Repainting a façade: cleaning, algae, chalking and water vapour permeability

This chapter guides you step by step through renovating an old façade render without blocking moisture transfer. You will learn to assess the condition of the substrate, to eradicate micro-organisms durably, to stabilise powdery surfaces and to select a vapour-open coating in line with the requirements of SIA 257.

Key takeaways

  • A precise diagnosis of the render determines the adhesion and durability of the chosen paint system.
  • Biocide treatment after washing eliminates algae spores deep within the mineral surface irregularities.
  • Applying a suitable fixative stops chalking without creating an impermeable film on the surface.
  • Water vapour permeability takes precedence over appearance to prevent any blistering of the render.

Diagnose the render, eliminate micro-organisms and stabilise chalking substrates

Before any work with brush or roller, the mechanical and sanitary condition of the existing mineral render must be examined methodically. The guidelines of SIA 257 require the painter to check the surface cohesion, the presence of micro-organisms and the porosity of the substrate. Rubbing the palm of the hand or a dark cloth against the render immediately reveals active chalking, caused by the degradation of the original binder under the action of weather and ultraviolet radiation. In parallel, a cross-cut test with a cutter or a sounding with a painter's hammer reveals any localised delamination.

The presence of red or green algae or black mould on façades exposed to the weather calls for rigorous chemical decontamination. Simple mechanical washing merely spreads the spores into the micro-cracks of the render. A no-rinse algicidal and fungicidal remediation product is applied after surface cleaning, onto a surface that has drained and dried. This curative treatment destroys the micro-organisms embedded in the depth of the grain and neutralises their vegetative regrowth before painting.

  1. Cleaning and removal of dirtWash the façade with clean water at moderate pressure to remove dust, atmospheric deposits and pollution crusts without eroding the mineral texture.
  2. Biocide decontaminationSpray a residual algicidal and fungicidal solution over the whole surface, then leave to act according to the technical recommendations without rinsing.
  3. Neutralising the chalkingApply a water-repellent penetrating primer or a silicate-based fixative to consolidate loose particles and regulate the absorption of the substrate.

When the render is chalking, applying an intermediate or finishing coat directly inevitably leads to rapid delamination due to lack of mechanical bond. The powdery substrate requires deep impregnation with a fluid colourless fixative. On a lime- or cement-based render, a potassium silicate impregnating primer consolidates by silicification within the pores of the masonry, while a solvent-borne or water-borne acrylic primer with ultrafine particles is suitable over old synthetic coatings that are still cohesive.

Ensuring water vapour permeability to prevent blistering of coatings

The colour and texture of a façade are only the visible envelope of a complex physical balance. Under SIA 257, the selection of an exterior paint system depends first and foremost on the water vapour permeability of the whole wall build-up. Water vapour from indoor activity and from the residual moisture of the masonry must be able to migrate outwards without meeting an impermeable obstacle. If an overly closed resin is applied to a breathable mineral substrate, the osmotic pressure built up behind the film eventually pushes the paint film off under the action of solar heat, causing blisters, flaking in sheets and disintegration of the underlying render.

Classification of façade paint families by hygrometric behaviour
Binder familyVapour permeability (Sd)Weather resistanceBehaviour on old render
Mineral silicateVery high (below 0.05 m)Excellent through chemical bondingIdeal on raw or restored mineral renders
Silicone resinHigh (between 0.05 and 0.14 m)Outstanding hydrophobic water-beading effectVersatile, permeable and protective
Acrylic dispersionMedium (between 0.14 and 1.4 m)Good mechanical strength and flexibilityRisk of stress on soft substrates
Pliolite or solvent-borne resinLow to mediumGood adhesion on chalking substratesPoorly suited to damp masonry

The assessment of permeability is based on the water vapour diffusion-equivalent air layer thickness, commonly referred to as the Sd value. To ensure the durability of a façade renovation on traditional render, the Sd value of the dry film must be as low as possible, generally below 0.14 metre. Silicone resin paints combine a very open microporosity with an external water-beading effect that prevents liquid rainwater from penetrating, thus protecting the envelope from freeze-thaw cycles.

