Key takeaways
- Saturated transparent bases lack opacity and require a suitable grey or chromatic tinted undercoat.
- A deep red or a midnight blue often requires three finishing coats in addition to the undercoat.
- The stability of organic pigments requires careful selection to avoid deterioration under ultraviolet radiation.
- The quote must state the precise number of coats to rule out any unforeseen additional cost being borne by the painter.
Hiding power and tinted undercoat: controlling saturation without multiplying unnecessary coats
Vivid or dark colours, such as bright reds, sunny yellows or petrol blues, cannot be obtained from white bases loaded with titanium dioxide. They require transparent or semi-transparent dispersion bases that can take a high concentration of pigment pastes without whitening the final shade. This absence of opaque mineral fillers drastically reduces the initial hiding power of the dispersion. Trying to saturate a white or uneven substrate directly with a transparent base leads to serious technical problems: the substrate inevitably shows through, even after two regular cross-coats with a microfibre roller.
- Hiding power
- The ability of a paint film to mask the colour contrasts of the substrate to which it is applied, measured under professional rules by the contrast ratio at a given dry film thickness.
In addition to the intrinsic lack of opacity, the formulation of intense colours makes the work more sensitive to metamerism and ultraviolet radiation. The synthetic organic pigments commonly used to develop pure, vibrant reds or yellows have markedly lower resistance to photochemical ageing than mineral pigments based on iron oxides. Under direct natural light or right next to a glazed opening, a coat that is too thin suffers accelerated colour degradation and changes in appearance. Applying a neutral or matched grey undercoat beforehand not only improves the optical reading of the final colour, but also stabilises the overall durability of the film against continuous exposure to light.
| Colour family | Type of industrial base | Recommended undercoat | Natural hiding power |
|---|---|---|---|
| Carmine red / purple | Transparent base without titanium dioxide | Mid-grey tinted primer (approx. 30%) | Low (diffuse reflection) |
| Ultramarine / midnight blue | Semi-opaque or transparent base | Dark grey tinted primer | Medium to low depending on dilution |
| Cadmium / vivid yellow | Intermediate base with low filler content | Light ochre-yellow tinted primer | Very low due to transparency |
| Forest / emerald green | Pigmented transparent base | Broken-green or grey tinted primer | Medium |
Actual number of coats and contractual impact on the quote
In common practice on construction sites in French-speaking Switzerland, standardised descriptions traditionally specify two coats of matt or satin dispersion paint to finish a prepared substrate. This standard formula proves technically inadequate as soon as deep or very vivid colours are involved. Achieving a perfectly uniform finish, with no sheen variation, no repairs visible under raking light and with a depth of colour matching the sample, requires an application system comprising four successive operations: a regulating impregnation or calibrated tinted undercoat, followed without fail by three crossed finishing coats, carefully denibbed between coats. If this full system is not priced from the initial tender, the painter alone bears the cost of the additional materials and labour hours.
- Qualification of the colour under considerationIdentify the colour code from the standardised colour charts and check the formulation base with the supplier to verify the theoretical opacity.
- Contractual pricing of the serviceBreak down the tender item by explicitly detailing the specific tinted undercoat and the additional finishing coats.
- Making a reference sample areaApply a test panel on the actual substrate so that site management can formally approve the shade, the sheen and the degree of hiding.
The financial impact of a dark colour is not limited to the increased paint consumption due to the greater surface coverage. Application time rises in proportion to the intermediate drying times needed to avoid lifting resins that are still soft during successive coats. Under the Code of Obligations (CO) governing the contract for work and services and the provisions of standard SIA 118, the contractor cannot claim additional payment for work essential to proper execution if they knew the nature of the chosen colour before submitting their offer. Any additional coat applied afterwards as a fix on the construction site falls entirely under their own economic risk and erodes the profitability of the job.
Chemical stability of pigments and lightfastness of deep colours
The formulation of paints for saturated interior colours is subject to particular physical constraints. In a carmine red, a saffron yellow or an ultramarine blue, the manufacturer removes titanium dioxide from the formula and uses a transparent base (base C or TR). This white pigment provides the usual opacity of light-coloured paints through light scattering; its absence prevents the colour from being washed out into a pastel shade, but makes the dry film inherently translucent. Without a mineral opacifying filler, the dispersion acts as a coloured glaze that lets the contrasts of the substrate show through. This is why the prior application of a tinted undercoat in a calibrated neutral grey (graded from grey 1 to grey 5 according to the manufacturer's recommendations) is essential: this intermediate grey blocks differences in the ground and provides a uniform light-absorbing base on which the final colour can develop fully.
