Skip to content
Website
🧱 CFC 281Levelling compounds, industrial floors and screeder safetyChapter 3 of 10 in the section

Surface hardening: quartz incorporation, mechanical floating and working window

This chapter provides you with construction site benchmarks for successfully incorporating a mineral hardener onto fresh screeds or slabs. You will learn how to precisely assess the consistency of the substrate using the footprint test, how to distribute the quartz aggregate at the correct dosage, and how to carry out mechanical floating until complete closure without any risk of delamination.

Key takeaways

  • The boot footprint test determines the exact timing for the first dusting on the construction site.
  • Incorporating too early drowns the aggregates while a delay prevents any durable mechanical bond.
  • The dosage is applied in two regular cross passes to prevent the layer from peeling.
  • The gradual tilting of the power trowel blades ensures a dense finish without burning.

Determine the incorporation window and distribute the mineral hardener

The installation of an incorporated wear screed or surface treatment using a mineral hardener is subject to strict physical constraints defined by the SIA 251 standard. Unlike an adhered bonded screed, the quartz- or corundum-based hardener must bond intimately with the cement matrix while it is still plastic. If application starts too early, before the bleed water has evaporated, the powder sinks into the mass, creates a friable crust and loses its abrasive power. Conversely, if the binder's setting process is too advanced, the quartz remains on the surface without being able to capture the moisture required for its hydration, leading to immediate delamination under forklift traffic.

Boot footprint test
Empirical construction site check consisting of placing a foot on the concrete as it sets; a residual mark between 3 and 5 mm deep indicates the exact start of the floating and broadcasting window.

Consistency diagnosis relies on the actual state of the material rather than the clock. Setting speed varies according to ambient relative humidity, slab temperature and air currents within the building. As soon as free bleed water has completely disappeared and the screeder's boot only sinks by a few millimetres, the first hardener pass must begin. Any additional delay compromises the bonding of the grains.

Indicative quartz dosage according to exposure class
Targeted stressRecommended dosageDistribution methodNumber of passes
Pedestrian traffic or light workshop3 to 4 kg per m²Manual or mechanical trolley1 to 2 passes
Medium industrial traffic4 to 5 kg per m²Towed mechanical spreader2 cross passes
Heavy traffic with hard wheels5 to 7 kg per m²Guided automatic spreader2 to 3 cross passes

To ensure uniform wear resistance, distribution is systematically carried out in cross passes. The first pass receives approximately 60 percent of the total load. The product absorbs moisture from the underlying concrete, which is visually reflected by a uniform darkening of the powder. Only after this spontaneous wetting can preliminary mechanical work begin.

Carry out mechanical floating and close the surface without burning the paste

Compacting the hardener requires the use of a power trowel, commonly referred to as a helicopter. The machine is initially equipped with a floating pan or combined blades set flat. This initial phase aims to mix the quartz powder with the surface laitance without digging ruts. The machine operator moves at a slow, constant speed, making regular circular movements to bring up the binder and coat each mineral grain.

  1. First pan floatingAs soon as the first quartz pass darkens, pass the pan flat to press the aggregate into the top layer and reactivate the laitance.
  2. Second hardener passSpread the remaining 40 percent perpendicularly to the first pass, wait for the powder to wet completely, then float again with the pan.
  3. Fitting floating bladesRemove the pan as soon as the paste gains cohesion; work with the blades angled at a minimum of two to three degrees.
  4. Closure and final smoothingGradually increase the angle of the finishing blades and the rotation speed to densify the skin without excessively darkening the surface.

Closure is complete when the floor presents a uniform satin sheen and the machine leaves no visible trace of its passage. According to Swiss rules of the art, the operation does not stop at the last turn of the power trowel: the immediate application of a certified curing product is essential to block the premature evaporation of residual water. This treatment prevents the appearance of surface map cracking and ensures that the wear resistance performances specified for industrial premises are achieved.

Immediate curing and matrix preservation according to SIA 251

As soon as mechanical smoothing with the power trowel or rotary floater is complete, the industrial screed enters a critical phase of thermal and hygrometric vulnerability. The quartz-enriched wear layer exhibits very high mineral density but a locally lowered water-cement ratio due to surface evaporation. The SIA 251 standard prescribes immediate and continuous protection against desiccation to guarantee the complete hydration of hydraulic binders at the surface. Without an effective barrier against early evaporation, differential shrinkage stresses cause irreversible surface micro-crazing, nullifying the hardness gain imparted by the quartz aggregates.

The choice of curing method depends on the subsequent operating constraints of the industrial room. Applying a resin-based curing product forms a temporary waterproof film that retains the mixing water essential for the crystallization of silicates. If the client plans the subsequent application of a silicate impregnation, floor marking paint or a specific anti-dust treatment, the use of a paraffinic curing wax is prohibited as it would inhibit adhesion. A wet cure using polyethylene sheeting kept in contact or degradable acrylic emulsions is therefore preferred.