Finally, application on the construction site requires rigorous attention to the weather conditions prescribed by manufacturers and Romandy practice. According to the rules of the trade, exterior painting work is carried out on a dry substrate, at an ambient and substrate temperature between 8 °C and 30 °C, with a relative air humidity not exceeding 80%. Drying too fast in full sun or excessive humidity impairs the polymerisation of the film or the setting process of the silicate, compromising the expected microporosity.

Selecting binders and microporous suitability of the system

The choice of finishing system on an existing façade render does not depend on aesthetic considerations but on building physics. The underlying mineral render works as a moisture regulator: it absorbs moisture from time to time and must be able to release it freely to the outside in gaseous form. Applying a closed film causes water to accumulate under pressure at the render-paint interface. Under the effect of cycles of solar heating and cooling, the vapour pressure lifts the film, causing blistering and then the tearing off in sheets of the surface layers of the render.

To maintain the hygrothermal balance of the masonry, the technical rule requires that each coat applied towards the outside be more open to vapour diffusion than the substrate it covers. Coatings fall into three main families with distinct physical behaviours. Pure silicate or organo-silicate paints form a chemical bond by silicification with mineral substrates, ensuring maximum permeability without forming an impermeable film. Silicone resin paints combine a microporous structure highly permeable to water vapour with a high water-beading effect against driving rain. By contrast, film-forming acrylic dispersions drastically reduce gas exchange and remain prohibited on old, uninsulated lime or cement renders.

Technical behaviour of façade binders on existing renders
Binder familyWater vapour permeability (Sd value)Liquid water-repellent action (w value)Adhesion and mechanismCompatibility on existing mineral render
Pure or dispersed potassium silicateVery high (Sd below 0.05 m)Medium to good depending on formulationChemical petrification (silicification)Optimal on raw or cleaned mineral renders, incompatible over old organic paints
Silicone resin (siloxane)High (Sd below 0.14 m)Very high (strong water-beading effect, low w)Mechanical keying and flexible cohesionUniversal on fixed mineral renders or well-adhering old paints
Pure acrylic dispersionLow to medium (Sd often above 0.30 m)Medium (sealing through film formation)Superficial thermoplastic adhesionTo be reserved for stable substrates already painted with resins; high risk of delamination on breathable renders

Application requirements on the construction site and acceptance of the work under SIA 257

SIA 257 strictly governs the execution of painting and rendering work. Before starting to paint, the foreman checks the ambient weather conditions and the condition of the substrate. Applying a façade coating requires an ambient and substrate temperature between 8 °C and 30 °C, and a relative humidity below 80%. Work in direct sunlight in midsummer or in strong wind dries the binder prematurely, causing visible lap marks and impairing the silicification or coalescence of the polymers. If the façades have been cleaned by pressure washing or treated against algae and fungi, a waiting period of several days of dry weather is required so that the residual moisture content of the render drops below the admissible threshold in the technical data sheets.

  1. Testing and regulating impregnationCheck the strength of the repaired render and the complete disappearance of algae residues. Apply the microporous fixative or levelling primer with a façade roller or square brush, from bottom to top to avoid runs, making sure the grain is saturated without forming a surface film.
  2. Intermediate levelling coatApply a first coat of compatible façade paint, formulated with silicate or silicone resin. This structural coat fills the grain of the existing render, closes shrinkage micro-cracks and evens out the absorption of the substrate.
  3. Protective finishing coatAfter observing the drying time prescribed by the manufacturer (generally twelve to twenty-four hours), apply the finishing coat crosswise and smoothed continuously, from one edge to the other without interruption, in order to avoid any scaffolding marks or lap marks.