Colour durability under light exposure depends on the chemical nature of the pigments and the quality of the binder. While mineral oxides (iron oxides, silicates and natural earths) are unaffected by ultraviolet light, bright reds and intense yellows rely on synthetic organic pigments such as quinacridones, perylenes or azo derivatives. These molecules give remarkable colour brilliance but are vulnerable to photochemical degradation. Behind south-facing glazed openings or under interior glass roofs, solar energy combined with the temperature rise behind glass causes rapid fading if the pigments are not stabilised. The choice of binder also plays a protective role: a pure acrylic resin withstands ageing far better than a styrene-acrylic dispersion prone to yellowing. The painter must require pigments rated 7 to 8 on the blue wool scale to guarantee the durability of vivid colours exposed to natural light.
| Pigment family | Example colours | Natural hiding power | UV lightfastness |
|---|---|---|---|
| Mineral oxides and earths | Venetian red, burgundy, ochres | High (naturally opaque) | Excellent (unalterable) |
| Azo organics | Bright reds, intense yellows | Very low (semi-transparent) | Medium to low behind glazing |
| Polycyclic organics | Deep blues, purples, magentas | Medium (requires grey ground) | Very good (high resistance) |
Careful execution, burnishing effect and pricing of additional costs
On the construction site, dark colours accentuate the slightest imperfection in texture. Deep matt finishes are very prone to the burnishing effect: mechanical rubbing displaces the mineral fillers at the surface and leaves an irreversible glossy mark. In circulation areas, it is recommended to specify polyurethane acrylic resins or washable matt dispersions that limit polishing. Application requires 9 to 10 mm microfibre rollers and immediate cutting-in with a short-pile roller to blend out brush marks. It is essential to work panel by panel without interruption to keep a wet edge. In addition, the drying time between coats must reach 12 to 24 hours to avoid lifting the lower coats that are still fresh.
This technical reality requires the offer to be adapted from the tender stage. Discovering on site that a saturated colour requires a grey undercoat and three finishing coats causes a dead loss if the quote allowed for only two ordinary coats. Under standard SIA 118, the contractor informs the client of the constraints specific to the prescribed materials. The description must itemise each phase: the primer in the recommended grey, the three saturated finishing coats and the production of a contractual sample area. This sample in situ allows the uniformity of the film to be approved in writing and avoids subjective disputes at acceptance of the work.
The overall financial impact of a four-coat system for a deep colour represents an additional cost of the order of 40% to 60% compared with a standard two-coat white, owing to the volume of labour and the cost of pigments; the detailed calculation bases can be consulted at /soumissions/.
Handling disputes and repairs on saturated colours with insufficient coverage
When a vermilion red, a midnight blue or a saffron yellow shows shadows or mottling after two coats, the construction site comes to a halt. The classic mistake is to immediately apply a third coat not provided for in the offer in an attempt to mask the defect. This additional coat consumes labour and material with no guarantee of result if the ground has not been calibrated by an intermediate coat saturated with grey or a complementary shade.
If the visual result is not uniform, the site manager must stop the work. It must be checked whether the system described in the tender provided for a standard neutral primer or a tinted undercoat specifically formulated for the selected colour. Standard SIA 257 governs painting work and serves as the technical basis for judging the evenness of the surface appearance under the agreed raking or direct light.
- Joint inspection record of the transparencySummon site management to record the insufficient hiding power inherent in the chosen organic pigments, supported by the manufacturer's documentation showing the need for a grey base or a third finishing coat.
- Written notification for additional workSubmit an addendum form pricing the additional coat in accordance with the rules of standard SIA 118 before any further application on the disputed wall section.
- Making a reference sample areaProduce a one-square-metre sample area so that the gain in opacity and the absence of burnishing effect can be approved before extending the correction to all the rooms.
If the dispute concerns a change of colour made during the course of the work, the initial quote based on two coats of white or pastel no longer applies. Transparent bases loaded with pure organic colourants have a different solids content and a longer drying time. The contractor exercises their duty to notify by stating in writing that achieving the colour chart shade requires an additional, chargeable coat.
Frequently asked questions
Why does a bright red often require three finishing coats?
Saturated red lacquers or dispersions are based on translucent organic pigments. Unlike mineral pigments based on iron oxides, they lack intrinsic opacity. Even with a well-loaded microfibre roller, the dry film lets light through to the substrate. Application systematically requires a calibrated grey undercoat followed by three even coats to block refraction and achieve the exact saturation of the colour chart.
How can the extra cost of a dark colour be justified to the client?
The justification relies on the manufacturer's technical data sheet and the nature of the binders. A deep colour requires a more expensive transparent base, a high dosage of colourants and a tinted ground preparation. Labour time increases directly because of the number of coats required and the care needed to avoid visible repairs. These technical factors explain the additional cost priced in from the quote.
What colour of undercoat should be applied under a midnight blue or a black?
A dark colour must never be applied directly onto a white primer or bare plaster. Manufacturers pair each deep colour with a precise level of neutral grey primer, often graded from one to five. For a midnight blue or a deep black, an undercoat tinted mid-grey or anthracite grey extinguishes the ground and guarantees a finish without shade variation from the second finishing coat.
How can the burnishing effect be avoided on a dark matt wall in a corridor?
On a deep matt finish, the slightest mechanical rubbing brings silica fillers to the surface, causing irreversible whitish streaks. For circulation areas, it is recommended to specify a washable matt paint reinforced with polyurethane or based on pure acrylic resin. The painter must apply the product in crossed coats without reloading the roller over areas that are starting to set, in order to preserve uniformity.
Texts and standards cited
- norme SIA 118General conditions for the execution of construction work, handling of change orders and additional work
- norme SIA 257Painting work, surface quality requirements, appearance tolerances and conditions for acceptance