🧱 CFC 224Sarking, ventilation and underlay membraneChapter 2 of 10 in the section

Roofing underlay: watertightness class, laying tension and overlap

This chapter details the selection criteria and execution rules for an underlay on a pitched roof according to SIA 232/1. You will learn to identify the required watertightness class from the pitch and exposure, to calibrate the tension of the sheets so as to guide water away from the fixings, and to make watertight overlaps able to withstand accidental infiltration and condensation.

Key takeaways

  • SIA 232/1 classifies underlays according to the roof pitch and exposure to the weather.
  • A pitch below the prescribed minimum pitch requires the adoption of a more demanding underlay class.
  • A laying sag of ten to twenty millimetres channels the water to the centre of the span.
  • Sealing strips nailed beneath the counter-batten protect the mechanical perforations against residual infiltration.

Identifying the watertightness class according to pitch and climatic exposure

In roofing work on pitched roofs (CFC 224), the roofing underlay is not a remedy for poor roof design. Its role is to provide a second line of defence against powder snow, condensation under tiles and accidental infiltration. SIA 232/1 classifies underlays according to three criteria: the pitch of the roof slope, the minimum pitch of the roofing material and the level of local climatic loads.

SIA 232/1 distinguishes three levels: normal, increased and extraordinary loads. A roof is subject to increased loads once the altitude exceeds 800 metres, on a windy ridge or when the geometry multiplies valleys and hips. If the pitch of the slope is below the minimum pitch of the tile, adopting a more demanding underlay class becomes an unavoidable technical obligation.

Underlay classes and application criteria according to SIA 232/1
Underlay classWatertightness requirementSlope pitch criteriaSubstrate and installation
Normal loadsGravity drainage without standing waterPitch greater than or equal to the minimum roofing pitchLoose-laid over rafters or over continuous rigid insulation
Increased loadsWatertightness under moderate water pressurePitch lower, down to 6° below the minimum pitch of the materialContinuous rigid substrate with sealing strip under counter-batten
Extraordinary loadsTotal watertightness equivalent to a flat roofVery low pitches or altitude above 1000 metresClose-boarded sheathing with heat-welded or cold-bonded membrane

In Alpine and Jura areas, snow accumulations at the bottom of the slope cause a blockage phenomenon during winter thaws. Meltwater meets the ice blocks formed in the gutters and rises back under the tiles. To prevent any rotting of the rafter foot, the connection at the eaves is made on a ventilated sheet-metal strip, bonded to the underlay with a suitable butyl adhesive.

Adjusting the laying sag, the counter-batten and the bridging of the overlaps

The service life of the underlay and of the roof structure depends directly on how water is guided towards the eaves. Stretching a sheet like a drumskin is a common mistake: run-off and condensation water then butts directly against the sides of the timber counter-battens. This prolonged contact leads to biological rotting of the counter-battening and allows moisture to seep through the perforations made by the fixing nails.

This sag of 10 to 20 mm creates a natural drainage channel at the centre of each interval between rafters. The ventilation counter-batten, whose minimum thickness of 45 to 50 mm ensures continuous air circulation under the tiles, must always be backed with a nail sealing strip on its underside. This closed-cell elastomer foam tape wraps around each threaded shank or galvanised nail, neutralising the risk of leaks caused by the mechanical piercing of the sheet.

  1. Unrolling and forming the sagUnroll the sheet parallel to the gutter and staple it onto the top of the rafters at the upper part, maintaining a regular curvature of about 15 mm in the span.
  2. Fitting the nail seal under the counter-battenFix the compressible sealing strip along the full length of the counter-batten before nailing it to the rafter, ensuring watertightness of the piercing.
  3. Aligning the horizontal overlapsOverlap the upper sheet by at least 100 mm for steep pitches, and by at least 150 mm for shallow pitches, aligning with the printed markings on the sheet.
  4. Bonding and rolling down the jointsRemove the silicone film from the integrated adhesive or apply a system adhesive with a gun, then press the joint firmly with a roller to ensure a continuous bond.

Vertical overlaps must always be located on the axis of a rafter, never in a free span. They are sealed with a watertight adhesive tape before being clamped under the counter-batten. Against walls, dormers or protrusions, the underlay is turned up at least 150 mm above the roofing plane, held by a mechanical fixing batten and connected with a solvent-free sealing paste.

Joining sheets and treating penetrations according to SIA 232/1

To meet the requirements of SIA 232/1, the continuity of the underlay does not rely on simply overlapping the strips. Under heavy exposure or on a low pitch, increased and extraordinary loads require a joint that is watertight to water and wind. Two technologies dominate: bonding with acrylic adhesive strips for flexible polypropylene (PP) underlays, and homogeneous welding for thermoplastic polyurethane (TPU) or polyolefin (FPO) membranes. Hot-air welding is carried out with a manual hot-air tool fitted with a 40 mm flat nozzle, with rolling down using a silicone roller. Cold chemical welding is carried out by capillary action using a tetrahydrofuran swelling agent, applied carefully with a brush or dosing bottle.

