Skip to content
Website
🧱 CFC 274Metal stairs and handrailsChapter 3 of 10 in the section

Do not slip: non-slip surface, contrasting nosing and wet grating

Outdoors, a wet metal step quickly turns an access stair into a critical slip zone. This chapter details the technical choice of walking surfaces according to their level of exposure, the integration of contrasting step nosings and the design of grating so that water drains away without creating a feeling of void under users' feet.

Key takeaways

  • Checker plate becomes extremely slippery as soon as rainwater or frost settles on it.
  • Pressed or electroforged grating ensures immediate drainage on steps regularly exposed to the weather.
  • The step nosing must provide continuous mechanical roughness and a clearly marked visual contrast.
  • Standard SIA 358 sets the safety criteria for crossing changes in level without risk of tripping.

Ban checker plate outdoors and size draining grating correctly

On a metal finishing work construction site, specifying or laying ribbed or checker plate on an uncovered exterior stair is a classic mistake with serious consequences. As soon as a film of water covers the diamond-pattern relief, smooth-soled or leather-soled shoes lose all grip through aquaplaning. In winter, the ribs retain meltwater, which freezes in the hollows, creating a flat, completely iced-over surface. Light metalwork requires checker plate to be reserved for dry interior technical rooms and genuinely draining solutions to be adopted for any flight exposed to the weather.

Electroforged or pressed grating
Rigid assembly made of vertical load-bearing bars and transverse spacers (twisted square bars or flat bars inserted under press), providing an open surface that instantly drains water, mud and melting snow.

For escape stairs, technical access routes and open exterior links, metal grating remains the most reliable standard answer. The usual safety mesh has an opening of 30 by 19 millimetres or 30 by 10 millimetres to prevent the passage of thin heels and to limit the feeling of vertigo for people sensitive to heights. For particularly greasy environments or those exposed to morning frost, the metalworker selects serrated or toothed load-bearing bars. These stop teeth break the film of oil or ice under the pressure of the step, providing a high grip class without increasing the dead weight of the structure.

Where the client rejects the visual appearance of open-type grating, hot-pressed perforated steel or aluminium sheet offers an excellent closed alternative. These steps have holes pressed upwards with serrated edges to grip the sole, alternating with holes flared downwards that allow water to drain by gravity. A slight transverse or forward slope of between one and two per cent prevents pools of standing water from forming on the resting landings.

Designing a visible, serrated step nosing that complies with safety rules

Circulation elements and their immediate surroundings must be designed to prevent falls and missteps, ensuring regular geometry, a non-slip surface and clear perception of edges.

norme SIA 358

Going down a stair is the critical phase in which most serious accidents occur. The foot lands mainly on the first four centimetres of the step. The metal step nosing must therefore combine impeccable mechanical strength, enhanced grip and unambiguous visual delimitation, in direct accordance with accessibility and safe-use requirements.

Behaviour of metal step nosing finishes in real conditions
Type of step nosingGrip on wet floorVisual contrastMaintenance and durability
One-piece pressed perforated profileVery high (raised serrations)Medium (uniform galvanised colour)Excellent, no detachment possible
Screwed-on ribbed angleMedium to low depending on foulingLow if same steel shadeRequires regular checking of fixings
Sand-filled polyurethane resin insertHigh (corundum aggregate)Very high (contrasting colours)Sensitive to repeated mechanical impacts
Two-colour powder-coated aluminium profileGood (longitudinal ribs)Very high (opposite RAL shade)Check countersunk-head screws on installation

On a standard grating step, the step nosing consists of a perforated angle or folded sheet with a return of at least 30 millimetres, welded in the workshop at the end of the panel. This front angle stiffens the step across its full width and marks the edge with its tighter perforation pattern. On smooth folded-sheet steps fitted with a covering, the metalworker fixes an aluminium or stainless steel profile with a non-slip insert whose light reflectance value differs clearly from that of the tread.

