Key takeaways
- The front apron flashing must always be laid before the cheek soakers and the tiles.
- The cheek foot is the critical low point where any backflow of water penetrates.
- The side soakers are slid in one by one with each course of roof covering laid.
- The dormer's ventilation must remain completely independent of the air circuit of the main roof slope.
Laying sequence of the four flashings and treatment of the low point
Carrying out the metal roofing work of a dormer on a pitched roof tolerates no disorder in the sequence of operations. Four distinct drainage systems meet in a confined area: the front apron flashing at the bottom, the side valleys or drainage channels upstream, the cheek flashings on the roof slopes and the under-roof ventilation. Errors in the overlapping of these elements are the most frequent damage in pitched-roof metalwork, creating a water trap that is invisible from the outside.
- Front corner piece
- Shaped or soldered sheet-metal piece ensuring the watertight transition between the front apron flashing laid over the exposed tile surface and the first side upstand of the dormer cheek, preventing water from penetrating under the first course of tiles.
- Laying the front apron flashingThe apron flashing, made of zinc, copper or pleated lead, is fixed to the dormer sole plate or the window sill. Its strip runs down over the roof covering with a minimum overlap determined by the roof pitch. It must discharge the water from the front face directly onto the upper surface of the lower course of tiles.
- Shaping and connecting the lower cornersAt the junction between the bottom of the cheek and the front face, the fold forms a critical internal angle. The connection requires a watertight weld or a folded-back corner fold without piercing cuts, in order to prevent capillary rise under the effect of the prevailing wind.
- Staggered laying of the soakers or the side channelDepending on the roofing material, either individual soakers are laid, interleaved between each element (slates, plain tiles), or a double-fold cradle channel is laid along the cheek. Laying is carried out strictly from bottom to top, each element overlapping the previous one.
- Junction of the upper valleyThe valley that collects water from the main roof upstream of the dormer opens out above the head of the cheek. Its discharge must direct the water into the side channel or onto the roof covering without ever butting against a straight fold of the cheek flashing.
The major weak point is systematically located at the lower corner of the dormer, where the main roof slope meets the front face. If the front apron flashing is slid under the first soakers without a raised corner piece, water driven back by the wind or the volume guided by the side valley accumulates on the timber lintel. Art. 229 CP punishes anyone who, when managing or carrying out a construction, intentionally breaches the recognised rules of the trade and knowingly endangers the life or physical integrity of persons, a provision that recalls the rigour required in the face of structural failures caused by continuous water infiltration.
Connecting the cheeks, routing the valleys and maintaining ventilation
The connection of the cheeks to the roof slope depends on the waterproofing system chosen. On interlocking tiles or pantiles, the use of a recessed side channel with lateral discharge prevents the troughs from clogging. On plain tiles or natural slate, the use of concealed metal soakers offers optimal protection against powder snow. In both cases, the vertical upstand against the cheek must measure at least 120 to 150 mm depending on the wind zone, protected at the top by a counter-flashing strip or chased into the cheek cladding.
| Waterproofing element | Minimum roof pitch | Vertical upstand height | Horizontal overlap width |
|---|---|---|---|
| Front apron flashing | From 15° | 100 mm against the dormer | 150 to 200 mm over the tiles |
| Side cheek soakers | From 25° | 120 mm minimum | Width of exposed tile surface + 30 mm |
| Recessed channel with discharge | Less than 25° | 150 mm with clip | 120 mm under the roof covering with edge |
| Dormer head valley | According to pitch of the main roof slope | 150 mm under the counter-battens | 200 mm on each side of the axis |
Interruption of the ventilation air gap by the body of the dormer is a frequent cause of hygrothermal damage. The counter-battening of the main roof stops against the dormer framing, blocking the rising airflow. It is essential to interrupt the battening under the lower trimmer to create an air inlet under the metal channel, and to fit ventilation tiles or a screened opening on the underside of the dormer eaves.
When working on the cheeks and dormer roofs, the risk of slipping on folded sheet metal or on wet tile surface calls for particular vigilance. Art. 41 OTConst prescribes appropriate measures to prevent falls at roof edges from a fall height of more than 2 m, including the roofer's working platform or a perimeter guardrail depending on the pitch; these protections eliminate any risk when shaping the corner flashings.
Sequence of the four flashings and control of the eaves low point
On a dormer on a pitched roof, watertightness management relies on the assembly of four distinct works: the front apron flashing, the connection of the cheeks to the roof slope, the side connecting valleys and the dormer's air vent or ventilation device. The classic error on construction sites is to lay the elements according to ease of access rather than strictly in the direction of gravity-driven water flow. Reversing this sequence inevitably creates a re-entrant sheet of water or a retention bottleneck at the meeting point between the base of the cheeks and the main roof slope.
The most vulnerable point of the work is at the lower front corner, where the vertical cheek meets the front apron flashing and the eaves bed of the first row of tiles. If the apron flashing is folded down after the soakers or the side welt strip, the water running down the cheek infiltrates under the front metal. Installation must absolutely begin with the front apron flashing, shaped in pleated lead or titanium-zinc with a welt clip on the lower drip edge, turned up 150 mm against the sill face of the dormer.
- Laying the front apron flashingShaping and mechanical fixing of the flashing on the lower kerb. The sheet is beaten to follow the profile of the roof covering downslope, while its two side ends are turned up as ears of at least 50 mm to contain splash-back water.
- Fitting the cheek flashing to the roof slopeInstalling the metal soakers or a welted side channel. The first soaker covers the raised ear of the front apron flashing by means of a tab soldered with tin or folded into a watertight double welt, preventing any infiltration at the corner.
