Key takeaways
- Choosing a species without sapwood determines biological resistance to climatic attack.
- Orientation and roof overhangs inevitably create differences in appearance across the walls.
- Factory pre-greying anticipates surface oxidation and limits visual contrasts between façades.
- A clear maintenance plan commits the client to the frequency of later interventions.
Qualify the species according to its natural durability and the exposure of the building
On a ventilated cladding falling under CFC 221, longevity depends first of all on the natural durability of the heartwood and the strict absence of sapwood on exterior facing surfaces. In French-speaking Switzerland, native species such as mountain larch, sapwood-free Douglas fir or thermally treated spruce meet the usual demands of a ventilated façade without requiring deep biocidal treatment, provided that the construction design ensures rapid drainage of runoff water and continuous ventilation of the air cavity.
- Natural durability of wood
- Intrinsic capacity of the heartwood of a species to resist attack by wood-destroying organisms (basidiomycete fungi, wood-boring insects) without the addition of a chemical preservative.
The ageing of untreated timber cladding is a purely surface phenomenon: ultraviolet radiation degrades the lignin at the surface, then rainwater washes away these decomposed components, revealing the greyish cellulose microfibres. This change of colour in no way alters the mechanical properties of the cladding board. However, the unevenness of this greying is the leading source of complaints if it has not been explained beforehand.
| Species | Natural durability of heartwood | Greying behaviour | Installation precautions |
|---|---|---|---|
| Alpine larch | Durable to moderately durable | Silvery greying to dark patina | Remove all sapwood; pre-drilling recommended to prevent splitting |
| Douglas fir | Moderately durable | Gradual greying with initial pinkish tones | Select sapwood-free timber; high resin content |
| Swiss spruce | Slightly durable | Rapid greying, mottling under driving rain | Impregnation treatment or extensive structural protection |
| European oak | Durable | Dark grey colour, leachable tannins | A4 stainless steel fixings mandatory to avoid black streaking |
Deciding between pre-greying, saturator and maintenance contract
To avoid the disappointment of a mottled visual transition over several seasons, workshop application of a pre-greying finish using a water-based non-film-forming stain is the reference solution. This initial treatment saturates the pores with grey mineral pigments that fade as natural oxidation takes over. The façade thus keeps a balanced tone from installation and throughout its transition.
If the client requires the original colour of freshly sawn timber to be maintained, the contractor must formally document the resulting maintenance burden. Saturators and tinted oils without a film require a new maintenance coat every two to four years depending on weather exposure and altitude, failing which partial flaking or indelible stains may occur. The work then requires scaffolding or aerial platforms to refresh the surfaces.
- Pre-greyed finish: requires no later corrective maintenance, the natural patina replacing the factory pigments.
- Clear or tinted saturator: requires gentle annual brushing and periodic reapplication without prior sanding.
- Semi-film-forming stain: prohibited on heavily exposed cladding because of the risk of blistering, which requires complete stripping.
- Raw timber without finish: requires formal acceptance of marked contrasts during the first years of exposure.
Under art. 365 CO, the contractor is obliged to notify the client where the materials chosen or the instructions received risk causing defects or results contrary to the expectations expressed. Handing over a signed technical information sheet before final award protects the company against claims for remedial work based on the natural aesthetic change of the timber.
Kinetics of greying under differential exposure
On a ventilated envelope, the ageing of timber is not a material defect but a photochemical reaction combined with surface leaching. Ultraviolet radiation degrades lignin into soluble compounds, which rainwater gradually removes, revealing the grey cellulose framework. This transformation immediately runs up against the geometry of the building: a façade never receives the same weather load on all its faces. In the Swiss climate, in lowlands as in mountains, south-west faces suffer direct driving rain and maximum sunshine, accelerating the patina within a few months. Conversely, a north façade or walls recessed under deep eaves keep their original colour for several years, creating marked visual differences.
| Exposure zone | Dominant stresses | Colour kinetics | Long-term appearance |
|---|---|---|---|
| West / South-West façade | Driving rain, thermal shocks, intense UV | Rapid greying (6 to 18 months), strong leaching | Even silvery grey to medium grey |
| North façade | Residual moisture, diffuse light, no direct UV | Very slow change (3 to 6 years), risk of soiling | Dull grey, greenish tints if ventilation is poor |
| Sheltered areas (soffits, upper bands) | No driving rain, indirect radiation | Prolonged persistence of the original golden or brown colour | Sharp demarcation with the washed areas |
| Façade base (splashback) | Droplet rebound, short wetting-drying cycles | Localised blackening, accelerated surface degradation | Uneven dark grey with mineral deposits |
Roof projections, continuous balconies, window reveals and sheet-metal copings cast rain shadows. Directly under a drip edge, the timber stays dry and keeps its original pigments, whereas fifty centimetres lower down, clear runoff bleaches the fibre. This sharp boundary often surprises the uninformed client, who wrongly interprets it as a failure of the product or of the installation. The design of the sheet-metal flashing details must include clean drip edges and regular overhangs to avoid slanting streaks caused by the prevailing wind.