At acceptance of the work under SIA 257, the façade is assessed with the naked eye, under diffuse natural light, at a conventional distance of two to three metres, perpendicular to the wall. Shadow effects created by raking light in the morning or evening are not a criterion of non-conformity for the evenness of appearance of the paint on an existing floated or rustic render. On the other hand, lack of opacity, the presence of runs, immediate chalking or a manifest lack of adhesion revealed by a cross-cut test are execution defects that the contractor must rectify.

Managing defects: blistering, delamination and remediation protocols

The appearance of blisters, water pockets or flaking after a few months in service almost always signals a break in moisture balance: the water vapour permeability of the applied system is lower than that of the existing mineral substrate. When the water contained in the masonry migrates in gaseous form under solar radiation, the vapour pressure pushes the impermeable synthetic film, forming swellings that eventually burst. Likewise, a solvent-borne fixative applied in excess on a chalking render forms an impermeable glassy film instead of soaking into the pores, turning the bonding zone into a shear plane.

  1. Testing and stripping the impermeable filmPrick and scrape all blisters with a painter's knife. Remove all of the failing coating by hydro-sanding or chemical stripping if general adhesion is compromised.
  2. Treatment of micro-organismsSpray a residual biocide solution onto the exposed renders to neutralise algae and lichen spores embedded in the pores, then leave to dry for forty-eight hours.
  3. Penetrating fixation of chalking areasImpregnate the mineral render with a fluid consolidant based on potassium silicate or a highly dilutable acrylic hydrosol, without creating any residual gloss on the surface.
  4. Rebuilding an open system in accordance with SIA 257Reapply a microporous mineral or siloxane façade paint guaranteeing an sd value below zero point fourteen metre, ensuring continuous escape of water vapour flows.

Handling such a dispute requires a rigorous examination on the construction site with the site management. A blister should be cut open to analyse its underside: the presence of torn-off render grains shows an unconsolidated chalking substrate, while a clean film laden with liquid moisture betrays a microporosity problem. In accordance with the general principles of the Code of Obligations (CO) governing the contract for work, liability depends on compliance with the rules of the trade, on implementing the manufacturers' technical data sheets and on observing the weather conditions during application under SIA 257.

Frequently asked questions

How can you determine whether the chalking render is sufficiently consolidated before applying the finish?

Carry out the standardised adhesive tape test or rub the hand over several representative areas. If the palm stays clean with no transfer of mineral dust and the adhesive torn off with a sharp pull retains no particles, the impregnation has properly hardened the substrate. If the substrate still chalks or if the fixative has created a glossy film on the surface, the treatment must be corrected before painting.

Why does a mineral silicate paint rarely blister compared with an acrylic dispersion paint?

Potassium silicate paint does not form a closed film on the render; it petrifies with the mineral substrate by chemical silicification. This reaction creates an open porous structure that lets water vapour pass freely without giving any hold to internal gas pressures. Conversely, acrylic dispersion dries by coalescence, forming a continuous plastic film that acts as a barrier and blisters as soon as the render releases its moisture.

Can a solvent-borne fixative be applied to a façade that still shows traces of moisture?

This is strictly prohibited. A solvent-phase fixative applied on a damp render does not penetrate deeply into pores saturated with water. It remains trapped at the surface, forms a milky or glassy skin without cohesion and traps moisture in the masonry. The substrate must be perfectly dry to the touch and measured with a residual moisture content complying with the manufacturer's requirements to ensure complete and uniform capillary penetration of the binder.

Is it compulsory to strip the old paint if algae reappear after high-pressure cleaning?

Complete stripping is only required if the old film is peeling or if the micro-organisms have damaged the matrix of the underlying render. If adhesion remains firm, simple pressure washing does not destroy the microscopic roots of the cryptogams. A curative fungicidal biocide should be applied without rinsing, the product left to act, and then a breathable finishing system containing preventive protection agents against greening applied.

Texts and standards cited

  • SIA 257Painting and varnishing work: execution requirements, substrates and acceptance of the work
  • code des obligationsGeneral rules governing the contract for work, defects in the work and the duty of care

In the same section