Key takeaways
- Sorting slates by thickness beforehand ensures a flat bearing surface and optimum watertightness.
- A clear sound when struck confirms the absence of internal microcracks in the material.
- The headlap varies strictly according to the slope pitch and exposure to the weather.
- The hook length must correspond to the exact headlap value plus three millimetres.
Sorting, sound and grain direction of natural slate
Natural slate is a schistose material quarried from rock, and its physical characteristics vary from one piece to another. Before installation on the roof, the roofer must systematically sort the pallets. The first selection criterion is grading by thickness. Slates are divided into three categories: thick pieces (used at the eaves and verges), medium-thickness pieces (laid in the body of the roof slope) and thin pieces (reserved for the top of the slope). This sorting avoids unevenness between neighbouring pieces, known as "pairs", which allow wind-driven water to infiltrate and risk breaking the upper slate under the pressure of the hook.
The sound of the slate is checked by lightly tapping the piece with the back of the slater's hammer. A clear, crystalline sound indicates sound, dense rock free of microcracks. A dull or flat sound reveals an internal flaw, friable grain or the presence of through-going pyrite, making the material unfit for roofing. At the same time, the journeyman identifies the grain direction (the cleavage). Water must run in the axial direction of the veins of the slate. Laying across the grain retains residual moisture, encourages moss growth and accelerates frost damage to the stone in winter.
| Category | Average thickness | Acoustic test | Location on the roof |
|---|---|---|---|
| Thick | 7 mm to 9 mm | Clear metallic sound | Doubling course, eaves, verges, valleys |
| Medium | 4 mm to 6 mm | Clear sound | Main roof covering, full slope |
| Thin | 3 mm to 4 mm | Clear high-mid sound | Ridge course, top of slope |
Headlap calculation, hook fixing and water run-off
The headlap value corresponds to the height of the zone where three thicknesses of slate overlap. This dimension depends directly on the pitch of the slope, the length of the horizontal projection of the roof slope and the exposure of the site (sheltered, normal or exposed). The lower the pitch, the greater the headlap must be to prevent water rising by capillarity and wind action. The exposed length (gauge) — the visible part of the slate that receives the rain — is calculated by subtracting the headlap from the total height of the slate, then dividing the result by two. The battening of the substrate is carried out according to this theoretical gauge.
- Headlap
- Minimum height over which a slate covers the piece of the course below and is itself covered by the piece of the course above, ensuring watertightness against driving rain.
Fixing with metal hooks (A2 stainless steel, or A4 in aggressive environments) replaces traditional nailing on battens. The hook length is calculated using the formula: hook length equals the headlap value plus 3 mm for clearance of the tip. The shank of the hook sits in the exposed length of the underlying slate, while the heel (the curved tip) holds the base of the upper slate. The hook point must be driven firmly into the timber without splitting the batten.
- Setting out and batteningMark the vertical and horizontal setting-out lines on the roof boarding or underlay, observing the calculated gauge.
- Laying the doubling course at the eavesFix the short eaves slates (cut to a third) under the first course to double the first headlap above the eaves board.
- Engaging the hooksDrive the hook point into the upper face of the batten at the vertical marking.
- Sliding in and clamping the slateInsert the slate into the heel of the hook, taking care to centre it in relation to the shank so as to leave a lateral clearance of one millimetre.
During installation, the alignment of the slate bevels ensures a clear drainage channel. The vertical joints of two consecutive courses must be strictly staggered by half the width of the piece (full-bond laying). In areas subject to severe climatic loads, the contractor checks that the load-bearing structure complies with safety requirements. The employer takes the necessary measures to prevent falls from a height in application of the Code of Obligations and the Ordinance on Construction Work, by providing a roofer's scaffold bridge or a suitable guardrail.
On roofs, appropriate measures must be taken to prevent falls from a fall height of more than 2 m.
art. 41 OTConst
Sorting on the construction site and grading of the material
The success of a natural slate roof depends on careful preparation of the pieces on the ground or on the loading platform. Slate is a fissile material extracted from metamorphic rock and shows natural variations in flatness and structure. Sorting beforehand allows thicknesses to be divided into categories to avoid unevenness and guarantee a stable bearing on the battens.
Each slate is checked against three basic criteria: sound, flatness and grain direction of the stone. The roofer's hammer (with anvil) is the everyday tool for testing sound and for hand-cutting verges and gauges.
- Sound test: A sound slate with no microcracks gives a clear, crystalline sound when struck with the hammer. A dull or muffled sound indicates a through-going pyrite vein, altered grain or an internal crack; the piece must be rejected.
- Grain direction (long grain): Cutting and notching must follow the natural cleavage of the stone. Working parallel to the grain guarantees a clean edge without unwanted shouldering.
- Elimination of defects: Knots, progressive pyrites or limestone inclusions are cut out or relegated to verge and eaves cuts.