Formalising the agreement and prior information protocol
For the façade installer, defusing a complaint about appearance requires a rigorous approach before the profiles are ordered. Signing an appearance protocol annexed to the works contract makes it possible to formalise the living nature of the substrate. The Code of Obligations provides that the client notifies defects after delivery; for a building work, art. 367 CO specifies that the client has 60 days to do so. However, a colour change inherent in the natural cycle of the material is not a defect if it was described and accepted in writing at the tender stage.
- Presentation of samples aged in situSubmit reference samples showing both states: the colour when new, planed or finely sawn, and the stabilised appearance after three years of outdoor weather exposure.
- Descriptive notice of transition zonesRecord on the execution drawings the foreseeable demarcation lines created by eaves, sun-shading devices and masonry set-backs.
- Deciding on the pre-greying finishPropose in the specification the workshop application of a mineral impregnation or a grey non-film-forming saturator in order to even out the colour transition across all orientations.
- Handover of the maintenance planDefine the frequency of inspections of the air cavities, dry dusting or gentle brushing, and recall the strict prohibition of high-pressure cleaning, which destroys the surface network of the wood fibres.
Choosing a system without finish means accepting a transitional phase of mottling lasting between one and three years depending on altitude and microclimate. If the client requires a lasting or constant colour, the specification must shift to a tinted microporous saturator with a maintenance commitment every three to five years on exposed faces, or to an industrial pre-patina applied in the factory. This choice affects overall operating costs: the initial treatment adds a cost of around CHF 25 to 45 per square metre installed, plus periodic refreshing work (see /soumissions/ for the full life-cycle cost assessment).
Managing appearance disputes and technical remedies
When the client disputes the appearance of the cladding during patina formation, the site manager first checks the integrity of the envelope. A colour variation is not a defect if the rules of good practice for ventilated cladding have been respected. The first step is to measure the moisture content of the boards with a calibrated pin-type moisture meter, then to check the free circulation of air in the ventilated cavity behind the façade.
If the client refuses acceptance, citing a visual defect under the eaves or at corner junctions, the contractor refers to the agreed contractual requirements. Art. 367 CO provides that the client checks the state of the work and notifies defects to the contractor, and either party may request an examination by experts. The appointed expert will then distinguish physical deterioration from a natural reaction to ultraviolet rays and rainwater.
- Joint inspection record on scaffolding with a hygrometric reading of the boards and a check of the upper and lower ventilation openings.
- Local application of an oxalic acid de-greyer on a sheltered test area to determine whether the original colour can be restored before any overall rework.
- Proposal of a pigment equalisation treatment if the unevenness between the South-West and North orientations disrupts the use of the building.
If agreement is reached on an aesthetic restoration, the work is formalised by a written addendum. If the dispute persists over the conformity of the material supplied by the company, art. 365 CO recalls the façade installer's responsibility for the good quality of the material delivered. The sample file approved during site preparation remains the pivotal document of the technical defence.
Frequently asked questions
What should be done about black streaks below window sills?
These streaks come from a concentration of runoff water leaching dust and tannins in an area sheltered from UV. First check the slope and water-shedding of the metal flashing. If the flashing does not project far enough beyond the face of the timber, correct the drip fold. Then clean the stained area with diluted oxalic salt, rinse at low pressure and let it dry completely.
Can a saturator applied at installation be discontinued without later sanding?
Yes, provided it is a non-film-forming, open-pore product. Unlike a conventional stain, a quality saturator wears away under the weather without forming flakes. The owner may decide to stop the periodic maintenance coats. The timber will then begin its natural greying gradually and evenly, without requiring heavy stripping or mechanical sanding of the façade.
How should a marked colour difference between two façades of the same building be handled?
The kinetics of oxidation depend directly on driving rain and ultraviolet radiation. The South-West façade greys within a few months while the North face keeps its brown pigments much longer. To correct this difference without sanding, apply a non-film-forming pre-greying stain to the lagging face. This matt product immediately stabilises the silver-grey shade and evens out all the exterior volumes of the building.
Can the client demand replacement of boards showing checks?
Shallow surface splits caused by wetting and drying cycles are normal behaviour of the material outdoors. They do not justify any replacement as long as they do not compromise the mechanical fixing to the framework, do not pass through the thickness of the profile and do not cause standing water retention. A simple joint examination of the depth of the splits is enough to reject the classification as a material defect.
Texts and standards cited
- CO art. 365material and ground: the contractor is responsible for the good quality of the material he supplies; if the material supplied by the client or the ground designated by him is found to be defective, or if another circumstance jeopardises the proper or timely execution of the work, he must immediately inform the client, failing which he bears the consequences (para. 3).
- CO art. 367after delivery, the client checks the state of the work as soon as he can and notifies defects to the contractor; for a building work, he has 60 days to notify them and a shorter contractual period is void (para. 1bis, in force since 1 January 2026); either party may request an examination by experts (para. 2).