- Laying the cheek claddingMetal cladding or facade slates laid from bottom to top, capping the vertical upstands of the soakers with a free overlap that allows thermal expansion without restraining the waterproofing pieces.
- Connecting the head and the valleysPositioning the side valleys that collect the water from the main roof and the dormer crown, whose final discharge must cross the roof covering overhanging the first row of soakers.
Confluence of the side valleys and continuity of ventilation
When the dormer roof has its own slopes — as with double-pitched or hipped (capucine) dormers — the connection with the main roof slope is made by metal side valleys. These valleys are channels with a high concentration of flow. They must have a drainage cross-section calculated according to the catchment area and a sufficient slope to prevent any lateral overflow under the adjacent tiles or slates.
| Connection component | Minimum girth | Fixing method | Main function |
|---|---|---|---|
| Front apron flashing | 250 to 330 mm | Sliding clips and welts | Discharge of facade water onto the downslope tiles |
| Cheek soakers | 180 to 220 mm | Nailed at the head on battens | Side watertightness, element by element, under the roof covering |
| Side valley channel | 330 to 500 mm | Indirect hooking clips | Collection of water from converging slopes without perforation |
| Ventilation grille | Continuous cross-section 200 cm²/m | Screwed under drip edge or fascia strip | Air inlet of the cheek and outlet of the under-roof air gap |
Integrating the dormer's ventilation complicates the geometry of the flashings. Air passage must be ensured to ventilate the underside of the cheeks and the dormer's own roof, while maintaining the watertight barrier of the main underlay. An abrupt interruption of the counter-battening against the side of the dormer creates a dead zone where condensation and summer heat accumulate. The ventilated air gap of the main roof, with a minimum thickness in accordance with the rules for ventilated roof coverings, must bypass the trimmer without being blocked by the folds of the metal strips.
For the safety of operators during the shaping and laying of these edge metal works, the Swiss requirements are clear: art. 41 OTConst imposes appropriate measures to prevent falls as soon as the fall height exceeds 2 m, by means of a roofer's working platform or a perimeter guardrail adapted to the pitch of the main roof slope. Mitre cuts and copper-iron soldering require a stable footing to ensure the extreme dimensional accuracy required at the junction points.
Handling damage at dormer flashings and rework
An error in the laying sequence of a dormer's four flashings almost systematically leads to water infiltration at the low point of the cheek. When the front apron flashing, the cheek connection, the side valley and the ventilation device do not overlap in the direction of gravity-driven flow, run-off water is diverted under the battens or behind the underlay barrier. Faced with proven damage, the foreman must act methodically: locate the watertightness failure without damaging the adjacent metalwork, secure the structural roof framing elements and notify the situation to the site management.
- Methodical removal of the downslope areaRemove the tiles or roofing elements surrounding the bottom of the cheek over a width of two courses to fully expose the pleated or beaten flashing. Uncover the underlay connection to establish the real path of the infiltration and the condition of the ventilation battens.
- Restoring the overlap cascadeRelease the lower tab of the side valley fixed over the cheek. Slide in a soldered or welted diverting kerb that clearly overlaps the front apron flashing, ensuring a minimum upstand height of 150 mm against the cheek panel.
- Watertight connection of the underlayReconstruct the underlay sheet with a bonded collar running up along the dormer gable. Fixing is carried out sheltered from run-off, above the line of the highest foreseeable water crest under the tiles.
- Checking the ventilation circuitCheck that the air inlet and outlet openings of the cheek and of the main roof remain completely unobstructed, with no pinching of the sheets and no blockage by the connection fittings.
If the timber support shows cubical rot or surface rot due to prolonged stagnant moisture, the metal roofer must suspend the repair of the metalwork. In accordance with art. 365 CO, the contractor immediately informs the client when the ground or the material supplied by the client is defective or if another circumstance jeopardises the timely and proper execution of the work. Repair of the roof framing timbers is the carpenter's responsibility before any final refitting of the metalwork.
Frequently asked questions
How should the connection at the low point be treated if the existing roof covering is already laid?
It is essential to remove at least two courses of tiles below the dormer eaves and around the cheeks. Attempting to slide in a flashing without removing the tiles prevents the correct fixing of the attachment clips and destroys the mechanical interlock of the sheet with the side valley elements. Local removal remains the only way to ensure a watertight overlap.
Why does the side valley regularly overflow during violent storms?
This backflow occurs when the valley channel is undersized or the tiles are cut too close to the axis, reducing the flow cross-section. The wave of water strikes the side of the cut tiles instead of falling freely onto the front apron flashing, causing a local hydraulic overload that infiltrates under the cheek sheet.
How can ventilation of the underlay be ensured at the cheek hip?
The ventilation gap under the roof covering must communicate with the free volume of the roof slope without being choked by the cladding sheets. Counter-battens are laid to leave a continuous ventilation slot, then a rodent-proof grille is fitted at the cheek foot. The metal facade cladding must never crush the underlay sheet against the framing.
Which material should be preferred for shaping the front apron flashing on strongly profiled tiles?
For strongly profiled tiles, rolled lead of sufficient thickness or a pleated aluminium composite strip lined with butyl offers the essential malleability. These materials faithfully follow the relief of the roof covering without excessive creasing, which prevents the formation of capillary channels bringing water back under the eaves during driving rain or snow accumulation.
Texts and standards cited
- CO art. 365material and ground: the contractor is responsible for the good quality of the material he supplies; if the material supplied by the client or the ground designated by the client is found to be defective, or if another circumstance jeopardises the proper or timely execution of the work, he informs the client immediately, failing which he bears the consequences (para. 3).