  1. Checking squareness with a templateCheck the flatness of the nosing before tightening the end bolts on the stringers to avoid any warping of the bearing surface.
  2. Mechanical fixing of edge profilesUse A4 stainless steel countersunk-head metal screws, perfectly flush, with no machining burrs on the walking surface.
  3. Checking drainage at the endsLeave a 5 millimetre gap between the end of the step nosing and the stringer to allow lateral drainage of water and dust.

Choosing surfaces according to exposure and draining standing water

In exterior metalwork, a metal step exposed to the weather tolerates no approximation as regards grip. The classic mistake is to underestimate the water film, the formation of ice at altitude or plant deposits under trees. Checker or ribbed plate, although accepted in a dry workshop, retains water between its reliefs and immediately becomes a slippery surface at the first rain. To meet accident-prevention requirements and the recognised rules of the trade, the metalworker must specify open profiles or profiles with a through-relief guaranteeing a high friction coefficient and instant drainage.

Suitability of metal step surfaces according to weather exposure in Switzerland
Type of surfaceRecommended exposure zoneDrainage capacitySensitivity to frost and leaves
Pressed serrated grating (sawtooth)Uncovered exterior and access walkwaysExcellent (opening above 75 %)Very low: ice does not build up
Pressed perforated sheet with raised holesSheltered exterior or escape stairsGood via the negative perforationsMedium: risk of fouling by residues
Epoxy or polyurethane resin with corundum sandCovered exterior landings and access balconiesNone: requires a drainage slopeHigh if residual water freezes on the surface
Galvanised checker or ribbed plateStrictly reserved for dry interior technical roomsNone (permanent standing water in the hollows)Critical: immediate formation of a slippery film

For open stairs in expanded metal or grating, water drains vertically by gravity without needing a slope on the tread. On the other hand, as soon as a perforated sheet or steel tray receives a solid infill, a minimum transverse slope of 1.5 to 2 % towards the front or the side strings is required when setting out the stringers. Without this fabricated fall, water stagnates in the centre of the sheet owing to the residual deflection of the steps, forming a film of standing water that hardens into overnight ice.

Serrated non-slip bar
Load-bearing bar or cross bar of metal grating machined with a sawtooth or deep notches on its upper part, increasing the contact pressure under the sole to break films of oil, water or frost.

Integrating the contrasting step nosing and mechanical fixing to the stringer

The step nosing is the first spatial reference when going down a stair. A grey metal edge that blends in with the lower tread encourages misplaced footing and serious falls into the void. Standard SIA 358 governs the geometric characteristics and safe use of balustrades and stairs, while the accessibility guidelines require step nosings to be identified unambiguously from the rest of the step. To obtain an effective visual contrast, the light reflectance coefficient between the nosing and the tread must show a sufficient difference, perceptible in the dark or under raking artificial lighting.

On a metal frame, marking the step nosing rests on three execution principles in the workshop and on the construction site. For grating, a specific front profile in hot-folded angle iron is preferred, perforated on its upper face and fitted with projecting stop serrations. This front flange, welded to the ends of the load-bearing bars, stiffens the step while delimiting the visual edge. On solid steps in galvanised or powder-coated folded sheet, inserting an added aluminium profile or a two-component resin loaded with corundum creates the visual and tactile break.

  1. Preparing the front edgeMachine or fold the step nosing with a bending radius of between 2 and 5 mm to avoid any sharp edge on the galvanised steel while keeping a clean line.
  2. Fitting the contrasting stripFit an added edge profile, black-anodised or safety yellow, 40 to 50 mm wide, fixed with A4 stainless steel countersunk-head screws to resist de-icing salts.
  3. Flushness and removal of protrusionsRecess the non-slip profile into a machined step or a suitable fold so that no excess thickness greater than 2 mm catches the toe of the sole when going up.
  4. Mechanical connection to the stringersBolt the side flanges of the step to the fixing plates welded to the steel stringers using high-strength galvanised bolts with neoprene sealing washers.
  • Check the visual alignment of the step nosings over the whole flight to avoid optical disturbances when going down.
  • Check the tightening torque of the stainless steel nosing profile screws to prevent any loosening under the vibrations of foot traffic.
  • Remove zinc splashes and galvanising burrs with a deburring tool before fixing the contrasting inserts.
  • Validate the continuity of visual contrast between the first and last step of the metal stair.