Comparison of curing methods on floated mineral screed
Curing methodImplementationAdvantagesConstruction site constraints
Acrylic film-forming productLow-pressure cross spraying as soon as the liquid sheen disappearsContinuous protection, compatible with certain floor markingsSensitive to strong air currents during application
Polyethylene sheetLaying flat with a 200 mm overlap and ballasting the edgesRetains water without chemical addition, economical on large areasRisk of coloured marbling due to heterogeneous condensation
Continuous wet cure (moistened geotextile)Placement after contact hardening, permanent gentle wateringOptimal hydration of very dense corundum or quartz layersTricky water management, prohibited on intermediate floors

Incorporation pathologies: diagnostics, debonding and acceptance

Rigorous compliance with the incorporation window determines the monolithic integrity of the industrial floor. The thermal difference between the substrate concrete and ambient air dictates the setting speed. If the mineral hardener is sown too early, excess bleed water drowns the quartz grains in a soft laitance that will erode under truck traffic. Conversely, late dusting on a substrate that has started its setting prevents the mechanical penetration of aggregates: the wear mixture then forms a detached surface crust a few millimeters thick that will delaminate in plates under rolling loads.

The qualification of defects relies on non-destructive testing and targeted core drilling prior to the acceptance of the work in accordance with SIA 118 and SIA 251 standards. Auscultation testing using a screeder's hammer or impact chain immediately reveals delaminations in the form of hollow resonances. If blistering occurs, it almost systematically results from air trapped by premature pore closure during the first pass of the wide blades: compressed water vapour unable to escape through the sealed surface lodges under the hardener crust.

  • Check of flatness according to SIA 251: maximum deflection measured under a 2 m rigid straightedge placed on the wear screed.
  • Verification of surface hardness by sclerometer or ball indentation to certify the cohesion of the quartz matrix.
  • Joint inspection record of spalling along contraction joint cuts, direct indicators of edge fragility linked to defective dusting.
  • Visual inspection under grazing light to locate local thickness excesses due to irregular dispersion of the hardener during seeding passes.

Managing setting discrepancies and surface corrective measures

On an industrial screed construction site, breaking the incorporation window requires rapid intervention. When quartz dusting occurs too early, the hardener migrates into the laitance under the simple weight of the grains. The surface then becomes enriched with fines lacking mechanical consistency, creating a friable crust sensitive to delamination. Conversely, late incorporation prevents the cement paste from coating the hard aggregates; mechanical floating tears the material instead of compacting it, producing immediate dusting under the passage of the blades.

  1. Diagnosis by impact and core drillingIn the presence of hollow sounds when hammered or chipping, locate the debonded areas. According to SIA 251, the surface cohesion of a wear screed must be measured by direct tension to quantify the depth of the defect.
  2. Planed milling or mechanical shot-blastingIf the quartz has not bitten and is powdering, remove the non-adherent area by steel shot-blasting or diamond milling. The operation must expose sound concrete without creating micro-cracks in the underlying matrix.
  3. Compensation by mineralising treatmentFor a loss of surface bond without frank debonding, apply a lithium silicate-based liquid hardener. The product penetrates residual pores to fix free lime and block abrasion.
  4. Reconstitution as a thin bonded screedIn the event of massive delamination exceeding operating tolerances, strip the altered layer by a minimum of ten millimetres, apply a specific bonding slurry and pull a micro-mortar with a high corundum content.

Rigorous management of these defects preserves the acceptance of the work without compromising the final flatness required by the specifications. Each mechanical rework must be recorded in the construction journal along with the corresponding pull-off test results.

Frequently asked questions

How to identify the exact moment to start quartz dusting?

Incorporation begins when the bleed water has completely evaporated and the screed supports a worker's step without sinking more than three to five millimetres. If the footprint remains visible without leaving liquid mud on the soles of the finishing boots, bearing capacity is optimal. Dusting before this phase causes aggregate submergence; acting later prevents the powder from wetting by capillarity.

What to do if the concrete sets too quickly at the edges due to air currents?

Areas near bays or doors set faster due to accelerated evaporation. The first manual hardener pass must be immediately concentrated on these peripheral strips before treating the main body of the surface. If setting has already started, applying a surface retarder by misting helps maintain sufficient plasticity for the mechanical embedding of the quartz grains by the pan.

What is the method to repair a surface burned by excessive smoothing?

Blackening or burning occurs when steel blades rub against a nearly dry paste with an excessively aggressive angle, leading to optical modification and superficial micro-cracking. The defect is purely aesthetic if the quartz remains compacted. To homogenise the appearance without weakening the matrix, fine dry sanding with a 120-grit diamond disc removes the burned surface film prior to applying a transparent mineral seal.

Why do we sometimes observe complete detachment of the quartz skin after a few weeks?

This delamination results from an application carried out after the pores of the base concrete have closed, often combined with excess floating water. The hardener forms a rigid crust superimposed without crystalline anchorage onto the underlying screed. At the first thermal shock or under forklift truck rolling, shear stresses exceed the low resistance of the interface, causing entire plates of hardener to burst off without cohesion.

Texts and standards cited

  • SIA 251Specifications and tests for floating and bonded screeds in construction

In the same section