Methods of joining underlay sheets according to the watertightness class of SIA 232/1
Load class (SIA 232/1)Underlay materialBridging methodMinimum overlap width
Normal loadsFlexible breathable polypropylene underlayIntegrated or added acrylic adhesive tape100 mm
Increased loadsReinforced synthetic membrane (PP or TPU)Double adhesive strip or system adhesive100 mm
Extraordinary loadsWeldable membrane (TPU / FPO) or bituminousHot-air thermal welding or cold chemical welding100 mm to 150 mm

Roof penetrations are the most exposed singular points. Whether it is a waste-water vent, a ventilation duct or a masonry chimney, a rough cutter cut without an upstand causes infiltration. The tradesperson cuts an envelope-style opening, raises the flaps along the shaft by at least 100 mm and bridges the junction with an EPDM elastomer sleeve or stretchable butyl sealing strips. Upstream of any penetration wider than 200 mm, fitting a deflector flashing sloped towards the neighbouring span is essential: this diverter valley guides condensation flows and accidental water downwards without forming standing water.

Eaves line, nailing strips and connection to sheet-metal work

Mechanical fixing of the ventilation counter-battens creates hundreds of perforations on each roof slope. During heavy rain or the winter thaw, these nail holes become infiltration paths towards the roof structure and the insulation. Under increased or extraordinary loads within the meaning of SIA 232/1, a 50 mm wide sealing strip under the counter-batten in closed-cell polyethylene foam or butyl mastic is required. This compressible strip is applied under the counter-batten or directly onto the rafter before nailing, ensuring a watertight and elastic seal around each metal nail.

At the eaves, the connection between the underlay and the sheet-metal work requires a rigid eaves support. The lower sheet must never dip directly into the throat of the gutter or hanging gutter: standing moisture and ultraviolet rays would degrade the membrane within a few months. The roofer fits a bevelled eaves fillet fitted with a copper or zinc metal drip edge. The underlay covers the upper flange of the drip edge and is bonded to it with double-sided butyl tape, stopping 20 mm from the drip fold. This arrangement drains underlay water without obstructing air entry under the counter-battens.

Work along the lower edge places workers facing the open drop. Art. 41 OTConst provides for appropriate measures to prevent falls from a fall height of more than 2 m (roofer's catch platform and/or perimeter guardrail depending on the roof pitch). Roofers and sheet-metal workers check the condition of these collective protections before fixing the eaves fillets and rolling down the eaves sheets, thus making the working area safe along the entire lower edge.

Managing non-conformities and damage on the roofing underlay

On a roofing construction site, defects affecting the roofing underlay frequently appear before the tiles are laid or during the first heavy rain episodes. A mechanical tear caused by a dropped tool, excessive tension without a drainage sag or delamination following prolonged exposure to ultraviolet rays compromises the water-drainage function of the secondary protection layer defined by SIA 232/1.

  1. Recording and documenting the defectAs soon as standing water under a counter-batten or infiltration at a rafter is spotted, the crew stops roofing the slope concerned. The condition of the substrate, the adhesion of the bridging strips and the actual watertightness class are recorded in writing with a photographic survey.
  2. Making the workstation safeAny corrective work on the slope requires appropriate measures to prevent falls from a fall height of more than 2 m according to art. 41 OTConst. Personnel check the presence of the roofer's catch platform before unloading or removing the counter-battens.
  3. Redoing overlaps and bridgingIf the laying sag is insufficient, water seeps along the nailing perforations. The counter-battens concerned are dismantled to insert closed-cell foam sealing strips under the counter-batten and restore the 10 to 20 mm sag between rafters. A piece of new sheet is slid under the upper sheet with a minimum overlap appropriate to the pitch.
  4. Drainage check before closing upA hose test without pressure is carried out from the ridge to check that there is no water retention upstream of the penetrations and to confirm that water runs clearly off towards the sheet-metal flashing at the foot of the slope.

If exposure to the weather exceeds the maximum duration permitted by the manufacturer, often set at eight or twelve weeks, the membrane loses its dynamic watertightness properties and its mechanical strength. The site manager must then order the complete replacement of the damaged sheets rather than multiply precarious patch repairs, which engage the company's liability when the works are handed over.

Frequently asked questions

How do you correct a roofing underlay laid too tight between the rafters?

An overly tight membrane holds water against the edges of the counter-battens and promotes infiltration through the fixing nails. To correct this defect, remove the counter-battens concerned, fit a nailable foam sealing strip under the counter-batten, then reform a laying sag of 10 to 20 mm at the centre of the span to guide condensate towards the free axis.

Which underlay class should be applied for a low-pitch roof in an Alpine area?

SIA 232/1 requires the class to be adapted to the climatic loads and to the minimum roofing pitch. At altitude, snow load and the risk of ice dams create increased requirements. An underlay for extraordinary loads is then prescribed, made by thermal welding or bonded bridging strips on a continuous rigid substrate.

Can a torn underlay sheet be joined with a simple adhesive tape?

No. Standard site adhesives lose their tack under the effect of moisture and temperature variations. A tear requires a system adhesive tape certified by the underlay manufacturer, with a pure solvent-free acrylic adhesive resistant to ageing. If the cut exceeds 50 mm, a coupon of membrane is inserted under the upper sheet before bonding around the perimeter.

Why fit a sealing strip under the counter-battens screwed onto the underlay?

Each perforation by nail or screw is a potential water path when the underlay is loaded by meltwater or driving rain. The sealing strip under the counter-batten, made of watertight cellular foam, compresses during mechanical fixing and plugs the hole around the metal shank, preventing water from travelling to the rafter.

Texts and standards cited

  • SIA 232/1Underlays, small-element roofing and linings of pitched roofs
  • OTConst art. 41measures to be taken at roof edges: appropriate measures to prevent falls from a fall height of more than 2 m (roofer's catch platform and/or perimeter guardrail depending on the roof pitch); on roofs with a pitch of more than 60°, work only from scaffolding or a mobile elevating work platform (para. 3)

In the same section