Handling non-conformities: critical slipperiness, lack of contrast and standing water

When an exterior metal stair undergoes its first autumn rains, the technical penalty is not long in coming: a checker plate laid by mistake becomes a genuine ice rink, or a poorly oriented grating landing accumulates a pool of standing water. As soon as site management or the safety expert raises a non-conformity within the meaning of standard SIA 358, the metalworker must act quickly to adapt the walking surface without having to remove all the stringers or weaken the workshop fixings.

  1. Diagnosing slipperiness and drainageAbsolutely check the orientation of the load-bearing bars of the grating and the flatness of the tread. An inverted grating retains dirt and prevents water from falling between the meshes. On a solid sheet step, measure the slope: the absence of a slight forward inclination retains the water film, encouraging plant deposits and winter ice.
  2. Mechanical fixing of serrated nosing profilesOn a slippery tread, screw a serrated or pressed metal profile onto the upper part. A flat bar in anodised aluminium or perforated stainless steel is preferred, secured with metric-pitch stainless steel countersunk-head screws with locknuts under the step, so as to create a sharp edge that grips the sole.
  3. Restoring the visual contrast of the nosingTreat the step nosing with a contrasting visual shade over a width of forty to fifty millimetres. A dark powder-coated angle on a light or galvanised sheet restores immediate perception of the leading edge, a fundamental criterion for making the descent safe for visually impaired users.
  4. Drilling and draining water-retention zonesWhere a rear fold or a support cross-member traps water at the bottom of the step, drill drainage holes of ten millimetres in diameter at the low points. Carefully deburr each hole and immediately apply a zinc-rich primer to prevent any onset of oxidation on the finished work.

To clear the reservations recorded in the acceptance report, submit a validated remedial sample to site management. Only a screwed-on, hard-wearing and draining grip solution restores safe use while preserving the warranty on the work under the Code of Obligations (CO).

Frequently asked questions

Can a slippery checker plate be corrected without replacing the steps?

Yes, by mechanically adding a suitable surfacing to each existing tread. A serrated profile in aluminium or perforated stainless steel is fixed at the step nosing, secured by through-screwing with nuts under the step. A polyurethane coating loaded with corundum aggregate can also be applied to the foot-bearing area, after careful degreasing and sanding of the sheet, to create a lasting and safe roughness.

How do you design a contrasting step nosing on metal grating?

On a pressed or electroforged grating step, the step nosing must be fitted with a specific perforated leading profile welded in the workshop. This front profile, often made of a domed perforated angle, provides both non-slip grip and a clear visual break from the open mesh of the tread. If necessary, contrasting powder coating of this front angle before galvanising or final powder coating accentuates the visual legibility required for the stair.

Which grating mesh ensures drainage without trapping shoes?

For an exterior stair used by the public or serving dwellings, standard SIA 358 and the safety recommendations advocate a so-called heel-safe mesh, generally thirty by ten millimetres or nineteen by nineteen millimetres. This configuration prevents the passage of a twenty-millimetre ball, prevents thin heels from catching, while still offering enough open area to drain rainwater and melting snow immediately.

Why is the laying direction of the grating bars crucial for safety?

The load-bearing bars must absolutely rest from one stringer to the other in the direction of the span to carry the mechanical load without bending. The cross bars inserted at the surface, often serrated, cross the direction of the user's stride, which improves slip resistance when walking. Reversing the panel dangerously weakens the step and reduces the longitudinal friction needed to stop the foot when going down.

Texts and standards cited

  • SIA 358Balustrades and safety when walking
  • code des obligationsGeneral rules of the contract for work and warranty for defects

In the same section