Headlap calculation, hook fixing and water run-off
The sizing of the headlap determines the overall watertightness of the pitched roof. It is established according to the roof pitch, the climatic wind-exposure zone and the length of the slate selected. An underlay complying with the requirements of CFC 224 supports the work beneath the counter-battening.
| Slope pitch | Sheltered / Normal site | Exposed site (wind / altitude) |
|---|---|---|
| Low pitch (30° to 40°) | 90 mm to 100 mm | 110 mm to 120 mm |
| Medium pitch (40° to 50°) | 80 mm to 90 mm | 90 mm to 100 mm |
| Steep pitch (> 50°) | 70 mm to 80 mm | 80 mm to 90 mm |
Fixing with stainless steel hooks (AISI 316 / 1.4401 stainless steel at altitude or in aggressive environments) guarantees superior mechanical hold against climatic loads. The hook is fixed to the batten or the eaves batten. Its point must penetrate firmly into the timber without splitting it, and the heel (tip of the hook) must grip the bottom of the slate without excessive constraint so as to allow for expansion.
- Setting out the gauge and batteningCalculate the visible gauge: $P = (H - R) / 2$, where $H$ is the height of the slate and $R$ the headlap adopted. Mark the gauge lines on the counter-battening.
- Laying the doubling course and the eavesFix the eaves board and lay the doubling course (cut slates) to close the first gauge at the metal eaves flashing strip.
- Fixing the hooks and laying upwardsDrive the hook into the batten along the chalk line. Lay the slate by sliding its foot into the heel of the upper hook, taking care to centre it between the two lower pieces.
- Checking for perfect run-offCheck the lateral offset of the vertical joints (bonding at mid-width) to prevent water rising by capillarity towards the battens.
In accordance with the Code of Obligations (art. 365 CO), if the plumber or roofer finds a defective eaves board support or battening installed by another trade, they must immediately inform the client in writing. As regards occupational safety on roofs, art. 41 OTConst requires perimeter guardrails and roofer's scaffold bridges to be put in place as soon as the fall height exceeds 2 metres.
Handling substrate non-conformities, slate sorting and laying defects
Installing a natural slate roof demands constant vigilance in the face of unforeseen events on the construction site. As soon as the gauges are set out, any deformation of the roof structure or any deviation in the flatness of the battening exceeding the tolerances of standard SIA 232/1 compromises watertightness against water and powder snow. In accordance with the general principles of contract law set out in the Code of Obligations (art. 365 CO), the roofer-plumber has a formal obligation to report any substrate anomaly in writing to the client or the site manager immediately, before laying the first course.
- Identifying the substrate or material defectNote any batten misalignment, and slates showing through-going pyrites, curved grain or a dull sound when struck with the slater's hammer.
- Written notification and stopping the affected workDraft a notice of defect stating the deviations measured. Stop laying in the non-conforming area until the site management has made a decision.
- Laying repairs and replacement with hooksTo replace a cracked element on a roof laid with stainless steel hooks, use the nail puller to release the defective piece, check the hook heel, then slide in the new slate, previously selected by thickness.
Strict compliance with the construction waste disposal process, required by the Ordinance on the Avoidance and the Disposal of Waste (OLED), requires source separation of copper or zinc plumbing offcuts and slate debris. For detailed pricing of repair work and daywork, refer to the section /soumissions/.
Frequently asked questions
How should you react if sorting reveals more than 10% cracked pieces in a pallet?
Stop unpacking immediately, document the batch with clear photos and draw up a reservation note for the supplier. Do not lay any suspect piece. The foreman must inform the site management so that a replacement pallet can be arranged, otherwise the pace of work on the construction site will slow and the overall quality of the work will be compromised.
What should you do if the actual pitch of the roof structure is lower than shown on the plans?
The headlap of the slate depends directly on the slope pitch and the snow zone. If the pitch measured on site is lower than planned, recalculate the gauge immediately. Insufficient headlap leads to water rising by capillarity. Notify the site management of the change in gauge before setting out the eaves batten.
How do you correct a hook that is too short or misplaced after the lines have been set out?
A hook of unsuitable length no longer guarantees the minimum grip of the heel on the head of the underlying slate. Remove the defective hook with a punch or a batten crowbar, then reposition a stainless steel hook of the correct length (generally equal to the headlap plus 3 to 5 mm).
How do you replace a broken slate in the middle of a slope already laid with hooks?
Use a nail puller to lift the upper elements slightly and swivel the retaining hook. Release the broken piece. Select a new slate of strictly identical thickness, slide the piece in as far as the stop of the lower hook, then return the upper hook to its axial position to lock the side lap.
Texts and standards cited
- code des obligations art. 365material and ground: the contractor is responsible for the good quality of the material he supplies; if the material supplied by the client or the ground designated by him is found to be defective, he must immediately inform the client.
- OTConst art. 41measures to be taken at roof edges: appropriate measures to prevent falls from a fall height of more than 2 m.
- SIA 232/1Pitched roofing - Technical requirements and tolerances
- OLEDOrdinance on the Avoidance and the Disposal of Waste