, easing the pressure on the roller frame. This movement unifies the orientation of the stipple and prevents material from being mechanically torn away at the still-fresh joining line.
Ambient factors and measures to keep the edge open
Site constraintEffect on the filmWorkshop measures
Through draughtAccelerated evaporation and premature closing of the liquid edgeTemporary closing of the windows and switching off of mechanical ventilation
High ambient temperatureCritical reduction of the open time of the dispersionScheduling the finishing coat for the cool morning hours
Substrate of uneven porosityUneven absorption of water causing local matt flashingMethodical application of a regulating impregnating sealer
Large wallImpossible to keep wet on wet when working aloneCoordinated team work with a mobile scaffolding

Dealing with sheen defects and visual inspection according to standard SIA 257

Flashing shows as a local drop in sheen or abnormal roughness, most often caused by differential suction of the substrate, particularly at unsaturated board joints. Conversely, lap marks create glossier bands or excess thicknesses at the joins between passes. Faced with these defects, no spot touching up can restore a uniform appearance. Remedial work requires waiting for the film to dry completely, a light sanding with fine abrasive paper to level the excess thickness, then the application of a complete finishing coat from one edge to the other.

A paint film is not checked under arbitrary lighting. Standard SIA 257 defines the acceptance of interior painting work. The inspection is carried out in diffuse natural light, without direct sunlight and at two metres facing the wall. Examination under artificial raking light, using a site floodlight aimed at the substrate, is not admissible for qualifying an appearance defect, unless permanent raking light is expressly provided for in the works contract. Slight nuances of texture visible only at a raking angle do not call into question the conformity of the work if the appearance remains regular under normal service lighting.

Handling a crisis on an open panel: corner-to-corner remedial protocol

When the fresh edge has been lost following an unforeseen interruption or excessive ventilation, any attempt at spot touching up with the roller produces a disastrous surface finish. Overlapping binder onto a film that is still curing instantly creates an excess thickness and a break in matt level. As soon as the paint starts to drag in the middle of a wall section, the painter must stop: the only technical solution is to let the work dry completely before starting a full remedial treatment of the delimited surface.

  1. Through-drying and neutralising the reliefLet the film harden according to the manufacturer's data sheets. Sand the demarcation zone with P180 or P220 grit on a dust-extraction block to remove the ridge without damaging the adjacent substrate.
  2. Regulating the substrate by impregnationApply a bonding primer or a diluted clear fixative to the sanded area to even out the absorption of the substrate and prevent a porosity flashing from reappearing during the general pass.
  3. Carrying out a continuous run from edge to edgeRecoat the entire wall from one internal corner to the other without stopping. Two operators work together if the height exceeds three metres: one cuts in the corners with a brush, the other applies and cross-rolls with a short-pile roller.

Acceptance of the work is carried out in accordance with the requirements of standard SIA 257. Surfaces are always examined from a minimum distance of two metres, under diffuse natural light, perpendicular to the treated plane. The use of artificial raking light or a torch is strictly excluded for judging the aesthetic conformity of the substrate. If differences in sheen remain under this standardised viewing angle, the whole panel must receive an additional general coat after careful light sanding.

Frequently asked questions

Can a localised flashing be hidden by dabbing on diluted paint?

No. Localised dabbing changes the light refraction index and creates a visible patch under raking light. Adding extra water or solvent soaks the underlying resin without restoring the microporosity of the film. To eliminate flashing, the absorption of the substrate must first be re-homogenised with a suitable primer, then a continuous finishing coat must be re-applied over the whole panel, from one corner to the other.

How do you keep the edge wet on a large ceiling in summer?

The organisation requires closing the windows to eliminate draughts and switching off the underfloor heating. The team applies a compatible drying retarder recommended by the manufacturer and works progressively as a pair, or with an airless spray gun backed up by a roller. Work always proceeds parallel to the main light source, dividing the ceiling into regular one-metre strips without stopping between passes.

What visual inspection method does standard SIA 257 stipulate?

Standard SIA 257 prescribes observation with the naked eye from a distance of at least two metres, under diffuse natural light, without direct sunlight or artificial raking light. The assessor stands perpendicular to the wall or according to the usual use of the room. Any defect not perceptible under these normal viewing conditions cannot be classed as an aesthetic defect justifying remedial work at the applicator's expense.

What should you do if the drying time prevents you from finishing the wall before the break?

The sequence of work on the construction site requires postponing the break until the wall section that has been started is finished. Interrupting the application in the middle of a wall inevitably condemns the work to a visible lap mark, which will later require sanding and complete redoing of the panel. The foreman plans the opening of the tins and the start of the surfaces by calculating the time needed to reach an internal corner or a clean edge.

Texts and standards cited

  • SIA 257Painting, varnishing and interior and exterior wall coverings: execution requirements, tolerances and acceptance criteria for finishes

In the same section